牙本质替代材料释放单体的评估

IF 3.4 4区 化学 Q2 POLYMER SCIENCE International Journal of Polymer Science Pub Date : 2024-03-12 DOI:10.1155/2024/9350118
Nurgül Çetin Tuncer, Sevde Gül Batmaz, Sergen Özdemir, Çağatay Barutçugil, Ayşe Dündar, Kardelen Yıldırım
{"title":"牙本质替代材料释放单体的评估","authors":"Nurgül Çetin Tuncer, Sevde Gül Batmaz, Sergen Özdemir, Çağatay Barutçugil, Ayşe Dündar, Kardelen Yıldırım","doi":"10.1155/2024/9350118","DOIUrl":null,"url":null,"abstract":"The aim of this study is to determine and quantify the monomer elution from four different resin-based composite dentin replacement materials for 3 months using HPLC. Four different composite dentin replacement materials were used in the present study: EverX (EVX), X-tra base (XTB), SDR (SDR), and GrandioSO Heavy Flow (GHF). Fifteen samples from each material were prepared (<span><svg height=\"8.69875pt\" style=\"vertical-align:-0.3499298pt\" version=\"1.1\" viewbox=\"-0.0498162 -8.34882 16.777 8.69875\" width=\"16.777pt\" xmlns=\"http://www.w3.org/2000/svg\" xmlns:xlink=\"http://www.w3.org/1999/xlink\"><g transform=\"matrix(.013,0,0,-0.013,0,0)\"></path></g><g transform=\"matrix(.013,0,0,-0.013,9.146,0)\"></path></g></svg><span></span><svg height=\"8.69875pt\" style=\"vertical-align:-0.3499298pt\" version=\"1.1\" viewbox=\"19.6321838 -8.34882 16.777 8.69875\" width=\"16.777pt\" xmlns=\"http://www.w3.org/2000/svg\" xmlns:xlink=\"http://www.w3.org/1999/xlink\"><g transform=\"matrix(.013,0,0,-0.013,19.682,0)\"><use xlink:href=\"#g113-54\"></use></g><g transform=\"matrix(.013,0,0,-0.013,28.828,0)\"><use xlink:href=\"#g117-42\"></use></g></svg><span></span><svg height=\"8.69875pt\" style=\"vertical-align:-0.3499298pt\" version=\"1.1\" viewbox=\"39.314183799999995 -8.34882 6.467 8.69875\" width=\"6.467pt\" xmlns=\"http://www.w3.org/2000/svg\" xmlns:xlink=\"http://www.w3.org/1999/xlink\"><g transform=\"matrix(.013,0,0,-0.013,39.364,0)\"></path></g></svg></span> mm). After preparation, each specimen was immersed in a 10 ml 75% ethanol/distilled water solution for three different periods: 1 h, 24 h, and 3 months (<span><svg height=\"8.32035pt\" style=\"vertical-align:-0.2063999pt\" version=\"1.1\" viewbox=\"-0.0498162 -8.11395 17.789 8.32035\" width=\"17.789pt\" xmlns=\"http://www.w3.org/2000/svg\" xmlns:xlink=\"http://www.w3.org/1999/xlink\"><g transform=\"matrix(.013,0,0,-0.013,0,0)\"></path></g><g transform=\"matrix(.013,0,0,-0.013,10.158,0)\"></path></g></svg><span></span><span><svg height=\"8.32035pt\" style=\"vertical-align:-0.2063999pt\" version=\"1.1\" viewbox=\"21.3711838 -8.11395 6.416 8.32035\" width=\"6.416pt\" xmlns=\"http://www.w3.org/2000/svg\" xmlns:xlink=\"http://www.w3.org/1999/xlink\"><g transform=\"matrix(.013,0,0,-0.013,21.421,0)\"><use xlink:href=\"#g113-54\"></use></g></svg>).</span></span> After the immersion period, 0.5 ml of solutions were taken from each bottle and analyzed using HPLC. At the end of the 3-month immersion period, the elution of monomers was determined mostly from SDR, GHF, EVX, and XTB, respectively. TEGDMA, the most released monomer of all groups, was released from all samples after 1 h, 24 h, and 3 months. The amount of monomer released in all composite groups at the end of the 3-month immersion period was significantly higher than the monomer amounts released after the 1-hour immersion period. The monomers were eluted from the composite dentin replacement materials during all immersion periods, and the amount of eluted monomers was increased with time.","PeriodicalId":14283,"journal":{"name":"International Journal of Polymer Science","volume":null,"pages":null},"PeriodicalIF":3.4000,"publicationDate":"2024-03-12","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Evaluation of Monomer Releasing from Dentin Replacement Materials\",\"authors\":\"Nurgül Çetin Tuncer, Sevde Gül Batmaz, Sergen Özdemir, Çağatay Barutçugil, Ayşe Dündar, Kardelen Yıldırım\",\"doi\":\"10.1155/2024/9350118\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The aim of this study is to determine and quantify the monomer elution from four different resin-based composite dentin replacement materials for 3 months using HPLC. Four different composite dentin replacement materials were used in the present study: EverX (EVX), X-tra base (XTB), SDR (SDR), and GrandioSO Heavy Flow (GHF). Fifteen samples from each material were prepared (<span><svg height=\\\"8.69875pt\\\" style=\\\"vertical-align:-0.3499298pt\\\" version=\\\"1.1\\\" viewbox=\\\"-0.0498162 -8.34882 16.777 8.69875\\\" width=\\\"16.777pt\\\" xmlns=\\\"http://www.w3.org/2000/svg\\\" xmlns:xlink=\\\"http://www.w3.org/1999/xlink\\\"><g transform=\\\"matrix(.013,0,0,-0.013,0,0)\\\"></path></g><g transform=\\\"matrix(.013,0,0,-0.013,9.146,0)\\\"></path></g></svg><span></span><svg height=\\\"8.69875pt\\\" style=\\\"vertical-align:-0.3499298pt\\\" version=\\\"1.1\\\" viewbox=\\\"19.6321838 -8.34882 16.777 8.69875\\\" width=\\\"16.777pt\\\" xmlns=\\\"http://www.w3.org/2000/svg\\\" xmlns:xlink=\\\"http://www.w3.org/1999/xlink\\\"><g transform=\\\"matrix(.013,0,0,-0.013,19.682,0)\\\"><use xlink:href=\\\"#g113-54\\\"></use></g><g transform=\\\"matrix(.013,0,0,-0.013,28.828,0)\\\"><use xlink:href=\\\"#g117-42\\\"></use></g></svg><span></span><svg height=\\\"8.69875pt\\\" style=\\\"vertical-align:-0.3499298pt\\\" version=\\\"1.1\\\" viewbox=\\\"39.314183799999995 -8.34882 6.467 8.69875\\\" width=\\\"6.467pt\\\" xmlns=\\\"http://www.w3.org/2000/svg\\\" xmlns:xlink=\\\"http://www.w3.org/1999/xlink\\\"><g transform=\\\"matrix(.013,0,0,-0.013,39.364,0)\\\"></path></g></svg></span> mm). After preparation, each specimen was immersed in a 10 ml 75% ethanol/distilled water solution for three different periods: 1 h, 24 h, and 3 months (<span><svg height=\\\"8.32035pt\\\" style=\\\"vertical-align:-0.2063999pt\\\" version=\\\"1.1\\\" viewbox=\\\"-0.0498162 -8.11395 17.789 8.32035\\\" width=\\\"17.789pt\\\" xmlns=\\\"http://www.w3.org/2000/svg\\\" xmlns:xlink=\\\"http://www.w3.org/1999/xlink\\\"><g transform=\\\"matrix(.013,0,0,-0.013,0,0)\\\"></path></g><g transform=\\\"matrix(.013,0,0,-0.013,10.158,0)\\\"></path></g></svg><span></span><span><svg height=\\\"8.32035pt\\\" style=\\\"vertical-align:-0.2063999pt\\\" version=\\\"1.1\\\" viewbox=\\\"21.3711838 -8.11395 6.416 8.32035\\\" width=\\\"6.416pt\\\" xmlns=\\\"http://www.w3.org/2000/svg\\\" xmlns:xlink=\\\"http://www.w3.org/1999/xlink\\\"><g transform=\\\"matrix(.013,0,0,-0.013,21.421,0)\\\"><use xlink:href=\\\"#g113-54\\\"></use></g></svg>).</span></span> After the immersion period, 0.5 ml of solutions were taken from each bottle and analyzed using HPLC. At the end of the 3-month immersion period, the elution of monomers was determined mostly from SDR, GHF, EVX, and XTB, respectively. TEGDMA, the most released monomer of all groups, was released from all samples after 1 h, 24 h, and 3 months. The amount of monomer released in all composite groups at the end of the 3-month immersion period was significantly higher than the monomer amounts released after the 1-hour immersion period. The monomers were eluted from the composite dentin replacement materials during all immersion periods, and the amount of eluted monomers was increased with time.\",\"PeriodicalId\":14283,\"journal\":{\"name\":\"International Journal of Polymer Science\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":3.4000,\"publicationDate\":\"2024-03-12\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"International Journal of Polymer Science\",\"FirstCategoryId\":\"5\",\"ListUrlMain\":\"https://doi.org/10.1155/2024/9350118\",\"RegionNum\":4,\"RegionCategory\":\"化学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"POLYMER SCIENCE\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Polymer Science","FirstCategoryId":"5","ListUrlMain":"https://doi.org/10.1155/2024/9350118","RegionNum":4,"RegionCategory":"化学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"POLYMER SCIENCE","Score":null,"Total":0}
引用次数: 0

摘要

本研究的目的是使用高效液相色谱法测定和量化四种不同树脂基复合牙本质替代材料 3 个月的单体洗脱情况。本研究使用了四种不同的复合牙本质替代材料:EverX (EVX)、X-tra base (XTB)、SDR (SDR) 和 GrandioSO Heavy Flow (GHF)。每种材料都制备了 15 个样品(毫米)。制备完成后,将每个试样浸泡在 10 毫升 75% 的乙醇/蒸馏水溶液中,浸泡时间分别为 1 小时、24 小时和 3 个月()。浸泡期结束后,从每个瓶子中提取 0.5 毫升溶液,使用高效液相色谱法进行分析。在 3 个月的浸泡期结束时,分别测定了 SDR、GHF、EVX 和 XTB 的单体洗脱情况。TEGDMA 是所有组别中释放量最大的单体,在 1 小时、24 小时和 3 个月后从所有样品中释放出来。所有复合材料组在 3 个月浸泡期结束时释放的单体量都明显高于 1 小时浸泡期后释放的单体量。在所有浸泡期中,单体都从复合牙本质替代材料中洗脱出来,而且洗脱出来的单体量随着时间的推移而增加。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Evaluation of Monomer Releasing from Dentin Replacement Materials
The aim of this study is to determine and quantify the monomer elution from four different resin-based composite dentin replacement materials for 3 months using HPLC. Four different composite dentin replacement materials were used in the present study: EverX (EVX), X-tra base (XTB), SDR (SDR), and GrandioSO Heavy Flow (GHF). Fifteen samples from each material were prepared ( mm). After preparation, each specimen was immersed in a 10 ml 75% ethanol/distilled water solution for three different periods: 1 h, 24 h, and 3 months (). After the immersion period, 0.5 ml of solutions were taken from each bottle and analyzed using HPLC. At the end of the 3-month immersion period, the elution of monomers was determined mostly from SDR, GHF, EVX, and XTB, respectively. TEGDMA, the most released monomer of all groups, was released from all samples after 1 h, 24 h, and 3 months. The amount of monomer released in all composite groups at the end of the 3-month immersion period was significantly higher than the monomer amounts released after the 1-hour immersion period. The monomers were eluted from the composite dentin replacement materials during all immersion periods, and the amount of eluted monomers was increased with time.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
6.10
自引率
0.00%
发文量
55
审稿时长
>12 weeks
期刊介绍: The International Journal of Polymer Science is a peer-reviewed, Open Access journal that publishes original research articles as well as review articles on the chemistry and physics of macromolecules.
期刊最新文献
Characterisation of Luffa cylindrica Fibre from Cameroon for Use in Composites: Effect of Alkaline Treatment An Experimental Study of the Properties of Carbon Fiber/Epoxy Composites Mixed with Rubber Granules Experimental Investigation on the 3D Printing of Nylon Reinforced by Carbon Fiber through Fused Filament Fabrication Process, Effects of Extruder Temperature, and Printing Speed Fracture Resistance of Endodontically Treated Teeth Restored Using Multifiber Posts Compared with Single Fiber Posts Comparison of the Film Properties of Lemon and Sour Cherry Seed Essential Oil-Added Glycerol and/or Sorbitol-Plasticized Corn, Potato, Rice, Tapioca, and Wheat Starch-Based Edible Films
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1