REASON OF PITTING CORROSION OF MARTENSITIC STEELIN SEA WATER

M.I. Baikenov
{"title":"REASON OF PITTING CORROSION OF MARTENSITIC STEELIN SEA WATER","authors":"M.I. Baikenov","doi":"10.31489/2024no1/38-48","DOIUrl":null,"url":null,"abstract":"Abstract. The assumption that corrosion of products from X17 martensitic stainless steel in seawater occurs due to incomplete oxidation of chromium atoms in cells on the surface of the products is made in the presented work. Incomplete oxidation of chromium atoms occurs in the cells of X17 steel. This is due to the fact that oxygen molecules at temperatures up to 350 °C not having enough energy for chemical interaction with trivalent chromium atoms entering the cubic body-centeredcells of martensitic stainless steel. There is a significant decrease in the corrosion rate after placing X17 stainless steel products in 5% iodine solution in ethanol after pre-treatment of the product surface with active forms of oxygen. The treatment was carried out during 12 hours with chemically active forms of oxygen (ozone and singlet oxygen) at a temperature of 350 °С. Most of the chromium atoms on the surface of X17 steel samples were completely oxidized as a result of 12 hours exposure to highly active forms of oxygen. The density of the oxide passivation layer on the surface of the products increased significantly as a result of the formation of new bonds CHROMIUM -OXYGEN -CHROMIUM. This resulted in increased corrosion resistance. The rate of interaction with an alcohol solution containing halogen ions was reduced by 71% for the samples with the oxide passivation layer compared to samples of untreated X17 steel.","PeriodicalId":11789,"journal":{"name":"Eurasian Physical Technical Journal","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2024-03-29","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Eurasian Physical Technical Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.31489/2024no1/38-48","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"Engineering","Score":null,"Total":0}
引用次数: 0

Abstract

Abstract. The assumption that corrosion of products from X17 martensitic stainless steel in seawater occurs due to incomplete oxidation of chromium atoms in cells on the surface of the products is made in the presented work. Incomplete oxidation of chromium atoms occurs in the cells of X17 steel. This is due to the fact that oxygen molecules at temperatures up to 350 °C not having enough energy for chemical interaction with trivalent chromium atoms entering the cubic body-centeredcells of martensitic stainless steel. There is a significant decrease in the corrosion rate after placing X17 stainless steel products in 5% iodine solution in ethanol after pre-treatment of the product surface with active forms of oxygen. The treatment was carried out during 12 hours with chemically active forms of oxygen (ozone and singlet oxygen) at a temperature of 350 °С. Most of the chromium atoms on the surface of X17 steel samples were completely oxidized as a result of 12 hours exposure to highly active forms of oxygen. The density of the oxide passivation layer on the surface of the products increased significantly as a result of the formation of new bonds CHROMIUM -OXYGEN -CHROMIUM. This resulted in increased corrosion resistance. The rate of interaction with an alcohol solution containing halogen ions was reduced by 71% for the samples with the oxide passivation layer compared to samples of untreated X17 steel.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
马氏体钢在海水中发生点蚀的原因
摘要本文假定 X17 马氏体不锈钢产品在海水中的腐蚀是由于产品表面晶胞中铬原子的不完全氧化造成的。铬原子的不完全氧化发生在 X17 钢的晶胞中。这是由于氧分子在高达 350 °C 的温度下没有足够的能量与进入马氏体不锈钢立方体中心电池的三价铬原子发生化学作用。在用活性氧预处理产品表面后,将 X17 不锈钢产品放入 5%的碘乙醇溶液中,其腐蚀率明显降低。用化学活性氧(臭氧和单线态氧)在 350 °С 的温度下进行了 12 小时的处理。在高活性氧环境中暴露 12 小时后,X17 钢样品表面的大部分铬原子完全氧化。由于形成了新的铬-氧-铬键,产品表面氧化物钝化层的密度显著增加。从而提高了耐腐蚀性。与未经处理的 X17 钢样品相比,带有氧化物钝化层的样品与含有卤素离子的酒精溶液的相互作用率降低了 71%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
CiteScore
1.10
自引率
0.00%
发文量
15
期刊最新文献
AUTOMATED CONTROL OFTHE THIN FILMS ELECTRICALCONDUCTIVITY BY THE EDDY CURRENT METHOD SIMULATION OF MULTIPOINT CONTACT UNDER THERMOELECTRIC TESTING TUDY OF THE INFLUENCE OF THE ACCUMULATED DOSE OF DAMAGE IN THE NEAR-SURFACE LAYER ON RESISTANCE TO EXTERNAL INFLUENCES ASSOCIATED WITH CORROSION PROCESSES DURING HIGH-TEMPERATURE ANNEALING Методика измерения диэлектрических коэффициентов полярных жидкостей в диапазоне микроволн ANALYSIS OF METHODS FOR SIMULATING THE DECAY HEAT IN CORIUM WHEN MODELING A SEVERE ACCIDENTS AT NUCLEAR POWER PLANT
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1