{"title":"将钛以金属箔的形式用于摩擦非金属材料,以润湿这些材料并用金属焊料进行焊接","authors":"V. S. Zhuravlev, V. P. Krasovskyy","doi":"10.15407/materials2023.07.007","DOIUrl":null,"url":null,"abstract":"Activation of filler metal alloys for brazing non-metals by introducing chemically active elements such as titanium, zirconium, etc. is a technically challenging task. This paper discusses some methods of brazing non-metallic materials with filler metal alloys. A brief review of publications on the metallisation of non-metallic materials by titanium friction for further brazing with filler metal alloys is given. Two types of titanium foil tools for friction coatings on non-metallic materials have been proposed and used, which, in comparison with friction with compact titanium, significantly reduce the destruction of the ceramic surface and facilitate their application. Samples of high-alumina ceramics A995 and WK94-1, were metallized by the proposed method. The wetting of ceramics coated with PSr72 filler alloy (copper-silver eutectic) was studied, brazed joints were obtained, and the microstructure of the metal-nonmetal contact zone was studied The main purpose of such a coating for brazing processes is to activate the filler metal alloys melt to wet the ceramic. The surface roughness of non-metals affects the microstructure of the applied coating. As the roughness decreases, the density of the coating increases. Studies of the microstructure of the brazed joint have shown that the PSr72 melt penetrates the titanium coating, saturates it with titanium and wets the ceramic. This means that such metallisation accelerates the saturation of the melt with titanium. The brazing modes of this method practically coincide with the brazing modes of titanium-containing filler metal alloys Using the method of friction the metallization layer reduces the cost of the brazing process. Keywords: rubbing with metals, titanium foil, soldering of ceramics, metal solders, microstructure.","PeriodicalId":509971,"journal":{"name":"Uspihi materialoznavstva","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2023-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"The use of titanium in the form of a foil for rubbing non-metallic materials with the purpose of wetting them and soldering them with metal solders\",\"authors\":\"V. S. Zhuravlev, V. P. Krasovskyy\",\"doi\":\"10.15407/materials2023.07.007\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Activation of filler metal alloys for brazing non-metals by introducing chemically active elements such as titanium, zirconium, etc. is a technically challenging task. This paper discusses some methods of brazing non-metallic materials with filler metal alloys. A brief review of publications on the metallisation of non-metallic materials by titanium friction for further brazing with filler metal alloys is given. Two types of titanium foil tools for friction coatings on non-metallic materials have been proposed and used, which, in comparison with friction with compact titanium, significantly reduce the destruction of the ceramic surface and facilitate their application. Samples of high-alumina ceramics A995 and WK94-1, were metallized by the proposed method. The wetting of ceramics coated with PSr72 filler alloy (copper-silver eutectic) was studied, brazed joints were obtained, and the microstructure of the metal-nonmetal contact zone was studied The main purpose of such a coating for brazing processes is to activate the filler metal alloys melt to wet the ceramic. The surface roughness of non-metals affects the microstructure of the applied coating. As the roughness decreases, the density of the coating increases. Studies of the microstructure of the brazed joint have shown that the PSr72 melt penetrates the titanium coating, saturates it with titanium and wets the ceramic. This means that such metallisation accelerates the saturation of the melt with titanium. The brazing modes of this method practically coincide with the brazing modes of titanium-containing filler metal alloys Using the method of friction the metallization layer reduces the cost of the brazing process. Keywords: rubbing with metals, titanium foil, soldering of ceramics, metal solders, microstructure.\",\"PeriodicalId\":509971,\"journal\":{\"name\":\"Uspihi materialoznavstva\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Uspihi materialoznavstva\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.15407/materials2023.07.007\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Uspihi materialoznavstva","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15407/materials2023.07.007","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

通过引入钛、锆等化学活性元素来活化用于非金属钎焊的填充金属合金是一项具有技术挑战性的任务。本文讨论了用填充金属合金钎焊非金属材料的一些方法。本文简要回顾了有关通过钛摩擦使非金属材料金属化并与填充金属合金进一步钎焊的出版物。提出并使用了两种用于在非金属材料上摩擦涂层的钛箔工具,与紧凑型钛摩擦相比,这两种工具大大减少了对陶瓷表面的破坏,便于应用。用提出的方法对高铝陶瓷 A995 和 WK94-1 样品进行了金属化处理。研究了涂有 PSr72 填充合金(铜银共晶)的陶瓷的润湿性,获得了钎焊接头,并研究了金属-非金属接触区的微观结构。非金属的表面粗糙度会影响涂层的微观结构。随着粗糙度的降低,涂层的密度也会增加。对钎焊接头微观结构的研究表明,PSr72 熔体可穿透钛涂层,使钛饱和并润湿陶瓷。这意味着这种金属化加速了熔体与钛的饱和。这种方法的钎焊模式实际上与含钛填充金属合金的钎焊模式相吻合 使用摩擦金属化层的方法可降低钎焊工艺的成本。关键词:金属摩擦、钛箔、陶瓷焊接、金属焊料、微观结构。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
The use of titanium in the form of a foil for rubbing non-metallic materials with the purpose of wetting them and soldering them with metal solders
Activation of filler metal alloys for brazing non-metals by introducing chemically active elements such as titanium, zirconium, etc. is a technically challenging task. This paper discusses some methods of brazing non-metallic materials with filler metal alloys. A brief review of publications on the metallisation of non-metallic materials by titanium friction for further brazing with filler metal alloys is given. Two types of titanium foil tools for friction coatings on non-metallic materials have been proposed and used, which, in comparison with friction with compact titanium, significantly reduce the destruction of the ceramic surface and facilitate their application. Samples of high-alumina ceramics A995 and WK94-1, were metallized by the proposed method. The wetting of ceramics coated with PSr72 filler alloy (copper-silver eutectic) was studied, brazed joints were obtained, and the microstructure of the metal-nonmetal contact zone was studied The main purpose of such a coating for brazing processes is to activate the filler metal alloys melt to wet the ceramic. The surface roughness of non-metals affects the microstructure of the applied coating. As the roughness decreases, the density of the coating increases. Studies of the microstructure of the brazed joint have shown that the PSr72 melt penetrates the titanium coating, saturates it with titanium and wets the ceramic. This means that such metallisation accelerates the saturation of the melt with titanium. The brazing modes of this method practically coincide with the brazing modes of titanium-containing filler metal alloys Using the method of friction the metallization layer reduces the cost of the brazing process. Keywords: rubbing with metals, titanium foil, soldering of ceramics, metal solders, microstructure.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Low-temperature phase stability of ceramics in the ZrO2—Y2O3—CeO2 system produced after heat treatment of the starting powders at 850 °C Wetting and contact interaction of semconductor oxide materials Ga2O3, In2O3, ZnO with metallic melts in vacuum ZrB2 ceramics with MoSi2, SiC and B4C additives: compaction kinetics, phase formation and creep resistance Hypothetical CeO2—Ln2O3 phase diagrams (Ln = yttrium lanthanides, Y2O3) The use of titanium in the form of a foil for rubbing non-metallic materials with the purpose of wetting them and soldering them with metal solders
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1