Clara Schlereth, Emma M. H. White, Maren Lepple, Benedikt Nowak, Heike Hattendorf, Mathias C. Galetz
{"title":"封面图片:材料与腐蚀》。3/2024","authors":"Clara Schlereth, Emma M. H. White, Maren Lepple, Benedikt Nowak, Heike Hattendorf, Mathias C. Galetz","doi":"10.1002/maco.202470031","DOIUrl":null,"url":null,"abstract":"<p><b>Cover:</b></p><p>Electron backscatter diffraction (EBSD) images of steel shot peened Ni-base alloy 699 XA after 480 h exposure in a carbon-rich gas at 620 °C and 19 bar. From left to right: secondary electron image, color coded using an inverse pole figure, and color coded by crystal structure. During high temperature exposure, α-Cr (BCC) precipitates formed in the highly deformed nearsurface zone. Images by Melanie Thalheimer.</p><p>More detailed information can be found in: <i>Clara Schlereth, Emma Marie Hamilton White, Maren Lepple, Benedikt Nowak, Heike Hattendorf, Mathias Christian Galetz</i>, Influence of the surface treatment on the metal dusting resistance of welds, <i>Materials and Corrosion</i> <b>2024</b>, <i>75</i>, 371.\n\n <figure>\n <div><picture>\n <source></source></picture><p></p>\n </div>\n </figure></p>","PeriodicalId":18225,"journal":{"name":"Materials and Corrosion-werkstoffe Und Korrosion","volume":"75 3","pages":"283"},"PeriodicalIF":1.6000,"publicationDate":"2024-02-29","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://onlinelibrary.wiley.com/doi/epdf/10.1002/maco.202470031","citationCount":"0","resultStr":"{\"title\":\"Cover Picture: Materials and Corrosion. 3/2024\",\"authors\":\"Clara Schlereth, Emma M. H. White, Maren Lepple, Benedikt Nowak, Heike Hattendorf, Mathias C. Galetz\",\"doi\":\"10.1002/maco.202470031\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><b>Cover:</b></p><p>Electron backscatter diffraction (EBSD) images of steel shot peened Ni-base alloy 699 XA after 480 h exposure in a carbon-rich gas at 620 °C and 19 bar. From left to right: secondary electron image, color coded using an inverse pole figure, and color coded by crystal structure. During high temperature exposure, α-Cr (BCC) precipitates formed in the highly deformed nearsurface zone. Images by Melanie Thalheimer.</p><p>More detailed information can be found in: <i>Clara Schlereth, Emma Marie Hamilton White, Maren Lepple, Benedikt Nowak, Heike Hattendorf, Mathias Christian Galetz</i>, Influence of the surface treatment on the metal dusting resistance of welds, <i>Materials and Corrosion</i> <b>2024</b>, <i>75</i>, 371.\\n\\n <figure>\\n <div><picture>\\n <source></source></picture><p></p>\\n </div>\\n </figure></p>\",\"PeriodicalId\":18225,\"journal\":{\"name\":\"Materials and Corrosion-werkstoffe Und Korrosion\",\"volume\":\"75 3\",\"pages\":\"283\"},\"PeriodicalIF\":1.6000,\"publicationDate\":\"2024-02-29\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://onlinelibrary.wiley.com/doi/epdf/10.1002/maco.202470031\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Materials and Corrosion-werkstoffe Und Korrosion\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://onlinelibrary.wiley.com/doi/10.1002/maco.202470031\",\"RegionNum\":4,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"MATERIALS SCIENCE, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials and Corrosion-werkstoffe Und Korrosion","FirstCategoryId":"88","ListUrlMain":"https://onlinelibrary.wiley.com/doi/10.1002/maco.202470031","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0
摘要
封面:在 620 °C 和 19 巴的富碳气体中暴露 480 小时后,钢丸强化镍基合金 699 XA 的电子反向散射衍射 (EBSD) 图像。从左至右:二次电子图像、使用反极点图进行的颜色编码以及根据晶体结构进行的颜色编码。高温暴露期间,α-Cr(BCC)沉淀物在高度变形的近表面区域形成。图片由 Melanie Thalheimer 提供:Clara Schlereth、Emma Marie Hamilton White、Maren Lepple、Benedikt Nowak、Heike Hattendorf、Mathias Christian Galetz,《表面处理对焊缝抗金属粉尘性的影响》,《材料与腐蚀》2024 年第 75 期,371 页。
Electron backscatter diffraction (EBSD) images of steel shot peened Ni-base alloy 699 XA after 480 h exposure in a carbon-rich gas at 620 °C and 19 bar. From left to right: secondary electron image, color coded using an inverse pole figure, and color coded by crystal structure. During high temperature exposure, α-Cr (BCC) precipitates formed in the highly deformed nearsurface zone. Images by Melanie Thalheimer.
More detailed information can be found in: Clara Schlereth, Emma Marie Hamilton White, Maren Lepple, Benedikt Nowak, Heike Hattendorf, Mathias Christian Galetz, Influence of the surface treatment on the metal dusting resistance of welds, Materials and Corrosion2024, 75, 371.
期刊介绍:
Materials and Corrosion is the leading European journal in its field, providing rapid and comprehensive coverage of the subject and specifically highlighting the increasing importance of corrosion research and prevention.
Several sections exclusive to Materials and Corrosion bring you closer to the current events in the field of corrosion research and add to the impact this journal can make on your work.