以榴莲淀粉和虾壳聚糖为原料,添加增塑剂甘油和聚甘油,微波改性生物可降解塑料

Saud Salomo, Astri Devi Br Pakpahan, Dea Gracella Siagian, Grecy Kristina Tampubolon, Salsabila Afani, E. Eddiyanto, J. Sihombing
{"title":"以榴莲淀粉和虾壳聚糖为原料,添加增塑剂甘油和聚甘油,微波改性生物可降解塑料","authors":"Saud Salomo, Astri Devi Br Pakpahan, Dea Gracella Siagian, Grecy Kristina Tampubolon, Salsabila Afani, E. Eddiyanto, J. Sihombing","doi":"10.24114/jpkim.v13i3.29017","DOIUrl":null,"url":null,"abstract":"Plastic waste takes up to 450 years to decompose. These problems can be overcome by creating other alternatives, one of which is by using biodegradable plastic. Biodegradable plastics are plastics made from natural polymers that are easily degraded by microorganisms. This study aims to examine the effect of the amount of plasticizer on the length of the degradation process and the effect of using microwaves on the length of time for molding biodegradable plastic. This biodegradable plastic is made by combining durian seed starch, shrimp chitosan and plasticizers in the form of glycerol and polyglycerol with volume variations of 1 mL, 2 mL, 3 mL, 4 mL, and 5 mL. This polymerization was carried out using a microwave with a power of 100 watts for 60 minutes. The resulting biodegradable plastics were characterized using the FTIR test, the Mechanical Properties test, the Absorbency test, and the Biodegradation test to determine the quality of the biodegradable plastic. The results of this study indicate the greatest tensile strength value is 1.9768 MPa, the largest elongation value is 21.2772%, the smallest water absorption is 45.40% for 5 minutes, and the largest degraded mass is 0.908 grams for 7 days. Based on this research, it can be concluded that the use of polyglycerol can accelerate the plastic degradation process. In addition, the use of microwaves can speed up the molding time of biodegradable plastics.","PeriodicalId":17697,"journal":{"name":"Jurnal Pendidikan Kimia","volume":"2 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2021-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Biodegradable plastic modification from durian seed starch and shrimp chitosan with the addition of plasticiziers glycerol and polyglycerol using microwaves\",\"authors\":\"Saud Salomo, Astri Devi Br Pakpahan, Dea Gracella Siagian, Grecy Kristina Tampubolon, Salsabila Afani, E. Eddiyanto, J. Sihombing\",\"doi\":\"10.24114/jpkim.v13i3.29017\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Plastic waste takes up to 450 years to decompose. These problems can be overcome by creating other alternatives, one of which is by using biodegradable plastic. Biodegradable plastics are plastics made from natural polymers that are easily degraded by microorganisms. This study aims to examine the effect of the amount of plasticizer on the length of the degradation process and the effect of using microwaves on the length of time for molding biodegradable plastic. This biodegradable plastic is made by combining durian seed starch, shrimp chitosan and plasticizers in the form of glycerol and polyglycerol with volume variations of 1 mL, 2 mL, 3 mL, 4 mL, and 5 mL. This polymerization was carried out using a microwave with a power of 100 watts for 60 minutes. The resulting biodegradable plastics were characterized using the FTIR test, the Mechanical Properties test, the Absorbency test, and the Biodegradation test to determine the quality of the biodegradable plastic. The results of this study indicate the greatest tensile strength value is 1.9768 MPa, the largest elongation value is 21.2772%, the smallest water absorption is 45.40% for 5 minutes, and the largest degraded mass is 0.908 grams for 7 days. Based on this research, it can be concluded that the use of polyglycerol can accelerate the plastic degradation process. In addition, the use of microwaves can speed up the molding time of biodegradable plastics.\",\"PeriodicalId\":17697,\"journal\":{\"name\":\"Jurnal Pendidikan Kimia\",\"volume\":\"2 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2021-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Jurnal Pendidikan Kimia\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.24114/jpkim.v13i3.29017\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Pendidikan Kimia","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.24114/jpkim.v13i3.29017","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

塑料垃圾需要长达450年的时间才能分解。这些问题可以通过创造其他替代品来克服,其中之一就是使用可生物降解的塑料。可生物降解塑料是由天然聚合物制成的塑料,很容易被微生物降解。本研究旨在考察增塑剂用量对降解过程长度的影响,以及使用微波对生物降解塑料成型时间的影响。这种可生物降解塑料是由榴莲籽淀粉、虾壳聚糖和增塑剂以甘油和聚甘油的形式(体积变化为1ml、2ml、3ml、4ml和5ml)合成而成的。这种聚合是在100瓦功率的微波炉中进行的,时间为60分钟。通过FTIR测试、力学性能测试、吸光性测试和生物降解测试对所得生物降解塑料进行表征,以确定生物降解塑料的质量。研究结果表明:拉伸强度最大值为1.9768 MPa,伸长率最大值为21.2772%,保温5 min吸水率最小为45.40%,保温7 d最大降解质量为0.908 g。基于本研究,可以得出结论,聚甘油的使用可以加速塑料的降解过程。此外,使用微波可以加快生物降解塑料的成型时间。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Biodegradable plastic modification from durian seed starch and shrimp chitosan with the addition of plasticiziers glycerol and polyglycerol using microwaves
Plastic waste takes up to 450 years to decompose. These problems can be overcome by creating other alternatives, one of which is by using biodegradable plastic. Biodegradable plastics are plastics made from natural polymers that are easily degraded by microorganisms. This study aims to examine the effect of the amount of plasticizer on the length of the degradation process and the effect of using microwaves on the length of time for molding biodegradable plastic. This biodegradable plastic is made by combining durian seed starch, shrimp chitosan and plasticizers in the form of glycerol and polyglycerol with volume variations of 1 mL, 2 mL, 3 mL, 4 mL, and 5 mL. This polymerization was carried out using a microwave with a power of 100 watts for 60 minutes. The resulting biodegradable plastics were characterized using the FTIR test, the Mechanical Properties test, the Absorbency test, and the Biodegradation test to determine the quality of the biodegradable plastic. The results of this study indicate the greatest tensile strength value is 1.9768 MPa, the largest elongation value is 21.2772%, the smallest water absorption is 45.40% for 5 minutes, and the largest degraded mass is 0.908 grams for 7 days. Based on this research, it can be concluded that the use of polyglycerol can accelerate the plastic degradation process. In addition, the use of microwaves can speed up the molding time of biodegradable plastics.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Formulation and antibacterial activity of frankincense sap extract deodorant spray (Styrax benzoin) Comparative assessment of human salivary α-amylase inhibitor from Indonesian herbs Self-efficacy assessment in chemistry learning: Development and validation using confirmatory factor analysis Preparing of chemical bonding learning media based android using smart apps creator program The evaluation of biochemistry practicum based on several parameters of laboratory services in chemistry department Universitas Negeri Surabaya during the even semester
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1