O. L. Semenova, O. S. Fomichov, K. A. Meleshevich, V. M. Talash, Yu.B. Rudenko
{"title":"Ni-Sc-Zr三元合金沿77.8 at的相互作用。% Ni切片。合金的电化学性能","authors":"O. L. Semenova, O. S. Fomichov, K. A. Meleshevich, V. M. Talash, Yu.B. Rudenko","doi":"10.1007/s11106-023-00388-z","DOIUrl":null,"url":null,"abstract":"<p>The interaction of Sc<sub>2</sub>Ni<sub>7</sub> and Zr<sub>2</sub>Ni<sub>7</sub> compounds (with C2/m and P6<sub>3</sub>/mmc crystal structures and congruent melting temperatures of 1270 and 1438°C) in the ternary Ni–Sc–Zr system was studied employing physicochemical analysis methods (metallography, X-ray diffraction, differential thermal analysis, and electron microprobe analysis). The section between the compounds was shown to be quasibinary of peritectic type, with peritectic points of 1340 ± 13°C and 14 at.% Sc. At the peritectic temperature, about 10 at.% Zr dissolves in the Sc<sub>2</sub>Ni<sub>7</sub>-based phase and about 8 at.% Sc in the Zr<sub>2</sub>Ni<sub>7</sub>-based phase. Electrochemical studies conducted through cathodic polarization of the ternary Sc<sub>2</sub>Ni<sub>7</sub> and Zr<sub>2</sub>Ni<sub>7</sub> alloys using a PI-50-1 potentiostat, with a three-electrode electrochemical cell consisting of a working ceramic anode, a platinum cathode, an electrolyte (a 3% NaCl aqueous solution), and a silver chloride Ag/AgCl/KCl reference electrode, did not reveal any tendency to hydrogenation in their solid solutions. The influence of preliminary cathodic reduction of the 77.8 at.% Ni–8 at.% Sc–Zr sample on its subsequent anodic dissolution was determined. The initial surface of the 77.8 at.% Ni–8 at.% Sc–Zr sample was found to be much more resistant to anodic oxidation than the surface preliminary subjected to cathodic reduction because of a significant decrease in its oxide component.</p>","PeriodicalId":742,"journal":{"name":"Powder Metallurgy and Metal Ceramics","volume":"62 3-4","pages":"241 - 249"},"PeriodicalIF":0.9000,"publicationDate":"2023-11-17","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Interaction in the Ni–Sc–Zr Ternary Alloys Along the 77.8 at.% Ni Section. Electrochemical Properties of the Alloys\",\"authors\":\"O. L. Semenova, O. S. Fomichov, K. A. Meleshevich, V. M. Talash, Yu.B. Rudenko\",\"doi\":\"10.1007/s11106-023-00388-z\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The interaction of Sc<sub>2</sub>Ni<sub>7</sub> and Zr<sub>2</sub>Ni<sub>7</sub> compounds (with C2/m and P6<sub>3</sub>/mmc crystal structures and congruent melting temperatures of 1270 and 1438°C) in the ternary Ni–Sc–Zr system was studied employing physicochemical analysis methods (metallography, X-ray diffraction, differential thermal analysis, and electron microprobe analysis). The section between the compounds was shown to be quasibinary of peritectic type, with peritectic points of 1340 ± 13°C and 14 at.% Sc. At the peritectic temperature, about 10 at.% Zr dissolves in the Sc<sub>2</sub>Ni<sub>7</sub>-based phase and about 8 at.% Sc in the Zr<sub>2</sub>Ni<sub>7</sub>-based phase. Electrochemical studies conducted through cathodic polarization of the ternary Sc<sub>2</sub>Ni<sub>7</sub> and Zr<sub>2</sub>Ni<sub>7</sub> alloys using a PI-50-1 potentiostat, with a three-electrode electrochemical cell consisting of a working ceramic anode, a platinum cathode, an electrolyte (a 3% NaCl aqueous solution), and a silver chloride Ag/AgCl/KCl reference electrode, did not reveal any tendency to hydrogenation in their solid solutions. The influence of preliminary cathodic reduction of the 77.8 at.% Ni–8 at.% Sc–Zr sample on its subsequent anodic dissolution was determined. The initial surface of the 77.8 at.% Ni–8 at.% Sc–Zr sample was found to be much more resistant to anodic oxidation than the surface preliminary subjected to cathodic reduction because of a significant decrease in its oxide component.</p>\",\"PeriodicalId\":742,\"journal\":{\"name\":\"Powder Metallurgy and Metal Ceramics\",\"volume\":\"62 3-4\",\"pages\":\"241 - 249\"},\"PeriodicalIF\":0.9000,\"publicationDate\":\"2023-11-17\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Powder Metallurgy and Metal Ceramics\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://link.springer.com/article/10.1007/s11106-023-00388-z\",\"RegionNum\":4,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"MATERIALS SCIENCE, CERAMICS\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Powder Metallurgy and Metal Ceramics","FirstCategoryId":"88","ListUrlMain":"https://link.springer.com/article/10.1007/s11106-023-00388-z","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
Interaction in the Ni–Sc–Zr Ternary Alloys Along the 77.8 at.% Ni Section. Electrochemical Properties of the Alloys
The interaction of Sc2Ni7 and Zr2Ni7 compounds (with C2/m and P63/mmc crystal structures and congruent melting temperatures of 1270 and 1438°C) in the ternary Ni–Sc–Zr system was studied employing physicochemical analysis methods (metallography, X-ray diffraction, differential thermal analysis, and electron microprobe analysis). The section between the compounds was shown to be quasibinary of peritectic type, with peritectic points of 1340 ± 13°C and 14 at.% Sc. At the peritectic temperature, about 10 at.% Zr dissolves in the Sc2Ni7-based phase and about 8 at.% Sc in the Zr2Ni7-based phase. Electrochemical studies conducted through cathodic polarization of the ternary Sc2Ni7 and Zr2Ni7 alloys using a PI-50-1 potentiostat, with a three-electrode electrochemical cell consisting of a working ceramic anode, a platinum cathode, an electrolyte (a 3% NaCl aqueous solution), and a silver chloride Ag/AgCl/KCl reference electrode, did not reveal any tendency to hydrogenation in their solid solutions. The influence of preliminary cathodic reduction of the 77.8 at.% Ni–8 at.% Sc–Zr sample on its subsequent anodic dissolution was determined. The initial surface of the 77.8 at.% Ni–8 at.% Sc–Zr sample was found to be much more resistant to anodic oxidation than the surface preliminary subjected to cathodic reduction because of a significant decrease in its oxide component.
期刊介绍:
Powder Metallurgy and Metal Ceramics covers topics of the theory, manufacturing technology, and properties of powder; technology of forming processes; the technology of sintering, heat treatment, and thermo-chemical treatment; properties of sintered materials; and testing methods.