{"title":"Studie on Malachite Green Dye Degradation by Biogenic Metal Nano Cuo And Cuo/Zno Nano Composites","authors":"M. Batool, Z. Qureshi, Nida Mehboob, Abdul Salam Shah","doi":"10.32474/ANOAJ.2018.01.000119","DOIUrl":null,"url":null,"abstract":"The biosynthesis of nanoparticles put forward a cost-free and eco-friendly method for the synthesis of nanoparticles. In this paper degradation of Malachite green has been carried out using Copper nanoparticles synthesized by Aloe Barbadensis leaf extracts. The green synthesis of the copper nanoparticles has been carried out using an aqueous solution of copper sulphate and extract of Aloe Barbadensis. The colour change of the reaction mixture containing 1mm copper sulphate has been observed from deep blue to colourless and then brick red to dark red indicating the formation of copper nanoparticles. For the characterization of CuO nanoparticles, Ultraviolet (UV), Infrared (IR), X-ray Diffraction (XRD), and Scanning Electron Microscopy (SEM) have been used. The experimental analysis has revealed an average 60n sized synthesized CuO nanoparticles. The shape of copper nanoparticles has been observed as spherical and cubic ranging between 80-120nm. The different functional group of synthesized nanoparticles has been examined usingFourier-Transform Infrared Spectroscopy (FTIR). The UV spectrophotometer has confirmedthe peak of Copper nanoparticles at 265-285nm.The maximum absorbance of Copper oxide nanoparticles has been observed at 280nm. copper oxide /zinc oxide nanocomposite were synthesized using cheap and cost effective sol-gel method. These cuo/zno nanocomposite were characterized by analytical techniques like (SEM), (TEM), X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR) and ultraviolet-visible spectroscopy (UV-VIS. The Fourier transform IR analysis result confirmed that composite material were formed. SEM images showed the particle size in the range between 15 to 35nm. Nanocomposite exhibited excellent microwave induced catalytic degradation for malachite green (MG) dye. The initial concentration was 1.8 X 10-5M degradation. The microwave induced catalysis reaction gained about 80% degradation of Malachite Green dye.","PeriodicalId":8322,"journal":{"name":"Archives of Nanomedicine: Open Access Journal","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2018-07-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Archives of Nanomedicine: Open Access Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.32474/ANOAJ.2018.01.000119","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

Abstract

The biosynthesis of nanoparticles put forward a cost-free and eco-friendly method for the synthesis of nanoparticles. In this paper degradation of Malachite green has been carried out using Copper nanoparticles synthesized by Aloe Barbadensis leaf extracts. The green synthesis of the copper nanoparticles has been carried out using an aqueous solution of copper sulphate and extract of Aloe Barbadensis. The colour change of the reaction mixture containing 1mm copper sulphate has been observed from deep blue to colourless and then brick red to dark red indicating the formation of copper nanoparticles. For the characterization of CuO nanoparticles, Ultraviolet (UV), Infrared (IR), X-ray Diffraction (XRD), and Scanning Electron Microscopy (SEM) have been used. The experimental analysis has revealed an average 60n sized synthesized CuO nanoparticles. The shape of copper nanoparticles has been observed as spherical and cubic ranging between 80-120nm. The different functional group of synthesized nanoparticles has been examined usingFourier-Transform Infrared Spectroscopy (FTIR). The UV spectrophotometer has confirmedthe peak of Copper nanoparticles at 265-285nm.The maximum absorbance of Copper oxide nanoparticles has been observed at 280nm. copper oxide /zinc oxide nanocomposite were synthesized using cheap and cost effective sol-gel method. These cuo/zno nanocomposite were characterized by analytical techniques like (SEM), (TEM), X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR) and ultraviolet-visible spectroscopy (UV-VIS. The Fourier transform IR analysis result confirmed that composite material were formed. SEM images showed the particle size in the range between 15 to 35nm. Nanocomposite exhibited excellent microwave induced catalytic degradation for malachite green (MG) dye. The initial concentration was 1.8 X 10-5M degradation. The microwave induced catalysis reaction gained about 80% degradation of Malachite Green dye.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
生物源金属纳米Cuo及Cuo/Zno纳米复合材料降解孔雀石绿染料的研究
纳米颗粒的生物合成为纳米颗粒的合成提供了一种经济、环保的方法。本文利用芦荟叶提取物合成的铜纳米颗粒对孔雀石绿进行了降解。使用硫酸铜水溶液和芦荟提取物进行了铜纳米颗粒的绿色合成。观察到含有1mm硫酸铜的反应混合物的颜色变化,从深蓝色到无色,然后砖红色到暗红色,表明铜纳米颗粒的形成。采用紫外(UV)、红外(IR)、x射线衍射(XRD)和扫描电子显微镜(SEM)对CuO纳米颗粒进行了表征。实验分析表明,合成的CuO纳米颗粒平均粒径为60n。观察到铜纳米颗粒的形状为球形和立方,范围在80-120nm之间。利用傅里叶变换红外光谱(FTIR)研究了合成的纳米颗粒的不同官能团。紫外分光光度计测定了铜纳米粒子在265 ~ 285nm处的峰值。氧化铜纳米粒子的最大吸光度在280nm处。采用溶胶-凝胶法制备了氧化铜/氧化锌纳米复合材料。利用扫描电镜(SEM)、透射电镜(TEM)、x射线衍射(XRD)、傅里叶变换红外光谱(FTIR)和紫外可见光谱(UV-VIS)等分析技术对纳米cuo/zno复合材料进行了表征。傅里叶变换红外分析结果证实了复合材料的形成。SEM图像显示,颗粒尺寸在15 ~ 35nm之间。纳米复合材料对孔雀石绿染料具有良好的微波催化降解性能。初始浓度为1.8 × 10-5M。微波催化反应对孔雀石绿染料的降解率达到80%左右。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Understanding Parallels Between Homeopathy and ‘Nanomedicine’ Nicardipine: Concise Review on Analytical Techniques Formation of Silver Nanoparticles in the root extract of Scutellaria baicalensis and their characterization Recent Development Issues in Nanotechnology for Gas Storage Removal of Melachite Green Dye by Using Zinc Oxide Nanoparticles Prepared by The Green Synthesis by Using Camellia Sinensis (Green Tea) Leafs Extract
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1