O3 型 NaMn1/3 Fe1/3Ni1/3O2 的高空气灵敏度起源和处理策略。

IF 14.4 1区 化学 Q1 CHEMISTRY, MULTIDISCIPLINARY Journal of the American Chemical Society Pub Date : 2024-08-14 Epub Date: 2024-07-19 DOI:10.1021/jacs.4c05255
Xian-Qi Xu, Jun-Yan Chen, Yao Jiang, Bo Xu, Xin-Lu Li, Chu-Ying Ouyang, Jia-Xin Zheng
{"title":"O3 型 NaMn1/3 Fe1/3Ni1/3O2 的高空气灵敏度起源和处理策略。","authors":"Xian-Qi Xu, Jun-Yan Chen, Yao Jiang, Bo Xu, Xin-Lu Li, Chu-Ying Ouyang, Jia-Xin Zheng","doi":"10.1021/jacs.4c05255","DOIUrl":null,"url":null,"abstract":"<p><p>Sodium-ion layered oxides are one of the most highly regarded sodium-ion cathode materials and are expected to be used in electric vehicles and large-scale grid-level energy storage systems. However, highly air-sensitive issues limit sodium-ion layered oxide cathode materials to maximize cost advantages. Industrial and scientific researchers have been developing cost-effective air sensitivity treatment strategies with little success because the impurity formation mechanism is still unclear. Using density functional theory calculations and ab initio molecular dynamics simulations, this work shows that the poor air stability of O3-type NaMn<sub>1/3</sub>Fe<sub>1/3</sub>Ni<sub>1/3</sub>O<sub>2</sub> (NMFNO) may be as follows: (1) low percentage of nonreactive (003) surface; (2) strong surface adsorption capacity and high surface reactivity; and (3) instability of the surface sodium ions. Our physical images point out that the high reactivity of the NMFNO surface originates from the increase in electron loss and unpaired electrons (magnetic moments) of the surface oxygen active site as well as the enhanced metal coactivation effect due to the large radius of the sodium ion. We also found that the hydrolysis reaction requires a higher reactivity of the surface oxygen active site, while the carbon hybridization mode transformation in carbonate formation depends mainly on metal activation and does not even require the involvement of surface oxygen active sites. Based on the calculation results and our proposed physical images, we discuss the feasibility of these treatment strategies (including surface morphology modulation, cation/anion substitution, and surface configuration design) for air-sensitive issues.</p>","PeriodicalId":49,"journal":{"name":"Journal of the American Chemical Society","volume":null,"pages":null},"PeriodicalIF":14.4000,"publicationDate":"2024-08-14","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Origins of High Air Sensitivity and Treatment Strategies in O3-Type NaMn<sub>1/3</sub> Fe<sub>1/3</sub>Ni<sub>1/3</sub>O<sub>2</sub>.\",\"authors\":\"Xian-Qi Xu, Jun-Yan Chen, Yao Jiang, Bo Xu, Xin-Lu Li, Chu-Ying Ouyang, Jia-Xin Zheng\",\"doi\":\"10.1021/jacs.4c05255\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>Sodium-ion layered oxides are one of the most highly regarded sodium-ion cathode materials and are expected to be used in electric vehicles and large-scale grid-level energy storage systems. However, highly air-sensitive issues limit sodium-ion layered oxide cathode materials to maximize cost advantages. Industrial and scientific researchers have been developing cost-effective air sensitivity treatment strategies with little success because the impurity formation mechanism is still unclear. Using density functional theory calculations and ab initio molecular dynamics simulations, this work shows that the poor air stability of O3-type NaMn<sub>1/3</sub>Fe<sub>1/3</sub>Ni<sub>1/3</sub>O<sub>2</sub> (NMFNO) may be as follows: (1) low percentage of nonreactive (003) surface; (2) strong surface adsorption capacity and high surface reactivity; and (3) instability of the surface sodium ions. Our physical images point out that the high reactivity of the NMFNO surface originates from the increase in electron loss and unpaired electrons (magnetic moments) of the surface oxygen active site as well as the enhanced metal coactivation effect due to the large radius of the sodium ion. We also found that the hydrolysis reaction requires a higher reactivity of the surface oxygen active site, while the carbon hybridization mode transformation in carbonate formation depends mainly on metal activation and does not even require the involvement of surface oxygen active sites. Based on the calculation results and our proposed physical images, we discuss the feasibility of these treatment strategies (including surface morphology modulation, cation/anion substitution, and surface configuration design) for air-sensitive issues.</p>\",\"PeriodicalId\":49,\"journal\":{\"name\":\"Journal of the American Chemical Society\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":14.4000,\"publicationDate\":\"2024-08-14\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of the American Chemical Society\",\"FirstCategoryId\":\"92\",\"ListUrlMain\":\"https://doi.org/10.1021/jacs.4c05255\",\"RegionNum\":1,\"RegionCategory\":\"化学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"2024/7/19 0:00:00\",\"PubModel\":\"Epub\",\"JCR\":\"Q1\",\"JCRName\":\"CHEMISTRY, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of the American Chemical Society","FirstCategoryId":"92","ListUrlMain":"https://doi.org/10.1021/jacs.4c05255","RegionNum":1,"RegionCategory":"化学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2024/7/19 0:00:00","PubModel":"Epub","JCR":"Q1","JCRName":"CHEMISTRY, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

摘要

钠离子层状氧化物是最受推崇的钠离子阴极材料之一,有望用于电动汽车和大规模电网级储能系统。然而,对空气高度敏感的问题限制了钠离子层状氧化物阴极材料最大限度地发挥成本优势。工业和科学研究人员一直在开发具有成本效益的空气敏感性处理策略,但收效甚微,因为杂质的形成机制尚不清楚。这项工作利用密度泛函理论计算和 ab initio 分子动力学模拟,表明 O3 型 NaMn1/3Fe1/3Ni1/3O2 (NMFNO) 空气稳定性差的原因可能如下:(1) 非反应性(003)表面比例低;(2) 表面吸附能力强,表面反应性高;(3) 表面钠离子不稳定。我们的物理图像表明,NMFNO 表面的高反应活性源于表面氧活性位点的电子损耗和未配对电子(磁矩)的增加,以及钠离子半径大导致的金属共激活效应的增强。我们还发现,水解反应需要表面氧活性位点具有更高的反应活性,而碳酸盐形成过程中的碳杂化模式转化主要取决于金属活化,甚至不需要表面氧活性位点的参与。基于计算结果和我们提出的物理图像,我们讨论了这些处理策略(包括表面形态调节、阳离子/阴离子置换和表面构型设计)在空气敏感问题上的可行性。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

摘要图片

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Origins of High Air Sensitivity and Treatment Strategies in O3-Type NaMn1/3 Fe1/3Ni1/3O2.

Sodium-ion layered oxides are one of the most highly regarded sodium-ion cathode materials and are expected to be used in electric vehicles and large-scale grid-level energy storage systems. However, highly air-sensitive issues limit sodium-ion layered oxide cathode materials to maximize cost advantages. Industrial and scientific researchers have been developing cost-effective air sensitivity treatment strategies with little success because the impurity formation mechanism is still unclear. Using density functional theory calculations and ab initio molecular dynamics simulations, this work shows that the poor air stability of O3-type NaMn1/3Fe1/3Ni1/3O2 (NMFNO) may be as follows: (1) low percentage of nonreactive (003) surface; (2) strong surface adsorption capacity and high surface reactivity; and (3) instability of the surface sodium ions. Our physical images point out that the high reactivity of the NMFNO surface originates from the increase in electron loss and unpaired electrons (magnetic moments) of the surface oxygen active site as well as the enhanced metal coactivation effect due to the large radius of the sodium ion. We also found that the hydrolysis reaction requires a higher reactivity of the surface oxygen active site, while the carbon hybridization mode transformation in carbonate formation depends mainly on metal activation and does not even require the involvement of surface oxygen active sites. Based on the calculation results and our proposed physical images, we discuss the feasibility of these treatment strategies (including surface morphology modulation, cation/anion substitution, and surface configuration design) for air-sensitive issues.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
24.40
自引率
6.00%
发文量
2398
审稿时长
1.6 months
期刊介绍: The flagship journal of the American Chemical Society, known as the Journal of the American Chemical Society (JACS), has been a prestigious publication since its establishment in 1879. It holds a preeminent position in the field of chemistry and related interdisciplinary sciences. JACS is committed to disseminating cutting-edge research papers, covering a wide range of topics, and encompasses approximately 19,000 pages of Articles, Communications, and Perspectives annually. With a weekly publication frequency, JACS plays a vital role in advancing the field of chemistry by providing essential research.
期刊最新文献
cis-Dihydroxylation by Synthetic Iron(III)-Peroxo Intermediates and Rieske Dioxygenases: Experimental and Theoretical Approaches Reveal the Key O-O Bond Activation Step. Retraction of "Solvent Polarity under Vibrational Strong Coupling". Ultra-Narrowband Circularly Polarized Luminescence from Multiple 1,4-Azaborine-Embedded Helical Nanographenes. Skeletal Editing of Mechanically Interlocked Molecules: Nitrogen Atom Deletion from Crown Ether-Dibenzylammonium Rotaxanes Microdroplet-Mediated Multiphase Cycling in a Cloud of Water Drives Chemoselective Electrolysis
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1