Impact of catalyst layer morphology on the operation of high temperature PEM fuel cells

IF 5.4 Q2 CHEMISTRY, PHYSICAL Journal of Power Sources Advances Pub Date : 2021-02-01 DOI:10.1016/j.powera.2020.100042
N. Bevilacqua , T. Asset , M.A. Schmid , H. Markötter , I. Manke , P. Atanassov , R. Zeis
{"title":"Impact of catalyst layer morphology on the operation of high temperature PEM fuel cells","authors":"N. Bevilacqua ,&nbsp;T. Asset ,&nbsp;M.A. Schmid ,&nbsp;H. Markötter ,&nbsp;I. Manke ,&nbsp;P. Atanassov ,&nbsp;R. Zeis","doi":"10.1016/j.powera.2020.100042","DOIUrl":null,"url":null,"abstract":"<div><p>Electrochemical impedance spectroscopy (EIS) is a well-established method to analyze a polymer electrolyte membrane fuel cell (PEMFC). However, without further data processing, the impedance spectrum yields only qualitative insight into the mechanism and individual contribution of transport, kinetics, and ohmic losses to the overall fuel cell limitations. The distribution of relaxation times (DRT) method allows quantifying each of these polarization losses and evaluates their contribution to a given electrocatalyst's depreciated performances. We coupled this method with a detailed morphology study to investigate the impact of the 3D-structure on the processes occurring inside a high-temperature polymer electrolyte membrane fuel cell (HT-PEMFC). We tested a platinum catalyst (Pt/C), a platinum-cobalt alloy catalyst (Pt<sub>3</sub>Co/C), and a platinum group metal-free iron-nitrogen-carbon (Fe–N–C) catalyst. We found that the hampered mass transport in the latter is mainly responsible for its low performance in the MEA (along with its decreased intrinsic performances for the ORR reaction). The better performance of the alloy catalyst can be explained by both improved mass transport and a lower ORR resistance. Furthermore, single-cell tests show that the catalyst layer morphology influences the distribution of phosphoric acid during conditioning.</p></div>","PeriodicalId":34318,"journal":{"name":"Journal of Power Sources Advances","volume":null,"pages":null},"PeriodicalIF":5.4000,"publicationDate":"2021-02-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1016/j.powera.2020.100042","citationCount":"23","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Power Sources Advances","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2666248520300421","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"CHEMISTRY, PHYSICAL","Score":null,"Total":0}
引用次数: 23

Abstract

Electrochemical impedance spectroscopy (EIS) is a well-established method to analyze a polymer electrolyte membrane fuel cell (PEMFC). However, without further data processing, the impedance spectrum yields only qualitative insight into the mechanism and individual contribution of transport, kinetics, and ohmic losses to the overall fuel cell limitations. The distribution of relaxation times (DRT) method allows quantifying each of these polarization losses and evaluates their contribution to a given electrocatalyst's depreciated performances. We coupled this method with a detailed morphology study to investigate the impact of the 3D-structure on the processes occurring inside a high-temperature polymer electrolyte membrane fuel cell (HT-PEMFC). We tested a platinum catalyst (Pt/C), a platinum-cobalt alloy catalyst (Pt3Co/C), and a platinum group metal-free iron-nitrogen-carbon (Fe–N–C) catalyst. We found that the hampered mass transport in the latter is mainly responsible for its low performance in the MEA (along with its decreased intrinsic performances for the ORR reaction). The better performance of the alloy catalyst can be explained by both improved mass transport and a lower ORR resistance. Furthermore, single-cell tests show that the catalyst layer morphology influences the distribution of phosphoric acid during conditioning.

Abstract Image

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
催化剂层形态对高温PEM燃料电池性能的影响
电化学阻抗谱(EIS)是一种成熟的聚合物电解质膜燃料电池(PEMFC)分析方法。然而,如果没有进一步的数据处理,阻抗谱只能定性地了解传输、动力学和欧姆损失对整体燃料电池局限性的机制和个人贡献。弛豫时间分布(DRT)方法可以量化每种极化损耗,并评估它们对给定电催化剂的贬值性能的贡献。我们将这种方法与详细的形态学研究相结合,研究了3d结构对高温聚合物电解质膜燃料电池(HT-PEMFC)内部过程的影响。我们测试了一种铂催化剂(Pt/C)、一种铂钴合金催化剂(Pt3Co/C)和一种不含铂族金属的铁氮碳(Fe-N-C)催化剂。我们发现后者的阻碍质量运输是其在MEA中的低性能的主要原因(以及其在ORR反应中的内在性能下降)。合金催化剂的优良性能可以用质量传递的改善和ORR阻力的降低来解释。此外,单电池试验表明,催化剂层的形态影响了调理过程中磷酸的分布。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
CiteScore
9.10
自引率
0.00%
发文量
18
审稿时长
64 days
期刊最新文献
Formulating PEO-polycarbonate blends as solid polymer electrolytes by solvent-free extrusion Enhancing performance and sustainability of lithium manganese oxide cathodes with a poly(ionic liquid) binder and ionic liquid electrolyte Enhancing the stability of sodium-ion capacitors by introducing glyoxylic-acetal based electrolyte The implementation of a voltage-based tunneling mechanism in aging models for lithium-ion batteries Electronic structure evolution upon lithiation: A Li K-edge study of silicon oxide anode through X-ray Raman spectroscopy
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1