{"title":"Optimization of test procedure to improve insulator performance under high electric stress","authors":"T. Asokan, T. S. Surdashan","doi":"10.1109/14.231537","DOIUrl":null,"url":null,"abstract":"Surface flashover properties in relation to test procedures were investigated, using single-cycle steady step, multiple-cycle steady-step, multiple-shot, and hill-valley tests. In general, the test procedures were found to influence significantly the surface flashover properties of large-bandgap insulators such as polycrystalline alumina and signal-crystal quartz in vacuum. The steady-step tests increased the degree of conditioning to a higher level during the second day. However, the samples subjected to these tests displayed a higher degree of deconditioning during the second and third day. A simultaneous increase of conditioning and decrease of deconditioning was observed for the multiple-shot and hill-valley tests. The surface flashover performances of 6- mu m-finish alumina specimens for different test procedures are also compared and discussed. The behavior of the insulators under a given test procedure is explained on the basis of surface electronic defects and adsorbed gaseous atoms or molecules. >","PeriodicalId":13105,"journal":{"name":"IEEE Transactions on Electrical Insulation","volume":"1 1","pages":"545-554"},"PeriodicalIF":0.0000,"publicationDate":"1993-08-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"5","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"IEEE Transactions on Electrical Insulation","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/14.231537","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 5
Abstract
Surface flashover properties in relation to test procedures were investigated, using single-cycle steady step, multiple-cycle steady-step, multiple-shot, and hill-valley tests. In general, the test procedures were found to influence significantly the surface flashover properties of large-bandgap insulators such as polycrystalline alumina and signal-crystal quartz in vacuum. The steady-step tests increased the degree of conditioning to a higher level during the second day. However, the samples subjected to these tests displayed a higher degree of deconditioning during the second and third day. A simultaneous increase of conditioning and decrease of deconditioning was observed for the multiple-shot and hill-valley tests. The surface flashover performances of 6- mu m-finish alumina specimens for different test procedures are also compared and discussed. The behavior of the insulators under a given test procedure is explained on the basis of surface electronic defects and adsorbed gaseous atoms or molecules. >