{"title":"素面混凝土路面收缩缝“触发”再密封技术综述","authors":"G. Vorobieff","doi":"10.33593/zjpybrnj","DOIUrl":null,"url":null,"abstract":"This paper provides a critical review of the ‘trigger’ to reseal transverse contraction joints in plain concrete pavements given that sealant distress is not uniform along the joint length, traffic management costs are a significant cost, minimising traffic disruption at high volume sites is important, and maintenance funding being limited and directed to ‘safety first’ maintenance activities. In NSW, Australia, all contraction joints are sealed with a highway grade silicone sealant. When sealed with the reservoir clean and dry, the joint sealant should remain in place without cracking for at least 15 years. However, joints sealed incorrectly typically result in early age adhesion failure. Poor joint cleanliness or sealing too early, has been shown to result in seal distress under the wheel paths within the first 2 years. It is also common for the sealant to become distressed in the slow (outer) lane while the sealant is in satisfactory condition in the fast (inner) lane. Recommendations for an interim empirical procedure are provided to assist asset managers evaluate the ‘triggers’ for resealing existing joints. The recommendations are based on the age of the pavement and incorporate: (a) Simplified definition for sealant defect, (b) Implementation of a random inspection technique to determine the extent of seal distress and more informed decision making on contraction joints to be resealed, and (c) The extent of resealing in a transverse joint over multiple lanes.","PeriodicalId":265129,"journal":{"name":"Proceedings of the 12th International Conference on Concrete Pavements","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2021-12-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"A review of the ``trigger'' to reseal contraction joints in plain concrete pavements\",\"authors\":\"G. Vorobieff\",\"doi\":\"10.33593/zjpybrnj\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"This paper provides a critical review of the ‘trigger’ to reseal transverse contraction joints in plain concrete pavements given that sealant distress is not uniform along the joint length, traffic management costs are a significant cost, minimising traffic disruption at high volume sites is important, and maintenance funding being limited and directed to ‘safety first’ maintenance activities. In NSW, Australia, all contraction joints are sealed with a highway grade silicone sealant. When sealed with the reservoir clean and dry, the joint sealant should remain in place without cracking for at least 15 years. However, joints sealed incorrectly typically result in early age adhesion failure. Poor joint cleanliness or sealing too early, has been shown to result in seal distress under the wheel paths within the first 2 years. It is also common for the sealant to become distressed in the slow (outer) lane while the sealant is in satisfactory condition in the fast (inner) lane. Recommendations for an interim empirical procedure are provided to assist asset managers evaluate the ‘triggers’ for resealing existing joints. The recommendations are based on the age of the pavement and incorporate: (a) Simplified definition for sealant defect, (b) Implementation of a random inspection technique to determine the extent of seal distress and more informed decision making on contraction joints to be resealed, and (c) The extent of resealing in a transverse joint over multiple lanes.\",\"PeriodicalId\":265129,\"journal\":{\"name\":\"Proceedings of the 12th International Conference on Concrete Pavements\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2021-12-31\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Proceedings of the 12th International Conference on Concrete Pavements\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.33593/zjpybrnj\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Proceedings of the 12th International Conference on Concrete Pavements","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.33593/zjpybrnj","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

本文对平原混凝土路面横向收缩缝重新密封的“触发因素”进行了关键审查,因为密封胶沿接缝长度不均匀,交通管理成本是重大成本,最大限度地减少高容量站点的交通中断是重要的,维护资金有限,并直接用于“安全第一”的维护活动。在新南威尔士州,澳大利亚,所有收缩接头密封与公路级硅胶密封胶。当与水库清洁和干燥密封时,接缝密封胶应保持在原地不开裂至少15年。然而,关节密封不正确通常会导致早期粘连失败。接缝清洁度差或过早密封,已被证明会在头2年内导致轮径下的密封窘迫。当密封胶在快速车道(内车道)状态良好时,在慢速车道(外车道)密封胶出现破损的情况也很常见。提供了临时经验程序的建议,以帮助资产管理公司评估重新密封现有接头的“触发因素”。这些建议是基于路面的年龄,包括:(a)对密封胶缺陷的简化定义,(b)实施随机检查技术,以确定密封损坏的程度,并对需要重新密封的收缩缝做出更明智的决策,以及(c)多车道横向接缝的重新密封程度。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
A review of the ``trigger'' to reseal contraction joints in plain concrete pavements
This paper provides a critical review of the ‘trigger’ to reseal transverse contraction joints in plain concrete pavements given that sealant distress is not uniform along the joint length, traffic management costs are a significant cost, minimising traffic disruption at high volume sites is important, and maintenance funding being limited and directed to ‘safety first’ maintenance activities. In NSW, Australia, all contraction joints are sealed with a highway grade silicone sealant. When sealed with the reservoir clean and dry, the joint sealant should remain in place without cracking for at least 15 years. However, joints sealed incorrectly typically result in early age adhesion failure. Poor joint cleanliness or sealing too early, has been shown to result in seal distress under the wheel paths within the first 2 years. It is also common for the sealant to become distressed in the slow (outer) lane while the sealant is in satisfactory condition in the fast (inner) lane. Recommendations for an interim empirical procedure are provided to assist asset managers evaluate the ‘triggers’ for resealing existing joints. The recommendations are based on the age of the pavement and incorporate: (a) Simplified definition for sealant defect, (b) Implementation of a random inspection technique to determine the extent of seal distress and more informed decision making on contraction joints to be resealed, and (c) The extent of resealing in a transverse joint over multiple lanes.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Sensitivity Analysis of FAARFIELD Rigid Airport Pavement Thickness Determination Guidance for Increasing the Use of Recycled Concrete Pavement Materials Performance Summary Of Precast Concrete Inlay Panel Trial In Ontario Validation Of A New Method For Determining The Remaining Service Life Of Rigid Pavements Impacts Of Flooding On Concrete Pavement
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1