{"title":"利用废米与米糠复合开发生物降解秸秆","authors":"H.V. Putri, M. Fallah","doi":"10.22146/aij.v8i2.76725","DOIUrl":null,"url":null,"abstract":"Plastics waste has been recently recognized as one of the most critical environmental issues. The most plastic is not recycleable and it takes 300-500 years to degraded perfectly. Plastics straw also contribute these negative impacts, so develop the biodegradable straw can be one of the solution. Natural ingredients that contain carbohydrates can be used as biodegradable straw materials are unused rice and rice bran, with glycerin from used cooking oil. This study aims to find out the effects of composition of unused rice flour and rice bran flour respectively on parameters. The parameters are the tensile strength, elongation, water uptake, and the biodegradation, then compare to the control. Statistical test were used to check, analysis, and compare between the data. The results show that combination variations in raw material flour had a significantly effect (p<0.05) on tensile strength, elongation, and biodegradation, but had not significantly effect (p≥0.05) on water uptake. Results obtained from the study of biodegradable straws for tensile strength ranges from 0.21-6.19 MPa, elongation range from 0.43-1.71%, water uptake 100%, and degraded 100%. Sample with a combination of 3 g unused rice flour : 0.5 g rice bran flour, has the highest tensile strength and elongation value and degraded within 4 days. However, the sample can not be used as an alternative to plastic straw because it does not have similar characteristics.","PeriodicalId":14920,"journal":{"name":"Journal of Agroindustrial Technology","volume":"31 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2022-08-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"Development of Biodegradable Straw using Combination of Unused Rice and Rice Bran\",\"authors\":\"H.V. Putri, M. Fallah\",\"doi\":\"10.22146/aij.v8i2.76725\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Plastics waste has been recently recognized as one of the most critical environmental issues. The most plastic is not recycleable and it takes 300-500 years to degraded perfectly. Plastics straw also contribute these negative impacts, so develop the biodegradable straw can be one of the solution. Natural ingredients that contain carbohydrates can be used as biodegradable straw materials are unused rice and rice bran, with glycerin from used cooking oil. This study aims to find out the effects of composition of unused rice flour and rice bran flour respectively on parameters. The parameters are the tensile strength, elongation, water uptake, and the biodegradation, then compare to the control. Statistical test were used to check, analysis, and compare between the data. The results show that combination variations in raw material flour had a significantly effect (p<0.05) on tensile strength, elongation, and biodegradation, but had not significantly effect (p≥0.05) on water uptake. Results obtained from the study of biodegradable straws for tensile strength ranges from 0.21-6.19 MPa, elongation range from 0.43-1.71%, water uptake 100%, and degraded 100%. Sample with a combination of 3 g unused rice flour : 0.5 g rice bran flour, has the highest tensile strength and elongation value and degraded within 4 days. However, the sample can not be used as an alternative to plastic straw because it does not have similar characteristics.\",\"PeriodicalId\":14920,\"journal\":{\"name\":\"Journal of Agroindustrial Technology\",\"volume\":\"31 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2022-08-30\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Agroindustrial Technology\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.22146/aij.v8i2.76725\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Agroindustrial Technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.22146/aij.v8i2.76725","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

摘要

塑料垃圾最近被认为是最严重的环境问题之一。大多数塑料是不可回收的,需要300-500年才能完全降解。塑料吸管也造成了这些负面影响,因此开发可生物降解的吸管可以是解决方案之一。含有碳水化合物的天然成分可以用作可生物降解的秸秆材料,如未使用的大米和米糠,以及用过的食用油中的甘油。本研究旨在找出未使用的米粉和米糠粉的组成分别对参数的影响。参数是拉伸强度、伸长率、吸水率和生物降解率,然后与对照进行比较。采用统计学检验对数据进行检验、分析和比较。结果表明:不同原料面粉组合对玉米的抗拉强度、伸长率和生物降解有显著影响(p<0.05),对水分吸收无显著影响(p≥0.05);研究结果表明,生物降解秸秆的抗拉强度范围为0.21-6.19 MPa,伸长率范围为0.43-1.71%,吸水率100%,降解率100%。样品用3g未使用米粉:0.5 g米糠粉组合,抗拉强度和延伸值最高,4天内降解。然而,样品不能作为塑料吸管的替代品,因为它不具有相似的特性。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Development of Biodegradable Straw using Combination of Unused Rice and Rice Bran
Plastics waste has been recently recognized as one of the most critical environmental issues. The most plastic is not recycleable and it takes 300-500 years to degraded perfectly. Plastics straw also contribute these negative impacts, so develop the biodegradable straw can be one of the solution. Natural ingredients that contain carbohydrates can be used as biodegradable straw materials are unused rice and rice bran, with glycerin from used cooking oil. This study aims to find out the effects of composition of unused rice flour and rice bran flour respectively on parameters. The parameters are the tensile strength, elongation, water uptake, and the biodegradation, then compare to the control. Statistical test were used to check, analysis, and compare between the data. The results show that combination variations in raw material flour had a significantly effect (p<0.05) on tensile strength, elongation, and biodegradation, but had not significantly effect (p≥0.05) on water uptake. Results obtained from the study of biodegradable straws for tensile strength ranges from 0.21-6.19 MPa, elongation range from 0.43-1.71%, water uptake 100%, and degraded 100%. Sample with a combination of 3 g unused rice flour : 0.5 g rice bran flour, has the highest tensile strength and elongation value and degraded within 4 days. However, the sample can not be used as an alternative to plastic straw because it does not have similar characteristics.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Frozen Tilapia Fillets Business Process Analysis Using Integration Definition for Function Modelling Fried Chicken Consumer’s Preference and Purchase Decision Analysis During Covid 19 Pandemic Era Potential Risk of Work Accident in The Production Process of Gudeg Chicken using The Failure Mode and Effect Analysis (FMEA) Method Analysis of Consumers’ Preferences for Melon Using the Conjoint Method Production of Biodegradable Straw from Banana Peel
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1