{"title":"Paper ID: HP006","authors":"Xiaobing Shan, Peixuan Wu, Z.Y. Cheng","doi":"10.1109/ISAF.2008.4693736","DOIUrl":null,"url":null,"abstract":"The development of high-k composites based on CaCu3Ti4O12 (CCTO) ceramic powder is reported. The CCTO ceramic powders were prepared by traditional sintering method and were milled with a relative uniform size. Based on solution casting method, the composite using P(VDF-TrFE) copolymer as matrix and CCTO powders as filler were prepared and its dielectric response were characterized. The dielectric properties of the 0¿3 composite with micro-size and nano-size CCTO particle, as well as different polymer matrixes were determined. The 0¿3 composites exhibit a very high dielectric constant, more than 1700 at 1 kHz at room temperature after surface modification.","PeriodicalId":228914,"journal":{"name":"2008 17th IEEE International Symposium on the Applications of Ferroelectrics","volume":"27 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2008-12-02","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2008 17th IEEE International Symposium on the Applications of Ferroelectrics","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ISAF.2008.4693736","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The development of high-k composites based on CaCu3Ti4O12 (CCTO) ceramic powder is reported. The CCTO ceramic powders were prepared by traditional sintering method and were milled with a relative uniform size. Based on solution casting method, the composite using P(VDF-TrFE) copolymer as matrix and CCTO powders as filler were prepared and its dielectric response were characterized. The dielectric properties of the 0¿3 composite with micro-size and nano-size CCTO particle, as well as different polymer matrixes were determined. The 0¿3 composites exhibit a very high dielectric constant, more than 1700 at 1 kHz at room temperature after surface modification.