{"title":"带有铬改性(镍、铂)铝键涂层的新型(Yb0.1Gd0.9)2Zr2O7 隔热涂层的热冲击行为","authors":"Tingyue Li, Xin Wang, Zhen Zhen, Rende Mu, Limin He, Zhenhua Xu","doi":"10.1016/j.ceramint.2024.07.083","DOIUrl":null,"url":null,"abstract":"<p>The durability of thermal barrier coatings (TBCs) is significantly influenced both by the ceramic top coat and the bond coat. In this study, novel YbGdZrO ceramic coats were deposited on the surfaces of three types of Cr-modified (Ni, Pt)Al bond coats via electron beam physical vapor deposition (EB-PVD) technique. These Cr-modified (Ni, Pt)Al bond coats were fabricated by magnetic sputtering Cr onto the (Ni, Pt)Al bond coats with varying sputtering times of 30, 60, and 90 minutes. The results indicates that the thickness of the Cr-modified layer increases with the extension of sputtering time. A short deposition time of 30 min is adequate for achieving an appropriate Cr content in the (Ni, Pt)Al bond coats, which ensures selective oxidation of Al element within the bond coat and further enhances the metallurgical interfacial bonding strength with the ceramic coat by adapting to the concentration gradient diffusion. However, as the sputtering time is extended to 60 and 90 minutes, α-Cr begins to form in the Cr-modified (Ni, Pt)Al bond coats, which negatively affects the oxidation resistance of the bond coat. Consequently, the thermal shock life of the TBCs samples is significantly reduced with increasing sputtering time. The longest thermal shock lifetime is obtained on the bond coat with Cr plating time of 30 minutes owing to a differing thermally grown oxide formation and failure mechanism.</p>","PeriodicalId":267,"journal":{"name":"Ceramics International","volume":null,"pages":null},"PeriodicalIF":5.1000,"publicationDate":"2024-07-08","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Thermal shock behavior of novel (Yb0.1Gd0.9)2Zr2O7 thermal barrier coatings with a Cr modified (Ni, Pt)Al bond coat\",\"authors\":\"Tingyue Li, Xin Wang, Zhen Zhen, Rende Mu, Limin He, Zhenhua Xu\",\"doi\":\"10.1016/j.ceramint.2024.07.083\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The durability of thermal barrier coatings (TBCs) is significantly influenced both by the ceramic top coat and the bond coat. In this study, novel YbGdZrO ceramic coats were deposited on the surfaces of three types of Cr-modified (Ni, Pt)Al bond coats via electron beam physical vapor deposition (EB-PVD) technique. These Cr-modified (Ni, Pt)Al bond coats were fabricated by magnetic sputtering Cr onto the (Ni, Pt)Al bond coats with varying sputtering times of 30, 60, and 90 minutes. The results indicates that the thickness of the Cr-modified layer increases with the extension of sputtering time. A short deposition time of 30 min is adequate for achieving an appropriate Cr content in the (Ni, Pt)Al bond coats, which ensures selective oxidation of Al element within the bond coat and further enhances the metallurgical interfacial bonding strength with the ceramic coat by adapting to the concentration gradient diffusion. However, as the sputtering time is extended to 60 and 90 minutes, α-Cr begins to form in the Cr-modified (Ni, Pt)Al bond coats, which negatively affects the oxidation resistance of the bond coat. Consequently, the thermal shock life of the TBCs samples is significantly reduced with increasing sputtering time. The longest thermal shock lifetime is obtained on the bond coat with Cr plating time of 30 minutes owing to a differing thermally grown oxide formation and failure mechanism.</p>\",\"PeriodicalId\":267,\"journal\":{\"name\":\"Ceramics International\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":5.1000,\"publicationDate\":\"2024-07-08\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Ceramics International\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.1016/j.ceramint.2024.07.083\",\"RegionNum\":2,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"MATERIALS SCIENCE, CERAMICS\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Ceramics International","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1016/j.ceramint.2024.07.083","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
Thermal shock behavior of novel (Yb0.1Gd0.9)2Zr2O7 thermal barrier coatings with a Cr modified (Ni, Pt)Al bond coat
The durability of thermal barrier coatings (TBCs) is significantly influenced both by the ceramic top coat and the bond coat. In this study, novel YbGdZrO ceramic coats were deposited on the surfaces of three types of Cr-modified (Ni, Pt)Al bond coats via electron beam physical vapor deposition (EB-PVD) technique. These Cr-modified (Ni, Pt)Al bond coats were fabricated by magnetic sputtering Cr onto the (Ni, Pt)Al bond coats with varying sputtering times of 30, 60, and 90 minutes. The results indicates that the thickness of the Cr-modified layer increases with the extension of sputtering time. A short deposition time of 30 min is adequate for achieving an appropriate Cr content in the (Ni, Pt)Al bond coats, which ensures selective oxidation of Al element within the bond coat and further enhances the metallurgical interfacial bonding strength with the ceramic coat by adapting to the concentration gradient diffusion. However, as the sputtering time is extended to 60 and 90 minutes, α-Cr begins to form in the Cr-modified (Ni, Pt)Al bond coats, which negatively affects the oxidation resistance of the bond coat. Consequently, the thermal shock life of the TBCs samples is significantly reduced with increasing sputtering time. The longest thermal shock lifetime is obtained on the bond coat with Cr plating time of 30 minutes owing to a differing thermally grown oxide formation and failure mechanism.
期刊介绍:
Ceramics International covers the science of advanced ceramic materials. The journal encourages contributions that demonstrate how an understanding of the basic chemical and physical phenomena may direct materials design and stimulate ideas for new or improved processing techniques, in order to obtain materials with desired structural features and properties.
Ceramics International covers oxide and non-oxide ceramics, functional glasses, glass ceramics, amorphous inorganic non-metallic materials (and their combinations with metal and organic materials), in the form of particulates, dense or porous bodies, thin/thick films and laminated, graded and composite structures. Process related topics such as ceramic-ceramic joints or joining ceramics with dissimilar materials, as well as surface finishing and conditioning are also covered. Besides traditional processing techniques, manufacturing routes of interest include innovative procedures benefiting from externally applied stresses, electromagnetic fields and energetic beams, as well as top-down and self-assembly nanotechnology approaches. In addition, the journal welcomes submissions on bio-inspired and bio-enabled materials designs, experimentally validated multi scale modelling and simulation for materials design, and the use of the most advanced chemical and physical characterization techniques of structure, properties and behaviour.
Technologically relevant low-dimensional systems are a particular focus of Ceramics International. These include 0, 1 and 2-D nanomaterials (also covering CNTs, graphene and related materials, and diamond-like carbons), their nanocomposites, as well as nano-hybrids and hierarchical multifunctional nanostructures that might integrate molecular, biological and electronic components.