IF 1.4 Q4 MATERIALS SCIENCE, MULTIDISCIPLINARY AIMS Materials Science Pub Date : 2022-01-01 DOI:10.3934/matersci.2022010
M. M. A. Filho, P. Piloto, Carlos Balsa
{"title":"钢甲板组合板在自然火灾下的承载性能","authors":"M. M. A. Filho, P. Piloto, Carlos Balsa","doi":"10.3934/matersci.2022010","DOIUrl":null,"url":null,"abstract":"Composite slabs with steel deck combine the load-bearing resistance of the steel deck and rebar with the compressive resistance of the concrete (components). Unprotected composite slabs may be exposed to natural fire conditions from below, and steel reduces its load-bearing capacity during the heating stage. In short fire events, with limited deformations, the composite slabs can recover the load-bearing capacity during the cooling stage. This research presents the validation of the numerical model and the development of a parametric study, to evaluate the load-bearing capacity during the fire event. This method includes a time step procedure, based on the average temperature calculation for each component, including the reduction coefficients applied to the design strength of each material. A new proposal is also presented to evaluate the residual load-bearing capacity. In some circumstances, the residual load-bearing can be reduced by more than 20%. The results showed that the highest variation in the load-bearing resistance of composite slabs occurs when the steel temperatures are between 20 and 600 ℃, after this temperature, the steel has already lost most of its mechanical strength. Moreover, it was observed that different heating rates and different cooling rates influence the rate of the reduction and recovery of the load-bearing capacity. It was also noticed that the lowest load-bearing capacity of the composite slabs was reached after the end of the heating phase, showing that the stability of the element during the heating phase does not guarantee fire safety during the cooling phase.","PeriodicalId":7670,"journal":{"name":"AIMS Materials Science","volume":"1 1","pages":""},"PeriodicalIF":1.4000,"publicationDate":"2022-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"4","resultStr":"{\"title\":\"The load-bearing of composite slabs with steel deck under natural fires\",\"authors\":\"M. M. A. Filho, P. Piloto, Carlos Balsa\",\"doi\":\"10.3934/matersci.2022010\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Composite slabs with steel deck combine the load-bearing resistance of the steel deck and rebar with the compressive resistance of the concrete (components). Unprotected composite slabs may be exposed to natural fire conditions from below, and steel reduces its load-bearing capacity during the heating stage. In short fire events, with limited deformations, the composite slabs can recover the load-bearing capacity during the cooling stage. This research presents the validation of the numerical model and the development of a parametric study, to evaluate the load-bearing capacity during the fire event. This method includes a time step procedure, based on the average temperature calculation for each component, including the reduction coefficients applied to the design strength of each material. A new proposal is also presented to evaluate the residual load-bearing capacity. In some circumstances, the residual load-bearing can be reduced by more than 20%. The results showed that the highest variation in the load-bearing resistance of composite slabs occurs when the steel temperatures are between 20 and 600 ℃, after this temperature, the steel has already lost most of its mechanical strength. Moreover, it was observed that different heating rates and different cooling rates influence the rate of the reduction and recovery of the load-bearing capacity. It was also noticed that the lowest load-bearing capacity of the composite slabs was reached after the end of the heating phase, showing that the stability of the element during the heating phase does not guarantee fire safety during the cooling phase.\",\"PeriodicalId\":7670,\"journal\":{\"name\":\"AIMS Materials Science\",\"volume\":\"1 1\",\"pages\":\"\"},\"PeriodicalIF\":1.4000,\"publicationDate\":\"2022-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"4\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"AIMS Materials Science\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.3934/matersci.2022010\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"MATERIALS SCIENCE, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"AIMS Materials Science","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3934/matersci.2022010","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 4

摘要

钢甲板组合板结合了钢甲板和钢筋的承重能力和混凝土(构件)的抗压能力。未保护的复合板可能暴露在下面的自然火灾条件下,并且钢在加热阶段降低了其承载能力。在短期火灾中,在有限的变形情况下,复合楼板在冷却阶段可以恢复承载能力。本研究提出了数值模型的验证和参数研究的发展,以评估火灾事件时的承载能力。该方法包括一个时间步进程序,基于每个部件的平均温度计算,包括应用于每种材料的设计强度的减少系数。提出了一种新的评价剩余承载能力的方法。在某些情况下,剩余承重可降低20%以上。结果表明:当钢的温度在20 ~ 600℃之间时,组合板的承载抗力变化最大,在此温度之后,钢的大部分机械强度已经丧失;此外,还观察到不同的加热速率和不同的冷却速率会影响承载能力的降低和恢复速度。还注意到,复合板的最低承载能力是在加热阶段结束后达到的,这表明元件在加热阶段的稳定性并不能保证冷却阶段的消防安全。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
The load-bearing of composite slabs with steel deck under natural fires
Composite slabs with steel deck combine the load-bearing resistance of the steel deck and rebar with the compressive resistance of the concrete (components). Unprotected composite slabs may be exposed to natural fire conditions from below, and steel reduces its load-bearing capacity during the heating stage. In short fire events, with limited deformations, the composite slabs can recover the load-bearing capacity during the cooling stage. This research presents the validation of the numerical model and the development of a parametric study, to evaluate the load-bearing capacity during the fire event. This method includes a time step procedure, based on the average temperature calculation for each component, including the reduction coefficients applied to the design strength of each material. A new proposal is also presented to evaluate the residual load-bearing capacity. In some circumstances, the residual load-bearing can be reduced by more than 20%. The results showed that the highest variation in the load-bearing resistance of composite slabs occurs when the steel temperatures are between 20 and 600 ℃, after this temperature, the steel has already lost most of its mechanical strength. Moreover, it was observed that different heating rates and different cooling rates influence the rate of the reduction and recovery of the load-bearing capacity. It was also noticed that the lowest load-bearing capacity of the composite slabs was reached after the end of the heating phase, showing that the stability of the element during the heating phase does not guarantee fire safety during the cooling phase.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
AIMS Materials Science
AIMS Materials Science MATERIALS SCIENCE, MULTIDISCIPLINARY-
CiteScore
3.60
自引率
0.00%
发文量
33
审稿时长
4 weeks
期刊介绍: AIMS Materials Science welcomes, but not limited to, the papers from the following topics: · Biological materials · Ceramics · Composite materials · Magnetic materials · Medical implant materials · New properties of materials · Nanoscience and nanotechnology · Polymers · Thin films.
期刊最新文献
Effect of sub-zero treatments on hardness and corrosion properties of low-alloy nickel steel Self-healing properties of augmented injectable hydrogels over time Analysis of the folding behavior of a paperboard subjected to indentation of a deviated creasing rule using the finite element method Characterization of the mechanical properties and thermal conductivity of epoxy-silica functionally graded materials Demonstration of ferroelectricity in PLD grown HfO2-ZrO2 nanolaminates
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1