温度作用和初始间隙损伤下中国轨道系统界面行为分析Ⅱ平板无砟轨道

Jun Wang, Zhao-Hui Lu, Xuan-Yi Zhang, Yan-Gang Zhao
{"title":"温度作用和初始间隙损伤下中国轨道系统界面行为分析Ⅱ平板无砟轨道","authors":"Jun Wang, Zhao-Hui Lu, Xuan-Yi Zhang, Yan-Gang Zhao","doi":"10.1177/09544097231194679","DOIUrl":null,"url":null,"abstract":"The interface damage is considered to be one of the main diseases of China Railway Track System (CRTS) Ⅱ slab ballastless track, which will affect the long-term performance of the track structure and safety operation of high-speed trains. This study aims to reveal the interface damage mechanism between the track slab and the cement asphalt (CA) mortar layer of CRTS Ⅱ slab ballastless track, under different combinations of temperature actions and initial gap damage. A three-dimensional finite element model of CRTS Ⅱ slab ballastless track was established, in which a cohesive constitutive model was incorporated to simulate the interaction behavior of the interface. The interface damage evolution under different temperature actions and initial gap damage was analyzed. The analysis results show that: (1) Overall temperature has a more obvious effect on interface damage compared with temperature gradient, and the greater the overall temperature drops, the lower the decrease of interface damage will be; (2) When initial gap damage occur at the slab end, the growth rate of interface damage under temperature gradient is greater than that under overall temperature; The interface will begin to delaminate when the overall temperature drop reaches −50°C and the gap length becomes greater than one fastener spacing; and (3) When initial gap damage occur at the slab edge, the influence of overall temperature on interface damage is greater than that of temperature gradient; The interface gap damage reaches level II (according to TG/GW 115-2012) at the slab edge under the combination of −50°C and −50°C/m, while the slab center interface is unlikely to be damaged under negative temperature.","PeriodicalId":54567,"journal":{"name":"Proceedings of the Institution of Mechanical Engineers Part F-Journal of Rail and Rapid Transit","volume":null,"pages":null},"PeriodicalIF":1.7000,"publicationDate":"2023-11-02","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Interface behaviour analysis of China railway track system Ⅱ slab ballastless track under temperature action and initial gap damage\",\"authors\":\"Jun Wang, Zhao-Hui Lu, Xuan-Yi Zhang, Yan-Gang Zhao\",\"doi\":\"10.1177/09544097231194679\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The interface damage is considered to be one of the main diseases of China Railway Track System (CRTS) Ⅱ slab ballastless track, which will affect the long-term performance of the track structure and safety operation of high-speed trains. This study aims to reveal the interface damage mechanism between the track slab and the cement asphalt (CA) mortar layer of CRTS Ⅱ slab ballastless track, under different combinations of temperature actions and initial gap damage. A three-dimensional finite element model of CRTS Ⅱ slab ballastless track was established, in which a cohesive constitutive model was incorporated to simulate the interaction behavior of the interface. The interface damage evolution under different temperature actions and initial gap damage was analyzed. The analysis results show that: (1) Overall temperature has a more obvious effect on interface damage compared with temperature gradient, and the greater the overall temperature drops, the lower the decrease of interface damage will be; (2) When initial gap damage occur at the slab end, the growth rate of interface damage under temperature gradient is greater than that under overall temperature; The interface will begin to delaminate when the overall temperature drop reaches −50°C and the gap length becomes greater than one fastener spacing; and (3) When initial gap damage occur at the slab edge, the influence of overall temperature on interface damage is greater than that of temperature gradient; The interface gap damage reaches level II (according to TG/GW 115-2012) at the slab edge under the combination of −50°C and −50°C/m, while the slab center interface is unlikely to be damaged under negative temperature.\",\"PeriodicalId\":54567,\"journal\":{\"name\":\"Proceedings of the Institution of Mechanical Engineers Part F-Journal of Rail and Rapid Transit\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":1.7000,\"publicationDate\":\"2023-11-02\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Proceedings of the Institution of Mechanical Engineers Part F-Journal of Rail and Rapid Transit\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1177/09544097231194679\",\"RegionNum\":4,\"RegionCategory\":\"工程技术\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"ENGINEERING, CIVIL\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Proceedings of the Institution of Mechanical Engineers Part F-Journal of Rail and Rapid Transit","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1177/09544097231194679","RegionNum":4,"RegionCategory":"工程技术","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"ENGINEERING, CIVIL","Score":null,"Total":0}
引用次数: 0

摘要

界面损伤被认为是中国铁路轨道系统(CRTS)Ⅱ平板无砟轨道的主要病害之一,将影响轨道结构的长期性能和高速列车的安全运行。本研究旨在揭示CRTSⅡ板式无砟轨道在不同温度作用和初始间隙损伤组合下,轨道板与水泥沥青砂浆层界面损伤机理。建立了CRTSⅡ平板无砟轨道三维有限元模型,采用内聚本构模型模拟界面相互作用行为。分析了不同温度作用下界面损伤的演化过程和初始间隙损伤。分析结果表明:(1)与温度梯度相比,整体温度对界面损伤的影响更为明显,整体温度降得越大,界面损伤的降幅越小;(2)初始间隙损伤发生在板坯端部时,温度梯度下界面损伤的增长速度大于整体温度下的增长速度;当整体温度降至- 50℃且间隙长度大于1个紧固件间距时,界面开始分层;(3)当坯边出现初始间隙损伤时,整体温度对界面损伤的影响大于温度梯度的影响;在- 50℃和- 50℃/m组合下,板坯边缘界面间隙损伤达到II级(根据TG/GW 115-2012),而板坯中心界面在负温度下不太可能出现损伤。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Interface behaviour analysis of China railway track system Ⅱ slab ballastless track under temperature action and initial gap damage
The interface damage is considered to be one of the main diseases of China Railway Track System (CRTS) Ⅱ slab ballastless track, which will affect the long-term performance of the track structure and safety operation of high-speed trains. This study aims to reveal the interface damage mechanism between the track slab and the cement asphalt (CA) mortar layer of CRTS Ⅱ slab ballastless track, under different combinations of temperature actions and initial gap damage. A three-dimensional finite element model of CRTS Ⅱ slab ballastless track was established, in which a cohesive constitutive model was incorporated to simulate the interaction behavior of the interface. The interface damage evolution under different temperature actions and initial gap damage was analyzed. The analysis results show that: (1) Overall temperature has a more obvious effect on interface damage compared with temperature gradient, and the greater the overall temperature drops, the lower the decrease of interface damage will be; (2) When initial gap damage occur at the slab end, the growth rate of interface damage under temperature gradient is greater than that under overall temperature; The interface will begin to delaminate when the overall temperature drop reaches −50°C and the gap length becomes greater than one fastener spacing; and (3) When initial gap damage occur at the slab edge, the influence of overall temperature on interface damage is greater than that of temperature gradient; The interface gap damage reaches level II (according to TG/GW 115-2012) at the slab edge under the combination of −50°C and −50°C/m, while the slab center interface is unlikely to be damaged under negative temperature.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
4.80
自引率
10.00%
发文量
91
审稿时长
7 months
期刊介绍: The Journal of Rail and Rapid Transit is devoted to engineering in its widest interpretation applicable to rail and rapid transit. The Journal aims to promote sharing of technical knowledge, ideas and experience between engineers and researchers working in the railway field.
期刊最新文献
The influence of semi-actively controlled magnetorheological bogie yaw dampers on the guiding behaviour of a railway vehicle in an S-curve: Simulation and on-track test Mechanism and improvement for tail vehicle swaying of power-centralized EMUs Long railway track modelling – A parallel computing approach Research on ultrasonic guided wave-based high-speed turnout switch rail base flaw detection Ballast stiffness estimation based on measurements during dynamic track stabilization
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1