FCPBGA无铅焊锡球贴附改进及SOP焊盘处理

W. T. Ling, E. P. Leng, N. Amin, I. Ahmad
{"title":"FCPBGA无铅焊锡球贴附改进及SOP焊盘处理","authors":"W. T. Ling, E. P. Leng, N. Amin, I. Ahmad","doi":"10.1109/IEMT.2008.5507837","DOIUrl":null,"url":null,"abstract":"In the recent years, lead-free solder material have been increasingly applied to the green semiconductor products for RoHS compliance. For Flip Chip Plastic Ball Grid Array (FCPBGA), recent industry trend is changing from ENIG pad finishing to Solder-on-pad (SOP) pad finishing using Sn3.0Ag0.5Cu to improve board level reliability due to black pad issue on ENIG pads. However, SOP has posted a challenge in ball attachment process due to higher oxide level on SOP pads. The use of Sn3.8AgO. 7Cu solder ball on SOP pad finishing has been facing slanted ball and wrinkled ball issues after ball attach reflow. Slanted ball is a defect as it fails the solder ball radius-trueposition and coplanarity specification. In this paper, Sn3.5Ag solder ball on 33 × 33 FCPBGA with SOP was being compared to conventional Sn3.8AgO.7Cu solder ball. After assembly, samples were subjected to laser scanning for slanted ball inspection. Visual inspection under low power scope was done to check for wrinkled balls. Cold ball pull (CBP) was used to evaluate the solder joint strength at 3 conditions, namely after assembly (TO), after six time reflow and after 168 hours high temperature storage (HTS). In addition, tray drop test and packing drop test were conducted to assess solder joint integrity due to handling and impact force. Solderability test was also performed per Jedec standard to assess board mounting reliability. Finally, Sn3.5Ag is recommended to replace Sn3.8AgO.7Cu ball for 33 × 33mm FCPBGA package to resolve the wrinkled and slanted ball issue and improve the overall solder joint reliability.","PeriodicalId":151085,"journal":{"name":"2008 33rd IEEE/CPMT International Electronics Manufacturing Technology Conference (IEMT)","volume":"21 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2008-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Lead-free solder ball attach improvement on FCPBGA with SOP pad finishing\",\"authors\":\"W. T. Ling, E. P. Leng, N. Amin, I. Ahmad\",\"doi\":\"10.1109/IEMT.2008.5507837\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In the recent years, lead-free solder material have been increasingly applied to the green semiconductor products for RoHS compliance. For Flip Chip Plastic Ball Grid Array (FCPBGA), recent industry trend is changing from ENIG pad finishing to Solder-on-pad (SOP) pad finishing using Sn3.0Ag0.5Cu to improve board level reliability due to black pad issue on ENIG pads. However, SOP has posted a challenge in ball attachment process due to higher oxide level on SOP pads. The use of Sn3.8AgO. 7Cu solder ball on SOP pad finishing has been facing slanted ball and wrinkled ball issues after ball attach reflow. Slanted ball is a defect as it fails the solder ball radius-trueposition and coplanarity specification. In this paper, Sn3.5Ag solder ball on 33 × 33 FCPBGA with SOP was being compared to conventional Sn3.8AgO.7Cu solder ball. After assembly, samples were subjected to laser scanning for slanted ball inspection. Visual inspection under low power scope was done to check for wrinkled balls. Cold ball pull (CBP) was used to evaluate the solder joint strength at 3 conditions, namely after assembly (TO), after six time reflow and after 168 hours high temperature storage (HTS). In addition, tray drop test and packing drop test were conducted to assess solder joint integrity due to handling and impact force. Solderability test was also performed per Jedec standard to assess board mounting reliability. Finally, Sn3.5Ag is recommended to replace Sn3.8AgO.7Cu ball for 33 × 33mm FCPBGA package to resolve the wrinkled and slanted ball issue and improve the overall solder joint reliability.\",\"PeriodicalId\":151085,\"journal\":{\"name\":\"2008 33rd IEEE/CPMT International Electronics Manufacturing Technology Conference (IEMT)\",\"volume\":\"21 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2008-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2008 33rd IEEE/CPMT International Electronics Manufacturing Technology Conference (IEMT)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/IEMT.2008.5507837\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2008 33rd IEEE/CPMT International Electronics Manufacturing Technology Conference (IEMT)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/IEMT.2008.5507837","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

近年来,无铅焊料越来越多地应用于符合RoHS要求的绿色半导体产品中。对于倒装芯片塑料球栅阵列(FCPBGA),最近的行业趋势是从ENIG焊盘整理转变为使用Sn3.0Ag0.5Cu的焊盘上焊(SOP)焊盘整理,以提高板级可靠性,因为ENIG焊盘上存在黑焊盘问题。然而,由于SOP垫片上的氧化物含量较高,SOP在球的附着过程中遇到了挑战。Sn3.8AgO的使用。铜焊锡球在SOP焊盘整理后一直面临着球倾斜和球起皱的问题。倾斜球是一个缺陷,因为它不符合焊球半径-真实位置和共平面规格。本文对采用SOP的33 × 33 FCPBGA上的Sn3.5Ag焊锡球与常规Sn3.8AgO焊锡球进行了比较。7Cu焊锡球。组装后,样品进行激光扫描进行斜球检查。在低倍镜下目视检查是否有皱球。采用冷球拉法(CBP)对焊点在组装后、6次回流焊后和168 h高温储存后3种条件下的强度进行评价。此外,还进行了托盘跌落试验和填料跌落试验,以评估焊点在搬运和冲击力下的完整性。焊接性测试也按照Jedec标准进行,以评估电路板安装的可靠性。最后推荐Sn3.5Ag代替Sn3.8AgO。7Cu球用于33 × 33mm FCPBGA封装,解决起皱和倾斜球问题,提高整体焊点可靠性。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Lead-free solder ball attach improvement on FCPBGA with SOP pad finishing
In the recent years, lead-free solder material have been increasingly applied to the green semiconductor products for RoHS compliance. For Flip Chip Plastic Ball Grid Array (FCPBGA), recent industry trend is changing from ENIG pad finishing to Solder-on-pad (SOP) pad finishing using Sn3.0Ag0.5Cu to improve board level reliability due to black pad issue on ENIG pads. However, SOP has posted a challenge in ball attachment process due to higher oxide level on SOP pads. The use of Sn3.8AgO. 7Cu solder ball on SOP pad finishing has been facing slanted ball and wrinkled ball issues after ball attach reflow. Slanted ball is a defect as it fails the solder ball radius-trueposition and coplanarity specification. In this paper, Sn3.5Ag solder ball on 33 × 33 FCPBGA with SOP was being compared to conventional Sn3.8AgO.7Cu solder ball. After assembly, samples were subjected to laser scanning for slanted ball inspection. Visual inspection under low power scope was done to check for wrinkled balls. Cold ball pull (CBP) was used to evaluate the solder joint strength at 3 conditions, namely after assembly (TO), after six time reflow and after 168 hours high temperature storage (HTS). In addition, tray drop test and packing drop test were conducted to assess solder joint integrity due to handling and impact force. Solderability test was also performed per Jedec standard to assess board mounting reliability. Finally, Sn3.5Ag is recommended to replace Sn3.8AgO.7Cu ball for 33 × 33mm FCPBGA package to resolve the wrinkled and slanted ball issue and improve the overall solder joint reliability.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Process development and reliability evaluation of Electrically conductive adhesives (ECA) for low temperature SMT assembly Lead-free solder ball attach improvement on FCPBGA with SOP pad finishing High efficiency 850 nm Vertical-Cavity Surface-Emitting Laser using fan-pad metallization and trench patterning A comparison study on SnAgNiCo and Sn3.8Ag0.7Cu C5 lead free solder system Pressure sensors based on MEMS, operating in harsh environments (touch-mode)
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1