{"title":"Color changes of ash wood (Fraxinus excelsior L.) caused by thermal modification in air and steam","authors":"J. Gawron, M. Marchwicka","doi":"10.5604/01.3001.0015.6639","DOIUrl":null,"url":null,"abstract":"Color changes of ash wood (Fraxinus excelsior L.) caused by thermal modification in air and steam. Ash wood samples of 20x20x30 mm were subjected to thermal modification in different conditions. The thermal modification was conducted in air at 190 °C and in steam at 160 °C. For both environments modification lasted 2, 6 and 10 hours. Samples color parameters were measured before and after thermal modification on the basis of the mathematical CIELab color space model. Changes in all parameters (L, a and b) were observed, the highest in lightness (L) - darker color. The total color difference (ΔE) and chromaticity change (ΔC) were calculated for all samples. The highest value of ΔE was obtained for wood modified in the air at 190 °C for 10 h. The highest value of ΔC was obtained for wood modified in steam at 160 °C for 10 h. However, the value obtained for wood modified in the air at 190 °C for 10 h were only slightly lower.\n\n","PeriodicalId":8020,"journal":{"name":"Annals of WULS, Forestry and Wood Technology","volume":"20 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2021-12-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Annals of WULS, Forestry and Wood Technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5604/01.3001.0015.6639","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2
Abstract
Color changes of ash wood (Fraxinus excelsior L.) caused by thermal modification in air and steam. Ash wood samples of 20x20x30 mm were subjected to thermal modification in different conditions. The thermal modification was conducted in air at 190 °C and in steam at 160 °C. For both environments modification lasted 2, 6 and 10 hours. Samples color parameters were measured before and after thermal modification on the basis of the mathematical CIELab color space model. Changes in all parameters (L, a and b) were observed, the highest in lightness (L) - darker color. The total color difference (ΔE) and chromaticity change (ΔC) were calculated for all samples. The highest value of ΔE was obtained for wood modified in the air at 190 °C for 10 h. The highest value of ΔC was obtained for wood modified in steam at 160 °C for 10 h. However, the value obtained for wood modified in the air at 190 °C for 10 h were only slightly lower.