{"title":"具有表面系留聚合物刷层的反渗透膜,可增强对硝酸盐、硼和砷的去除","authors":"Yian Chen , Yoram Cohen","doi":"10.1016/j.memlet.2023.100062","DOIUrl":null,"url":null,"abstract":"<div><p>Thin-film composite (TFC) polyamide (PA) RO membrane modified with a layer of tethered poly(acrylic acid) (PAA) chains displayed intrinsic rejections of nitrate, boron, As(III), and As(V) of 98.0%, 90.7%, 96%, and 99.6%, respectively. The solute permeability coefficients for nitrate, boron, As(III), and As(V) by the SNS-PAA-PA membrane were lower by 31–38%, 49–63%, 57–72% and 87–93% relative to tested commercial membranes. The above results indicate that the SNS-PAA-PA membrane should be suitable for purification of brackish source water contaminated with nitrate, boron, As(III), and As(V) to levels 1219 ppm, 2 ppm, 95 ppb, and 948 ppb, respectively. The study results suggest that there is merit in further exploration of the potential of the present approach for enhancing RO membranes performance for targeted solute removal.</p></div>","PeriodicalId":100805,"journal":{"name":"Journal of Membrane Science Letters","volume":"3 2","pages":"Article 100062"},"PeriodicalIF":4.9000,"publicationDate":"2023-09-09","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"RO membrane with a surface tethered polymer brush layer for enhanced rejection of nitrate, boron, and arsenic\",\"authors\":\"Yian Chen , Yoram Cohen\",\"doi\":\"10.1016/j.memlet.2023.100062\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>Thin-film composite (TFC) polyamide (PA) RO membrane modified with a layer of tethered poly(acrylic acid) (PAA) chains displayed intrinsic rejections of nitrate, boron, As(III), and As(V) of 98.0%, 90.7%, 96%, and 99.6%, respectively. The solute permeability coefficients for nitrate, boron, As(III), and As(V) by the SNS-PAA-PA membrane were lower by 31–38%, 49–63%, 57–72% and 87–93% relative to tested commercial membranes. The above results indicate that the SNS-PAA-PA membrane should be suitable for purification of brackish source water contaminated with nitrate, boron, As(III), and As(V) to levels 1219 ppm, 2 ppm, 95 ppb, and 948 ppb, respectively. The study results suggest that there is merit in further exploration of the potential of the present approach for enhancing RO membranes performance for targeted solute removal.</p></div>\",\"PeriodicalId\":100805,\"journal\":{\"name\":\"Journal of Membrane Science Letters\",\"volume\":\"3 2\",\"pages\":\"Article 100062\"},\"PeriodicalIF\":4.9000,\"publicationDate\":\"2023-09-09\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Membrane Science Letters\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/S2772421223000260\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"ENGINEERING, CHEMICAL\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Membrane Science Letters","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2772421223000260","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"ENGINEERING, CHEMICAL","Score":null,"Total":0}
RO membrane with a surface tethered polymer brush layer for enhanced rejection of nitrate, boron, and arsenic
Thin-film composite (TFC) polyamide (PA) RO membrane modified with a layer of tethered poly(acrylic acid) (PAA) chains displayed intrinsic rejections of nitrate, boron, As(III), and As(V) of 98.0%, 90.7%, 96%, and 99.6%, respectively. The solute permeability coefficients for nitrate, boron, As(III), and As(V) by the SNS-PAA-PA membrane were lower by 31–38%, 49–63%, 57–72% and 87–93% relative to tested commercial membranes. The above results indicate that the SNS-PAA-PA membrane should be suitable for purification of brackish source water contaminated with nitrate, boron, As(III), and As(V) to levels 1219 ppm, 2 ppm, 95 ppb, and 948 ppb, respectively. The study results suggest that there is merit in further exploration of the potential of the present approach for enhancing RO membranes performance for targeted solute removal.