{"title":"Synthesis and Characterisation of PVA/PVOH Based Super Porous Hydrogel","authors":"S. K. Barik, H. Sutar, S. Mishra","doi":"10.9734/ACSJ/2016/22127","DOIUrl":null,"url":null,"abstract":"The present paper explains the synthesis of super porous hydrogel (SPH) with reinforcement of different concentrations (0.05, 0.1, 0.15 and 0.2 g) of PVA by solution polymerization. The polymerisation process is conducted at a pH value of 5. The corollaries of PVA on different characteristics of super porous hydrogel were studied. The characterization study involves measurement of apparent density, swelling, mechanical strength and microstructure. The PVA added SPH are treated for a total time of 550 minutes in double distilled water and acid salt solution to analyse the swelling properties. The result shows that inclusion of PVA to SPH reduces its swelling tendency culminating that; the empathy for swelling is more in double distilled water than acid medium.","PeriodicalId":7399,"journal":{"name":"American Chemical Science Journal","volume":"33 1","pages":"1-7"},"PeriodicalIF":0.0000,"publicationDate":"2016-01-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"American Chemical Science Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.9734/ACSJ/2016/22127","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The present paper explains the synthesis of super porous hydrogel (SPH) with reinforcement of different concentrations (0.05, 0.1, 0.15 and 0.2 g) of PVA by solution polymerization. The polymerisation process is conducted at a pH value of 5. The corollaries of PVA on different characteristics of super porous hydrogel were studied. The characterization study involves measurement of apparent density, swelling, mechanical strength and microstructure. The PVA added SPH are treated for a total time of 550 minutes in double distilled water and acid salt solution to analyse the swelling properties. The result shows that inclusion of PVA to SPH reduces its swelling tendency culminating that; the empathy for swelling is more in double distilled water than acid medium.