{"title":"二次枝晶臂间距与凝固条件的关系——ⅱ。Sr和Sb处理的Al-7 Si-0.5 Mg合金","authors":"Q. S. Hamed, R. Elliott","doi":"10.1080/09534962.1993.11819125","DOIUrl":null,"url":null,"abstract":"AbstractSteady-state directional solidification studies are described for Sr- and Sb-treated commercial purity Al-7 Si-0.5 Mg (LM25) casting alloys. The minor additions refine the secondary dendrit...","PeriodicalId":9691,"journal":{"name":"Cast Metals","volume":"90 1","pages":"42-46"},"PeriodicalIF":0.0000,"publicationDate":"1993-03-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"6","resultStr":"{\"title\":\"The Dependence of Secondary Dendrite Arm Spacing on Solidification Conditions—II. Al-7 Si-0.5 Mg Alloys treated with Sr and Sb\",\"authors\":\"Q. S. Hamed, R. Elliott\",\"doi\":\"10.1080/09534962.1993.11819125\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"AbstractSteady-state directional solidification studies are described for Sr- and Sb-treated commercial purity Al-7 Si-0.5 Mg (LM25) casting alloys. The minor additions refine the secondary dendrit...\",\"PeriodicalId\":9691,\"journal\":{\"name\":\"Cast Metals\",\"volume\":\"90 1\",\"pages\":\"42-46\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1993-03-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"6\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Cast Metals\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1080/09534962.1993.11819125\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Cast Metals","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/09534962.1993.11819125","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
The Dependence of Secondary Dendrite Arm Spacing on Solidification Conditions—II. Al-7 Si-0.5 Mg Alloys treated with Sr and Sb
AbstractSteady-state directional solidification studies are described for Sr- and Sb-treated commercial purity Al-7 Si-0.5 Mg (LM25) casting alloys. The minor additions refine the secondary dendrit...