{"title":"老化金属玻璃的结构返老还老","authors":"","doi":"10.1016/j.fmre.2022.12.004","DOIUrl":null,"url":null,"abstract":"<div><div>Rejuvenation of glassy structures in general is characterized by the exothermic enthalpy prior to the glass transition. In the present work, we find that this situation is not applicable to a heavily-aged Zr-based metallic glass that rejuvenates by anelastic deformation before yield. Instead, its rejuvenation can be precisely captured by the low-temperature boson heat capacity peak as well as the effective enthalpy change with the glass-to-liquid transition. These results demonstrate that a structurally stable glass could rejuvenate by decreasing mechanical stability of its basin of potential energy landscape, but without changing the basin's energy level. The underlying mechanism points toward the redistribution of the atomic free volume with a constant system-averaged value. We further find that the rejuvenation limit of this glass is its steady-flow state with self-similar inherent structures at both short- and long-time scales. Our findings refresh the understanding of glass rejuvenation and suggest that the boson peak is a better probe for the structural rejuvenation of glasses.</div></div>","PeriodicalId":34602,"journal":{"name":"Fundamental Research","volume":"4 5","pages":"Pages 1266-1271"},"PeriodicalIF":6.2000,"publicationDate":"2024-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Structural rejuvenation of a well-aged metallic glass\",\"authors\":\"\",\"doi\":\"10.1016/j.fmre.2022.12.004\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><div>Rejuvenation of glassy structures in general is characterized by the exothermic enthalpy prior to the glass transition. In the present work, we find that this situation is not applicable to a heavily-aged Zr-based metallic glass that rejuvenates by anelastic deformation before yield. Instead, its rejuvenation can be precisely captured by the low-temperature boson heat capacity peak as well as the effective enthalpy change with the glass-to-liquid transition. These results demonstrate that a structurally stable glass could rejuvenate by decreasing mechanical stability of its basin of potential energy landscape, but without changing the basin's energy level. The underlying mechanism points toward the redistribution of the atomic free volume with a constant system-averaged value. We further find that the rejuvenation limit of this glass is its steady-flow state with self-similar inherent structures at both short- and long-time scales. Our findings refresh the understanding of glass rejuvenation and suggest that the boson peak is a better probe for the structural rejuvenation of glasses.</div></div>\",\"PeriodicalId\":34602,\"journal\":{\"name\":\"Fundamental Research\",\"volume\":\"4 5\",\"pages\":\"Pages 1266-1271\"},\"PeriodicalIF\":6.2000,\"publicationDate\":\"2024-09-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Fundamental Research\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/S2667325822004472\",\"RegionNum\":3,\"RegionCategory\":\"综合性期刊\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"Multidisciplinary\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Fundamental Research","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2667325822004472","RegionNum":3,"RegionCategory":"综合性期刊","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"Multidisciplinary","Score":null,"Total":0}
引用次数: 0

摘要

玻璃结构的返老还童一般以玻璃转变前的放热焓为特征。在本研究中,我们发现这种情况并不适用于一种严重老化的锆基金属玻璃,这种玻璃在屈服前会通过非弹性形变恢复活力。相反,低温玻色子热容量峰以及玻璃到液体转变过程中的有效焓变可以精确捕捉到它的年轻化过程。这些结果表明,结构稳定的玻璃可以通过降低其势能景观盆地的机械稳定性而恢复活力,但盆地的能级不会发生变化。其基本机制是以恒定的系统平均值重新分配原子自由体积。我们进一步发现,这种玻璃的年轻化极限是其在短期和长期尺度上具有自相似固有结构的稳定流动状态。我们的发现刷新了人们对玻璃年轻化的认识,并表明玻色子峰是玻璃结构年轻化的更好探针。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

摘要图片

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Structural rejuvenation of a well-aged metallic glass
Rejuvenation of glassy structures in general is characterized by the exothermic enthalpy prior to the glass transition. In the present work, we find that this situation is not applicable to a heavily-aged Zr-based metallic glass that rejuvenates by anelastic deformation before yield. Instead, its rejuvenation can be precisely captured by the low-temperature boson heat capacity peak as well as the effective enthalpy change with the glass-to-liquid transition. These results demonstrate that a structurally stable glass could rejuvenate by decreasing mechanical stability of its basin of potential energy landscape, but without changing the basin's energy level. The underlying mechanism points toward the redistribution of the atomic free volume with a constant system-averaged value. We further find that the rejuvenation limit of this glass is its steady-flow state with self-similar inherent structures at both short- and long-time scales. Our findings refresh the understanding of glass rejuvenation and suggest that the boson peak is a better probe for the structural rejuvenation of glasses.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Fundamental Research
Fundamental Research Multidisciplinary-Multidisciplinary
CiteScore
4.00
自引率
1.60%
发文量
294
审稿时长
79 days
期刊介绍:
期刊最新文献
Structural rejuvenation of a well-aged metallic glass Reaction mechanism of toluene decomposition in non-thermal plasma: How does it compare with benzene? Event-triggered neuroadaptive predefined practical finite-time control for dynamic positioning vessels: A time-based generator approach Unsupervised learning of interacting topological phases from experimental observables Reactions with Criegee intermediates are the dominant gas-phase sink for formyl fluoride in the atmosphere
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1