{"title":"以聚甲醛(POM)为原料通过压缩成型获得高密度 7075 铝合金的微观结构和机械性能","authors":"Heng Zou, Yi Sun, Mengxiong Chen, Yuan Jiang, Yang Fu, Huiwen Xiong, Lei Zhang, Kechao Zhou","doi":"10.1016/j.jmrt.2024.09.025","DOIUrl":null,"url":null,"abstract":"Metal injection molding of aluminium alloy (MIM-Al) attracts attention, owing to the lightweight, corrosion resistance and good thermal conductivity. However, it is hard to fabricate high-quality MIM-Al due to the hard-to-sinter powder and poor mechanical properties. Here, we report a facile compression molding process for fabricating high-density 7075Al alloy parts using polyformaldehyde (POM)-based feedstock. Pressureless sintering with a high nitrogen flow rate was adopted to promote sintering densification process. The wetting behavior, rheological properties, and morphology of the feedstock were characterized, showcasing the shear-thinning behavior and suitable viscosity for POM-PP-SA binder. Through controlling the compact pressure, mold temperature and holding time, green gear part with good shape retention and dense microstructure was achieved. Influence of process factors and sintering temperature on the microstructure and mechanical properties of 7075Al alloy are investigated. Remarkably, the aluminum alloy components sintered at 610 °C exhibited excellent performance, with a relative density reaching 97.6 % and a tensile strength of 214.8 MPa. This achievement provides a foundation for the industrial application of complex-shaped aluminum alloy components through the compression molding process.","PeriodicalId":501120,"journal":{"name":"Journal of Materials Research and Technology","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2024-09-07","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Microstructure and mechanical property of high-density 7075 Al alloy by compression molding of POM-based feedstock\",\"authors\":\"Heng Zou, Yi Sun, Mengxiong Chen, Yuan Jiang, Yang Fu, Huiwen Xiong, Lei Zhang, Kechao Zhou\",\"doi\":\"10.1016/j.jmrt.2024.09.025\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Metal injection molding of aluminium alloy (MIM-Al) attracts attention, owing to the lightweight, corrosion resistance and good thermal conductivity. However, it is hard to fabricate high-quality MIM-Al due to the hard-to-sinter powder and poor mechanical properties. Here, we report a facile compression molding process for fabricating high-density 7075Al alloy parts using polyformaldehyde (POM)-based feedstock. Pressureless sintering with a high nitrogen flow rate was adopted to promote sintering densification process. The wetting behavior, rheological properties, and morphology of the feedstock were characterized, showcasing the shear-thinning behavior and suitable viscosity for POM-PP-SA binder. Through controlling the compact pressure, mold temperature and holding time, green gear part with good shape retention and dense microstructure was achieved. Influence of process factors and sintering temperature on the microstructure and mechanical properties of 7075Al alloy are investigated. Remarkably, the aluminum alloy components sintered at 610 °C exhibited excellent performance, with a relative density reaching 97.6 % and a tensile strength of 214.8 MPa. This achievement provides a foundation for the industrial application of complex-shaped aluminum alloy components through the compression molding process.\",\"PeriodicalId\":501120,\"journal\":{\"name\":\"Journal of Materials Research and Technology\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2024-09-07\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Materials Research and Technology\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1016/j.jmrt.2024.09.025\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Materials Research and Technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1016/j.jmrt.2024.09.025","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

金属注射成型铝合金(MIM-Al)因其轻质、耐腐蚀和良好的导热性而备受关注。然而,由于难以烧结的粉末和较差的机械性能,很难制造出高质量的 MIM-Al。在此,我们报告了一种使用聚甲醛(POM)为原料制造高密度 7075Al 合金零件的简便压缩成型工艺。采用高氮气流量的无压烧结工艺来促进烧结致密化过程。对原料的润湿行为、流变特性和形态进行了表征,结果表明 POM-PP-SA 粘合剂具有剪切稀化行为和合适的粘度。通过控制压制压力、模具温度和保温时间,获得了形状保持良好、微观结构致密的绿色齿轮零件。研究了工艺因素和烧结温度对 7075Al 合金微观结构和机械性能的影响。值得注意的是,在 610 °C 下烧结的铝合金部件性能优异,相对密度达到 97.6 %,抗拉强度达到 214.8 MPa。这一成果为通过压缩成型工艺生产复杂形状的铝合金部件的工业应用奠定了基础。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Microstructure and mechanical property of high-density 7075 Al alloy by compression molding of POM-based feedstock
Metal injection molding of aluminium alloy (MIM-Al) attracts attention, owing to the lightweight, corrosion resistance and good thermal conductivity. However, it is hard to fabricate high-quality MIM-Al due to the hard-to-sinter powder and poor mechanical properties. Here, we report a facile compression molding process for fabricating high-density 7075Al alloy parts using polyformaldehyde (POM)-based feedstock. Pressureless sintering with a high nitrogen flow rate was adopted to promote sintering densification process. The wetting behavior, rheological properties, and morphology of the feedstock were characterized, showcasing the shear-thinning behavior and suitable viscosity for POM-PP-SA binder. Through controlling the compact pressure, mold temperature and holding time, green gear part with good shape retention and dense microstructure was achieved. Influence of process factors and sintering temperature on the microstructure and mechanical properties of 7075Al alloy are investigated. Remarkably, the aluminum alloy components sintered at 610 °C exhibited excellent performance, with a relative density reaching 97.6 % and a tensile strength of 214.8 MPa. This achievement provides a foundation for the industrial application of complex-shaped aluminum alloy components through the compression molding process.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Revealing the microstructural evolution and mechanical response of repaired Fe–Cr–Si based alloy by directed energy deposition Non-planar additive manufacturing of pre-impregnated continuous fiber reinforced composites using a three-axis printer Microstructure and mechanical property of high-density 7075 Al alloy by compression molding of POM-based feedstock Effect of microstructural inheritance window on the mechanical properties of an intercritically annealed Q&P steel Clarifying the effect of irradiation and thermal treatment on the austenitic microstructure and austenitic hardening in austenitic stainless steel weld metal
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1