盐雾试验研究表面处理301和304不锈钢的耐蚀性

T. Olugbade, B. O. Omiyale
{"title":"盐雾试验研究表面处理301和304不锈钢的耐蚀性","authors":"T. Olugbade, B. O. Omiyale","doi":"10.14232/analecta.2021.2.9-19","DOIUrl":null,"url":null,"abstract":"The corrosion rate of surface-conditioned 301 and 304 stainless\n steels (SS) was determined by salt spray test in a controlled accelerated\n corrosive medium (9.5 L of pure distilled water + 500 g NaCl). By surface\n conditioning via mechanical attrition treatment, a gradient-structured\n layer was firstly generated on the surface of the samples before the salt\n spray test. The corrosion rate was determined by the weight loss before and\n after the salt spray test. Compared to the untreated 301 SS sample with a\n weight loss of 0.15 g, the surface-conditioned samples treated for 300 s\n and 1200 s experienced a lower weight loss of 0.04 and 0.02 g,\n respectively. A similar reduction in weight loss was achieved for 304 SS\n sample when treated for 5, 10, and 20 mins.","PeriodicalId":213647,"journal":{"name":"Analecta Technica Szegedinensia","volume":"53 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2021-12-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"5","resultStr":"{\"title\":\"Corrosion resistance of surface-conditioned 301 and 304 stainless\\n steels by salt spray test\",\"authors\":\"T. Olugbade, B. O. Omiyale\",\"doi\":\"10.14232/analecta.2021.2.9-19\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The corrosion rate of surface-conditioned 301 and 304 stainless\\n steels (SS) was determined by salt spray test in a controlled accelerated\\n corrosive medium (9.5 L of pure distilled water + 500 g NaCl). By surface\\n conditioning via mechanical attrition treatment, a gradient-structured\\n layer was firstly generated on the surface of the samples before the salt\\n spray test. The corrosion rate was determined by the weight loss before and\\n after the salt spray test. Compared to the untreated 301 SS sample with a\\n weight loss of 0.15 g, the surface-conditioned samples treated for 300 s\\n and 1200 s experienced a lower weight loss of 0.04 and 0.02 g,\\n respectively. A similar reduction in weight loss was achieved for 304 SS\\n sample when treated for 5, 10, and 20 mins.\",\"PeriodicalId\":213647,\"journal\":{\"name\":\"Analecta Technica Szegedinensia\",\"volume\":\"53 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2021-12-15\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"5\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Analecta Technica Szegedinensia\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.14232/analecta.2021.2.9-19\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Analecta Technica Szegedinensia","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.14232/analecta.2021.2.9-19","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 5

摘要

采用盐雾试验测定了表面处理301和304不锈钢(SS)在受控加速腐蚀介质(9.5 L纯蒸馏水+ 500 g NaCl)中的腐蚀速率。在盐雾试验前,通过机械摩擦处理的表面调理,首先在试样表面形成梯度结构层。腐蚀速率由盐雾试验前后的失重量决定。与未处理的301 SS样品(失重0.15 g)相比,处理300 s和1200 s的表面处理样品的失重率分别为0.04 g和0.02 g。304 SS样品在处理5分钟、10分钟和20分钟时,重量损失也有类似的减少。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Corrosion resistance of surface-conditioned 301 and 304 stainless steels by salt spray test
The corrosion rate of surface-conditioned 301 and 304 stainless steels (SS) was determined by salt spray test in a controlled accelerated corrosive medium (9.5 L of pure distilled water + 500 g NaCl). By surface conditioning via mechanical attrition treatment, a gradient-structured layer was firstly generated on the surface of the samples before the salt spray test. The corrosion rate was determined by the weight loss before and after the salt spray test. Compared to the untreated 301 SS sample with a weight loss of 0.15 g, the surface-conditioned samples treated for 300 s and 1200 s experienced a lower weight loss of 0.04 and 0.02 g, respectively. A similar reduction in weight loss was achieved for 304 SS sample when treated for 5, 10, and 20 mins.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
The Situation of Freight Transport and Other Logistics Tasks in Laos Dielectric Monitoring of Microwave Extraction Processes Comparative analysis of meat products made from various chicken meat raw material Development of an IoT based 3D printed Mobile Robot Platform for training of Mechatronics Engineering Students Two sample unpaired T-test power calculation using simulation
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1