{"title":"天然石壳矿渣与化学添加剂对混凝土混合料工艺性能的综合影响研究","authors":"A. Tolegenova, A.S. Espayeva, Z. Altayeva","doi":"10.51488/1680-080x/2023.2-24","DOIUrl":null,"url":null,"abstract":"The influence of saw waste from the extraction of natural shell stone from the Beineu deposit and chemical additives on the preservation of the properties of the concrete mixture is investigated. It was determined that when using the MasterRheobuild 5555 superplasticizer (1.6% of the binder weight or 6.75 kg/m3), the mobility of the concrete mixture is maintained for 2 hours, then its sharp decrease occurs and this is accompanied by a decrease in the volume of entrained air to 16%. The introduction of the Sika ViscoCrete 20HE KZ superplasticizer into the concrete mixture B35 in an amount of 1% of the binder weight or 4.20 kg / m3 prolongs the retention of mobility up to 4 hours 30 minutes and a decrease in the precipitation of the cone is accompanied by a decrease in the initial volume of entrained air to 7%. The research results have shown that in order to increase the preservation of concrete mixtures with superplasticizers, it is necessary first of all to select the components of \"superplasticizer – cement - filler\", which have good compatibility.","PeriodicalId":314558,"journal":{"name":"Bulletin of Kazakh Leading Academy of Architecture and Construction","volume":"15 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-06-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"INVESTIGATION OF THE COMBINED EFFECT OF NATURAL STONE-SHELL MINING WASTE AND CHEMICAL ADDITIVES ON THE TECHNOLOGICAL PROPERTIES OF THE CONCRETE MIXTURE\",\"authors\":\"A. Tolegenova, A.S. Espayeva, Z. Altayeva\",\"doi\":\"10.51488/1680-080x/2023.2-24\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The influence of saw waste from the extraction of natural shell stone from the Beineu deposit and chemical additives on the preservation of the properties of the concrete mixture is investigated. It was determined that when using the MasterRheobuild 5555 superplasticizer (1.6% of the binder weight or 6.75 kg/m3), the mobility of the concrete mixture is maintained for 2 hours, then its sharp decrease occurs and this is accompanied by a decrease in the volume of entrained air to 16%. The introduction of the Sika ViscoCrete 20HE KZ superplasticizer into the concrete mixture B35 in an amount of 1% of the binder weight or 4.20 kg / m3 prolongs the retention of mobility up to 4 hours 30 minutes and a decrease in the precipitation of the cone is accompanied by a decrease in the initial volume of entrained air to 7%. The research results have shown that in order to increase the preservation of concrete mixtures with superplasticizers, it is necessary first of all to select the components of \\\"superplasticizer – cement - filler\\\", which have good compatibility.\",\"PeriodicalId\":314558,\"journal\":{\"name\":\"Bulletin of Kazakh Leading Academy of Architecture and Construction\",\"volume\":\"15 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-06-15\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Bulletin of Kazakh Leading Academy of Architecture and Construction\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.51488/1680-080x/2023.2-24\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Bulletin of Kazakh Leading Academy of Architecture and Construction","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.51488/1680-080x/2023.2-24","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
摘要
研究了贝纽矿开采天然贝壳石锯材废料和化学添加剂对混凝土混合料性能保存的影响。当使用MasterRheobuild 5555高效减水剂(粘结剂重量的1.6%或6.75 kg/m3)时,混凝土混合料的流动性保持2小时,然后流动性急剧下降,同时携带的空气体积减少到16%。在B35混凝土混合料中加入西卡粘胶混凝土20HE KZ高效减水剂,用量为粘结剂重量的1%,即4.20 kg / m3,可延长流动性保持时间达4小时30分钟,锥体沉淀的减少伴随着初始携带空气体积的减少至7%。研究结果表明,为了提高掺有高效减水剂的混凝土配合比的保存性,首先要选择具有良好相容性的“高效减水剂-水泥-填料”组份。
INVESTIGATION OF THE COMBINED EFFECT OF NATURAL STONE-SHELL MINING WASTE AND CHEMICAL ADDITIVES ON THE TECHNOLOGICAL PROPERTIES OF THE CONCRETE MIXTURE
The influence of saw waste from the extraction of natural shell stone from the Beineu deposit and chemical additives on the preservation of the properties of the concrete mixture is investigated. It was determined that when using the MasterRheobuild 5555 superplasticizer (1.6% of the binder weight or 6.75 kg/m3), the mobility of the concrete mixture is maintained for 2 hours, then its sharp decrease occurs and this is accompanied by a decrease in the volume of entrained air to 16%. The introduction of the Sika ViscoCrete 20HE KZ superplasticizer into the concrete mixture B35 in an amount of 1% of the binder weight or 4.20 kg / m3 prolongs the retention of mobility up to 4 hours 30 minutes and a decrease in the precipitation of the cone is accompanied by a decrease in the initial volume of entrained air to 7%. The research results have shown that in order to increase the preservation of concrete mixtures with superplasticizers, it is necessary first of all to select the components of "superplasticizer – cement - filler", which have good compatibility.