Production of SBS Reinforced Polyester Composite: Characterization of Physical and Chemical Properties

H. Şahal, E. Aydoğmuş
{"title":"Production of SBS Reinforced Polyester Composite: Characterization of Physical and Chemical Properties","authors":"H. Şahal, E. Aydoğmuş","doi":"10.18596/jotcsa.1208503","DOIUrl":null,"url":null,"abstract":"In this study, dissolved styrene butadiene styrene (SBS) copolymer is homogeneously reinforced into orthophthalic unsaturated polyester (UP) resin. Polyester composite production is carried out with the help of methyl ethyl ketone peroxide (MEKP) and cobalt octoate (Co Oc) catalysts. The density, Shore D hardness, thermal conductivity coefficient, thermal stability, morphological surface structure, and chemical bond structure of the obtained composite have been examined. According to the results, SBS reinforcement decreases the density of the composite and increases the thermal conductivity coefficient. The addition of SBS at different weight ratios (1%, 3%, 5%, 7%, and 10% w/w) reduces both the hardness and thermal stability of the polyester composite. According to the test and analysis results, 5 wt.% SBS reinforced polyester composite production is determined as the optimum ratio. 7 wt.% and above SBS reinforcement negatively affect the physical and chemical properties of the obtained composite. For example, when 10 wt.% SBS reinforced composite is examined by scanning electron microscope (SEM), and irregular pores are observed in the surface morphology. Also, it is understood by Fourier transform infrared spectroscopy (FTIR) that there is a physical interaction between SBS and polyester and that no chemical bond is formed. The thermal decomposition behavior of the composite has been determined according to the decrease in the activation energy. As SBS ratio increases, it is understood that the thermal stability of the product obtained with the decrease in the activation energy of the polyester composite weakens.","PeriodicalId":17299,"journal":{"name":"Journal of the Turkish Chemical Society Section A: Chemistry","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2023-07-12","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of the Turkish Chemical Society Section A: Chemistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.18596/jotcsa.1208503","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

In this study, dissolved styrene butadiene styrene (SBS) copolymer is homogeneously reinforced into orthophthalic unsaturated polyester (UP) resin. Polyester composite production is carried out with the help of methyl ethyl ketone peroxide (MEKP) and cobalt octoate (Co Oc) catalysts. The density, Shore D hardness, thermal conductivity coefficient, thermal stability, morphological surface structure, and chemical bond structure of the obtained composite have been examined. According to the results, SBS reinforcement decreases the density of the composite and increases the thermal conductivity coefficient. The addition of SBS at different weight ratios (1%, 3%, 5%, 7%, and 10% w/w) reduces both the hardness and thermal stability of the polyester composite. According to the test and analysis results, 5 wt.% SBS reinforced polyester composite production is determined as the optimum ratio. 7 wt.% and above SBS reinforcement negatively affect the physical and chemical properties of the obtained composite. For example, when 10 wt.% SBS reinforced composite is examined by scanning electron microscope (SEM), and irregular pores are observed in the surface morphology. Also, it is understood by Fourier transform infrared spectroscopy (FTIR) that there is a physical interaction between SBS and polyester and that no chemical bond is formed. The thermal decomposition behavior of the composite has been determined according to the decrease in the activation energy. As SBS ratio increases, it is understood that the thermal stability of the product obtained with the decrease in the activation energy of the polyester composite weakens.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
SBS增强聚酯复合材料的生产:物理和化学性能表征
在本研究中,溶解的苯乙烯-丁二烯-苯乙烯(SBS)共聚物被均匀增强成邻苯二甲酸不饱和聚酯(UP)树脂。在过氧化甲乙酮(MEKP)和八酸钴(Co Oc)催化剂的帮助下,进行了聚酯复合材料的生产。测试了复合材料的密度、邵氏硬度、导热系数、热稳定性、表面形态结构和化学键结构。结果表明,SBS增强降低了复合材料的密度,提高了导热系数。不同重量比(1%、3%、5%、7%和10% w/w)的SBS的加入降低了聚酯复合材料的硬度和热稳定性。根据试验分析结果,确定了5 wt.% SBS增强聚酯复合材料的最佳配比。7 wt.%及以上的SBS增强对得到的复合材料的物理和化学性能有负面影响。例如,当用扫描电镜观察10 wt.% SBS增强复合材料时,在表面形貌上观察到不规则的孔隙。此外,通过傅里叶变换红外光谱(FTIR)可以了解SBS与聚酯之间存在物理相互作用,而没有形成化学键。根据活化能的降低来确定复合材料的热分解行为。据了解,随着SBS比的增加,随着聚酯复合材料活化能的降低而得到的产品的热稳定性减弱。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Microdetermination of Piroxicam in Pharmaceutical Formulations by Complexation with Fe(III) and Image Scanning Densitometry New Generation Nanoadsorbents and Conventional Techniques for Arsenic Removal from Waters Enhancing Biogas Production with The Addition of Nano-catalysts Degradation of Tolonium Chloride Dye by Phosphate Ion in Aqueous Acidic Solution: Kinetic Approach Preparation of Poly (N-Isopropylacrylamide) -Poly (2-Ethyl-2-Oxazoline) and Their Self-Assembly Properties with Dicarboxylic Acid
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1