Ca和Mg-Al改性对S50C模具钢复合夹杂物影响的对比分析

IF 0.9 4区 材料科学 Q3 METALLURGY & METALLURGICAL ENGINEERING Metallurgical Research & Technology Pub Date : 2021-01-01 DOI:10.1051/metal/2021049
Chengying Cao, Gao-feng Wang, Jie Li, Qianghua Tian, Qi Zhu, Ke-nan Ai, Jianxun Fu
{"title":"Ca和Mg-Al改性对S50C模具钢复合夹杂物影响的对比分析","authors":"Chengying Cao, Gao-feng Wang, Jie Li, Qianghua Tian, Qi Zhu, Ke-nan Ai, Jianxun Fu","doi":"10.1051/metal/2021049","DOIUrl":null,"url":null,"abstract":"At present, the effective ways to improve the cleanliness of S50C die steel are Ca or Mg-Al treatment processes. In order to explore the effect difference of two kinds of modification process of S50C killed steel, evaluate the industrial application prospect of the two processes, and clarify the modification mechanism. In this paper, the advantages of Mg-Al modification are demonstrated from the aspects of theoretical basis and actual sample modification effect. The thermodynamics and kinetics of inclusion precipitation, composition, morphology, and distribution are analyzed. The results show that: the precipitation temperature of MnS in S50C die steel is 1686 K, the corresponding solid-phase rate is 0.98. In Mg-Al modification, when the Al content is 332 ppm, the Mg content should be controlled below 14.1 ppm. When the Al content is higher than 0.02%, the Ca content should be controlled below 28.7 ppm. Kinetic calculations show that the equilibrium shape size of MnS is in the range of 0.3‑1.4 µm. Both modifications increase the nucleation rate of inclusions and control the shape and size of inclusions by pre-precipitation. Ca treatment is preventing the formation of large inclusions by forming calcium aluminate. Mg can provide more uniform nucleation sites and form smaller inclusions.","PeriodicalId":18527,"journal":{"name":"Metallurgical Research & Technology","volume":"26 1","pages":""},"PeriodicalIF":0.9000,"publicationDate":"2021-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"Comparative analysis of the effect of Ca and Mg-Al modification on the composite inclusions in S50C Die steel\",\"authors\":\"Chengying Cao, Gao-feng Wang, Jie Li, Qianghua Tian, Qi Zhu, Ke-nan Ai, Jianxun Fu\",\"doi\":\"10.1051/metal/2021049\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"At present, the effective ways to improve the cleanliness of S50C die steel are Ca or Mg-Al treatment processes. In order to explore the effect difference of two kinds of modification process of S50C killed steel, evaluate the industrial application prospect of the two processes, and clarify the modification mechanism. In this paper, the advantages of Mg-Al modification are demonstrated from the aspects of theoretical basis and actual sample modification effect. The thermodynamics and kinetics of inclusion precipitation, composition, morphology, and distribution are analyzed. The results show that: the precipitation temperature of MnS in S50C die steel is 1686 K, the corresponding solid-phase rate is 0.98. In Mg-Al modification, when the Al content is 332 ppm, the Mg content should be controlled below 14.1 ppm. When the Al content is higher than 0.02%, the Ca content should be controlled below 28.7 ppm. Kinetic calculations show that the equilibrium shape size of MnS is in the range of 0.3‑1.4 µm. Both modifications increase the nucleation rate of inclusions and control the shape and size of inclusions by pre-precipitation. Ca treatment is preventing the formation of large inclusions by forming calcium aluminate. Mg can provide more uniform nucleation sites and form smaller inclusions.\",\"PeriodicalId\":18527,\"journal\":{\"name\":\"Metallurgical Research & Technology\",\"volume\":\"26 1\",\"pages\":\"\"},\"PeriodicalIF\":0.9000,\"publicationDate\":\"2021-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Metallurgical Research & Technology\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.1051/metal/2021049\",\"RegionNum\":4,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"METALLURGY & METALLURGICAL ENGINEERING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Metallurgical Research & Technology","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1051/metal/2021049","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 1

摘要

目前,提高S50C模具钢洁净度的有效途径是Ca或Mg-Al处理工艺。为了探讨S50C钢两种改性工艺的效果差异,评价两种工艺的工业应用前景,阐明改性机理。本文从理论基础和实际样品改性效果两方面论证了Mg-Al改性的优越性。分析了夹杂物析出、组成、形貌和分布的热力学和动力学。结果表明:MnS在S50C模具钢中的析出温度为1686 K,固相速率为0.98;在Mg-Al改性中,当Al含量为332 ppm时,Mg含量应控制在14.1 ppm以下。当Al含量高于0.02%时,Ca含量应控制在28.7 ppm以下。动力学计算表明,MnS的平衡形状尺寸在0.3 ~ 1.4µm之间。这两种变质均通过预沉淀作用提高了夹杂物的成核速率,控制了夹杂物的形状和大小。钙处理通过形成铝酸钙来防止大包裹体的形成。Mg能提供更均匀的核位,形成更小的包裹体。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Comparative analysis of the effect of Ca and Mg-Al modification on the composite inclusions in S50C Die steel
At present, the effective ways to improve the cleanliness of S50C die steel are Ca or Mg-Al treatment processes. In order to explore the effect difference of two kinds of modification process of S50C killed steel, evaluate the industrial application prospect of the two processes, and clarify the modification mechanism. In this paper, the advantages of Mg-Al modification are demonstrated from the aspects of theoretical basis and actual sample modification effect. The thermodynamics and kinetics of inclusion precipitation, composition, morphology, and distribution are analyzed. The results show that: the precipitation temperature of MnS in S50C die steel is 1686 K, the corresponding solid-phase rate is 0.98. In Mg-Al modification, when the Al content is 332 ppm, the Mg content should be controlled below 14.1 ppm. When the Al content is higher than 0.02%, the Ca content should be controlled below 28.7 ppm. Kinetic calculations show that the equilibrium shape size of MnS is in the range of 0.3‑1.4 µm. Both modifications increase the nucleation rate of inclusions and control the shape and size of inclusions by pre-precipitation. Ca treatment is preventing the formation of large inclusions by forming calcium aluminate. Mg can provide more uniform nucleation sites and form smaller inclusions.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Metallurgical Research & Technology
Metallurgical Research & Technology METALLURGY & METALLURGICAL ENGINEERING-
CiteScore
1.70
自引率
9.10%
发文量
65
审稿时长
4.4 months
期刊介绍: Metallurgical Research and Technology (MRT) is a peer-reviewed bi-monthly journal publishing original high-quality research papers in areas ranging from process metallurgy to metal product properties and applications of ferrous and non-ferrous metals and alloys, including light-metals. It covers also the materials involved in the metal processing as ores, refractories and slags. The journal is listed in the citation index Web of Science and has an Impact Factor. It is highly concerned by the technological innovation as a support of the metallurgical industry at a time when it has to tackle severe challenges like energy, raw materials, sustainability, environment... Strengthening and enhancing the dialogue between science and industry is at the heart of the scope of MRT. This is why it welcomes manuscripts focusing on industrial practice, as well as basic metallurgical knowledge or review articles.
期刊最新文献
Bend forming of aluminum alloy integral panel: a review Kinetic and mechanical properties of boronized AISI 1020 steel with Baybora-2 powder The method of reducing energy consumption in large blast furnace smelting by increasing top pressure Distribution behavior and deportation of arsenic in copper top-blown smelting process Effect of slag properties and non-uniform bottom blowing gas supply mode on fluid flow and mixing behavior in converter
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1