{"title":"镍钛弓丝与添加铜的镍钛弓丝在人工唾液中耐腐蚀性能的差异","authors":"E. H. Habar, Fransiske Tatengkeng","doi":"10.15562/JDMFS.V5I2.1089","DOIUrl":null,"url":null,"abstract":"Objective: The aim of this experiment showed the difference of corrosion resistance between Nickel-Titanium (NiTi) archwire and NiTi archwire with additional cooper (NiTi-Cu) in artificial saliva. Material and Methods: This research was conducted in these laboratory experiments, immersed the NiTi archwires and NiTi-Cu archwires on artificial saliva at pH= 7 and incubated on 37°C, with the ratio of the archwire and the saliva was 0.02 gr: 1 ml during 1 day, 33 days and 66 days. Results: Corrosion resistances reviewed by average saliva artificial contained ion Ni after immersed 1 day of NiTi archwires and NiTi-Cu were 0.033 ± 0.000, and after immersed 33 days were 0.053 ± 0.022 and 0.101 ± 0.050, and after 66 days immersed were 0.101 ± 0.050","PeriodicalId":31119,"journal":{"name":"Journal of Dentomaxillofacial Science","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2020-08-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"5","resultStr":"{\"title\":\"The difference of corrosion resistance between NiTi archwires and NiTi with additional cooper archwires in artificial saliva\",\"authors\":\"E. H. Habar, Fransiske Tatengkeng\",\"doi\":\"10.15562/JDMFS.V5I2.1089\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Objective: The aim of this experiment showed the difference of corrosion resistance between Nickel-Titanium (NiTi) archwire and NiTi archwire with additional cooper (NiTi-Cu) in artificial saliva. Material and Methods: This research was conducted in these laboratory experiments, immersed the NiTi archwires and NiTi-Cu archwires on artificial saliva at pH= 7 and incubated on 37°C, with the ratio of the archwire and the saliva was 0.02 gr: 1 ml during 1 day, 33 days and 66 days. Results: Corrosion resistances reviewed by average saliva artificial contained ion Ni after immersed 1 day of NiTi archwires and NiTi-Cu were 0.033 ± 0.000, and after immersed 33 days were 0.053 ± 0.022 and 0.101 ± 0.050, and after 66 days immersed were 0.101 ± 0.050\",\"PeriodicalId\":31119,\"journal\":{\"name\":\"Journal of Dentomaxillofacial Science\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-08-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"5\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Dentomaxillofacial Science\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.15562/JDMFS.V5I2.1089\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Dentomaxillofacial Science","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15562/JDMFS.V5I2.1089","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 5

摘要

目的:研究人工唾液中镍钛(NiTi)弓丝与添加铜(NiTi- cu)镍钛弓丝的耐蚀性差异。材料与方法:本研究在这些实验室实验中进行,将NiTi弓丝和NiTi- cu弓丝浸入pH= 7的人工唾液中,37℃孵育,弓丝与唾液的比例为0.02 gr: 1 ml,分别进行1天、33天和66天。结果:NiTi弧线和NiTi- cu浸泡1天后的平均唾液含离子Ni的耐蚀性为0.033±0.000,浸泡33天后的耐蚀性分别为0.053±0.022和0.101±0.050,浸泡66天后的耐蚀性分别为0.101±0.050
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
The difference of corrosion resistance between NiTi archwires and NiTi with additional cooper archwires in artificial saliva
Objective: The aim of this experiment showed the difference of corrosion resistance between Nickel-Titanium (NiTi) archwire and NiTi archwire with additional cooper (NiTi-Cu) in artificial saliva. Material and Methods: This research was conducted in these laboratory experiments, immersed the NiTi archwires and NiTi-Cu archwires on artificial saliva at pH= 7 and incubated on 37°C, with the ratio of the archwire and the saliva was 0.02 gr: 1 ml during 1 day, 33 days and 66 days. Results: Corrosion resistances reviewed by average saliva artificial contained ion Ni after immersed 1 day of NiTi archwires and NiTi-Cu were 0.033 ± 0.000, and after immersed 33 days were 0.053 ± 0.022 and 0.101 ± 0.050, and after 66 days immersed were 0.101 ± 0.050
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
0.50
自引率
0.00%
发文量
0
审稿时长
16 weeks
期刊最新文献
Association between eating pattern and food neophobia in children with Autism Spectrum Disorder (ASD): Parents' perceptions Combination of surgical exposure and fixed orthodontic appliance in bilateral impacted canine Oral potentially malignant disorder awareness level among elder community in the Belawa Distric, Wajo, South Sulawesi, Indonesia Management of central diastema with high-frenulum labialis Immunohistochemistry assay of osteocalcin on bone healing with CHA-10% propolis
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1