Microstructural Investigation of Wire Failure in Wire Drawing Process

F. A. Hashim, Sadiq M. Ihmood, K. Mohammed, Ghaffar Alwan Mohsin
{"title":"Microstructural Investigation of Wire Failure in Wire Drawing Process","authors":"F. A. Hashim, Sadiq M. Ihmood, K. Mohammed, Ghaffar Alwan Mohsin","doi":"10.32792/utq/utj/vol14/1/5","DOIUrl":null,"url":null,"abstract":"This investigation concern to explain the failure operation that connected with wire drawing process. Microstructural examination was carried out for several samples of drawn wires. Copper and aluminum wires were pulled from 8 mm diameter to 3.5 mm for aluminum and to 1.75 mm for copper. The cross-sectional microstructure shows some porosity at the normal drawing condition, while no porosity at the drawing direction surface. The conclusion of this work represents that porosity will be created due to heat results from drawing process, which equal to recrystallization temperature or more, and accumulated porosity will be progressive to the final stage of wire failure.","PeriodicalId":23465,"journal":{"name":"University of Thi-Qar Journal","volume":"47 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-04-25","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"University of Thi-Qar Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.32792/utq/utj/vol14/1/5","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

This investigation concern to explain the failure operation that connected with wire drawing process. Microstructural examination was carried out for several samples of drawn wires. Copper and aluminum wires were pulled from 8 mm diameter to 3.5 mm for aluminum and to 1.75 mm for copper. The cross-sectional microstructure shows some porosity at the normal drawing condition, while no porosity at the drawing direction surface. The conclusion of this work represents that porosity will be created due to heat results from drawing process, which equal to recrystallization temperature or more, and accumulated porosity will be progressive to the final stage of wire failure.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
拉丝过程中钢丝失效的显微组织研究
本调查旨在解释与拉丝工艺有关的失效操作。对几根拉丝试样进行了显微组织检查。铜线和铝线的直径从8毫米缩短到3.5毫米,铜线缩短到1.75毫米。断面微观结构在正常拉伸状态下有一定的孔隙度,而在拉伸方向表面无孔隙度。本研究的结论表明,拉拔过程中产生的等于或高于再结晶温度的热量会产生气孔,并且气孔的积累会逐渐累积到钢丝失效的最后阶段。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Shear Strength Evaluation of Directly and Indirectly Loaded Rectangular Recycled Self-Compacted Reinforced Concrete Slender Beams Using Experimental and Finite Element Analysis Study of Some Hematological Parameters in Offpring of Heperlipidemic Female Laboratory Rats After Slmvastatln Treatment During Lactation. Study of Some Hematological Parameters in Offpring of Heperlipidemic Female Laboratory Rats After Slmvastatln Treatment During Lactation Preparation and Characterization of New Ligand Azo-Schiff-2- Naphthol and Mixed Complexes With Ortho- Aminophenol and Ortho-Aminobenzoic Acid. Selected Antenatal Health Care Parameters of Pregnant Women’s in Duhok Province, Iraq.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1