R. V. Lytvyn, K. E. Grinkevich, O. M. Myslyvchenko, I. V. Trachenko, O. M. Bloschanevych, S. E. Ivanchenko, O. V. Derev’yanko, A. I. Stegniy, V. D. Belik, O. B. Zgalat-Lozynskyy
{"title":"通过电火花沉积和激光加工用 TiN-TiB2 和 TiN-Si3N4 复合材料制作耐磨涂层","authors":"R. V. Lytvyn, K. E. Grinkevich, O. M. Myslyvchenko, I. V. Trachenko, O. M. Bloschanevych, S. E. Ivanchenko, O. V. Derev’yanko, A. I. Stegniy, V. D. Belik, O. B. Zgalat-Lozynskyy","doi":"10.1007/s11106-024-00421-9","DOIUrl":null,"url":null,"abstract":"<p>The TiN–20% TiB<sub>2</sub> and TiN–20% Si<sub>3</sub>N<sub>4</sub> nanocomposites sintered in a microwave field with a frequency of 2.45 GHz were applied to a steel substrate by electrospark deposition in the temperature range 1400–1500°C in a nitrogen atmosphere. In deposition modes with an energy of isolated pulses ranging from 0.2 to 0.75 J, changed surface layers consisting of a coating 50–90 μm thick and a heat-affected zone of increased hardness 40–60 μm thick on the substrate were produced. A part of the samples was subjected to additional surface laser processing to increase the density and homogeneity of the deposited layers. Substantial influence of electrospark mass transfer on the phase composition of the transferred material was established. According to XRD data, the TiN–TiB<sub>2</sub> composite, with all its components being present in the coating, was more stable. In the case of the TiN–Si<sub>3</sub>N<sub>4</sub> composite, silicon nitride completely dissociated to form Ti<sub>5</sub>Si<sub>3</sub> and Ti<sub>2</sub>N compounds. For both compositions, iron, penetrating into the coating from the substrate, was found in the deposited layer. The TiN–TiB<sub>2</sub> and TiN–Si<sub>3</sub>N<sub>4</sub> coatings had a hardness of 14–15 GPa and 11–12 GPa, respectively. Comparative tribotechnical tests of the coatings with a spherical VK6 hardmetal counterface in quasistatic and dynamic modes revealed that the electrospark deposition of the TiN–TiB<sub>2</sub> composite combined with subsequent laser processing was highly efficient. In tribotechnical tests, the linear wear of this coating was 0.5 μm, corresponding to a twelvefold increase in the wear resistance as compared to that of the TiN–Si<sub>3</sub>N<sub>4</sub> coating for dynamic friction tests. The deposition of the TiN–Si<sub>3</sub>N<sub>4</sub> composite enabled a double increase in the wear resistance of the substrate in dynamic testing mode. In this case, additional laser processing of the coating turned out to be inefficient.</p>","PeriodicalId":742,"journal":{"name":"Powder Metallurgy and Metal Ceramics","volume":"62 9-10","pages":"611 - 620"},"PeriodicalIF":0.9000,"publicationDate":"2024-05-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Wear-Resistant Coatings Produced from TiN–TiB2 and TiN–Si3N4 Composites by Electrospark Deposition and Laser Processing\",\"authors\":\"R. V. Lytvyn, K. E. Grinkevich, O. M. Myslyvchenko, I. V. Trachenko, O. M. Bloschanevych, S. E. Ivanchenko, O. V. Derev’yanko, A. I. Stegniy, V. D. Belik, O. B. Zgalat-Lozynskyy\",\"doi\":\"10.1007/s11106-024-00421-9\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The TiN–20% TiB<sub>2</sub> and TiN–20% Si<sub>3</sub>N<sub>4</sub> nanocomposites sintered in a microwave field with a frequency of 2.45 GHz were applied to a steel substrate by electrospark deposition in the temperature range 1400–1500°C in a nitrogen atmosphere. In deposition modes with an energy of isolated pulses ranging from 0.2 to 0.75 J, changed surface layers consisting of a coating 50–90 μm thick and a heat-affected zone of increased hardness 40–60 μm thick on the substrate were produced. A part of the samples was subjected to additional surface laser processing to increase the density and homogeneity of the deposited layers. Substantial influence of electrospark mass transfer on the phase composition of the transferred material was established. According to XRD data, the TiN–TiB<sub>2</sub> composite, with all its components being present in the coating, was more stable. In the case of the TiN–Si<sub>3</sub>N<sub>4</sub> composite, silicon nitride completely dissociated to form Ti<sub>5</sub>Si<sub>3</sub> and Ti<sub>2</sub>N compounds. For both compositions, iron, penetrating into the coating from the substrate, was found in the deposited layer. The TiN–TiB<sub>2</sub> and TiN–Si<sub>3</sub>N<sub>4</sub> coatings had a hardness of 14–15 GPa and 11–12 GPa, respectively. Comparative tribotechnical tests of the coatings with a spherical VK6 hardmetal counterface in quasistatic and dynamic modes revealed that the electrospark deposition of the TiN–TiB<sub>2</sub> composite combined with subsequent laser processing was highly efficient. In tribotechnical tests, the linear wear of this coating was 0.5 μm, corresponding to a twelvefold increase in the wear resistance as compared to that of the TiN–Si<sub>3</sub>N<sub>4</sub> coating for dynamic friction tests. The deposition of the TiN–Si<sub>3</sub>N<sub>4</sub> composite enabled a double increase in the wear resistance of the substrate in dynamic testing mode. In this case, additional laser processing of the coating turned out to be inefficient.</p>\",\"PeriodicalId\":742,\"journal\":{\"name\":\"Powder Metallurgy and Metal Ceramics\",\"volume\":\"62 9-10\",\"pages\":\"611 - 620\"},\"PeriodicalIF\":0.9000,\"publicationDate\":\"2024-05-31\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Powder Metallurgy and Metal Ceramics\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://link.springer.com/article/10.1007/s11106-024-00421-9\",\"RegionNum\":4,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"MATERIALS SCIENCE, CERAMICS\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Powder Metallurgy and Metal Ceramics","FirstCategoryId":"88","ListUrlMain":"https://link.springer.com/article/10.1007/s11106-024-00421-9","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
Wear-Resistant Coatings Produced from TiN–TiB2 and TiN–Si3N4 Composites by Electrospark Deposition and Laser Processing
The TiN–20% TiB2 and TiN–20% Si3N4 nanocomposites sintered in a microwave field with a frequency of 2.45 GHz were applied to a steel substrate by electrospark deposition in the temperature range 1400–1500°C in a nitrogen atmosphere. In deposition modes with an energy of isolated pulses ranging from 0.2 to 0.75 J, changed surface layers consisting of a coating 50–90 μm thick and a heat-affected zone of increased hardness 40–60 μm thick on the substrate were produced. A part of the samples was subjected to additional surface laser processing to increase the density and homogeneity of the deposited layers. Substantial influence of electrospark mass transfer on the phase composition of the transferred material was established. According to XRD data, the TiN–TiB2 composite, with all its components being present in the coating, was more stable. In the case of the TiN–Si3N4 composite, silicon nitride completely dissociated to form Ti5Si3 and Ti2N compounds. For both compositions, iron, penetrating into the coating from the substrate, was found in the deposited layer. The TiN–TiB2 and TiN–Si3N4 coatings had a hardness of 14–15 GPa and 11–12 GPa, respectively. Comparative tribotechnical tests of the coatings with a spherical VK6 hardmetal counterface in quasistatic and dynamic modes revealed that the electrospark deposition of the TiN–TiB2 composite combined with subsequent laser processing was highly efficient. In tribotechnical tests, the linear wear of this coating was 0.5 μm, corresponding to a twelvefold increase in the wear resistance as compared to that of the TiN–Si3N4 coating for dynamic friction tests. The deposition of the TiN–Si3N4 composite enabled a double increase in the wear resistance of the substrate in dynamic testing mode. In this case, additional laser processing of the coating turned out to be inefficient.
期刊介绍:
Powder Metallurgy and Metal Ceramics covers topics of the theory, manufacturing technology, and properties of powder; technology of forming processes; the technology of sintering, heat treatment, and thermo-chemical treatment; properties of sintered materials; and testing methods.