{"title":"氧化铝与铝铸造合金摩擦焊接接头的显微结构和机械特性","authors":"Tsuyoshi Takahashi, Son Thanh Nguyen, Masaaki Kimura","doi":"10.4028/p-9esrhc","DOIUrl":null,"url":null,"abstract":"In this study, the Al2O3 round bar and Al-Si12CuNi (AC8A) round bar were joined by friction welding. AC8A is a typical piston material treated by the heat treatment T6. The parameters of the joining condition are friction time and upset pressure. SEM observed the microstructure at the interface region of joined materials. 1) Judging from these photographs, the damages to the microstructures at the interface region of joined materials by upset pressure are more significant than those caused by friction time. 2) The relationship between the joint conditions and mechanical characteristics from three points of bending test results for the joint material specimens. 3) The residual stresses around the interface were measured by the Raman spectroscopy method. There is a possibility that the friction welding conditions are correlated to the residual stresses.","PeriodicalId":18262,"journal":{"name":"Materials Science Forum","volume":"38 21","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-05-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Microstructure and Mechanical Characteristics of Friction Welded Joint between Alumina and Aluminum Casting Alloy\",\"authors\":\"Tsuyoshi Takahashi, Son Thanh Nguyen, Masaaki Kimura\",\"doi\":\"10.4028/p-9esrhc\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In this study, the Al2O3 round bar and Al-Si12CuNi (AC8A) round bar were joined by friction welding. AC8A is a typical piston material treated by the heat treatment T6. The parameters of the joining condition are friction time and upset pressure. SEM observed the microstructure at the interface region of joined materials. 1) Judging from these photographs, the damages to the microstructures at the interface region of joined materials by upset pressure are more significant than those caused by friction time. 2) The relationship between the joint conditions and mechanical characteristics from three points of bending test results for the joint material specimens. 3) The residual stresses around the interface were measured by the Raman spectroscopy method. There is a possibility that the friction welding conditions are correlated to the residual stresses.\",\"PeriodicalId\":18262,\"journal\":{\"name\":\"Materials Science Forum\",\"volume\":\"38 21\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2024-05-21\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Materials Science Forum\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.4028/p-9esrhc\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials Science Forum","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4028/p-9esrhc","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

在这项研究中,Al2O3 圆棒和 Al-Si12CuNi (AC8A) 圆棒通过摩擦焊接连接在一起。AC8A 是经过 T6 热处理的典型活塞材料。焊接条件参数为摩擦时间和破坏压力。扫描电镜观察了接合材料界面区域的微观结构。1) 从这些照片来看,镦粗压力对接合材料界面区微观结构的破坏比摩擦时间造成的破坏更为严重。2) 从接合材料试样的三点弯曲试验结果来看,接合条件与力学特性之间的关系。3) 用拉曼光谱法测量了界面周围的残余应力。摩擦焊接条件有可能与残余应力相关。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Microstructure and Mechanical Characteristics of Friction Welded Joint between Alumina and Aluminum Casting Alloy
In this study, the Al2O3 round bar and Al-Si12CuNi (AC8A) round bar were joined by friction welding. AC8A is a typical piston material treated by the heat treatment T6. The parameters of the joining condition are friction time and upset pressure. SEM observed the microstructure at the interface region of joined materials. 1) Judging from these photographs, the damages to the microstructures at the interface region of joined materials by upset pressure are more significant than those caused by friction time. 2) The relationship between the joint conditions and mechanical characteristics from three points of bending test results for the joint material specimens. 3) The residual stresses around the interface were measured by the Raman spectroscopy method. There is a possibility that the friction welding conditions are correlated to the residual stresses.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
1.20
自引率
0.00%
发文量
0
期刊最新文献
The Effect of Friction Stir Weld (FSW) Process Parameters on Tensile Strength, Macro Structure, and Hardness in Results of AA7075 Butt Joints Study of the Physic-Mechanical Properties of a Typha Concrete Composites: A Possible New Material for Sustainable Construction Incorporating Graphene Nanofiller for the Improvement of Hydrophobic Properties of Cassava Peel Starch Bioplastic Microstructure and Mechanical Characteristics of Friction Welded Joint between Alumina and Aluminum Casting Alloy Effect of Silanized Zirconium Oxide (ZrO2) Filler on Hardness of Acrylic-Based Denture Teeth
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1