{"title":"Calcium Fluoride Precipitation and Deposition From 12 mmol/L Fluoride Solutions With Different Calcium Addition Rates.","authors":"M Markovic, S Takagi, L C Chow, S Frukhtbeyn","doi":"10.6028/jres.114.021","DOIUrl":null,"url":null,"abstract":"<p><p>The effects of different Ca-addition rates on calcium fluoride (CaF2) precipitation and deposition were investigated in 12 mmol/L sodium fluoride solutions to which 0.1 mol/L calcium chloride solution was continuously added at average rates of (5, 7.5, 10, 12.5, 15 or 20) mmol L(-1) min(-1). The changes in ionic fluoride and calcium concentrations, as well as turbidity, were continuously recorded by F and Ca electrodes, and a fiber optic based spectrophotometer, respectively. The F(-) concentration decreased and turbidity increased with time indicating precipitation of CaF2. For the systems with Ca-addition rates of (5, 7.5, 10, 12.5, 15, and 20) mmol L(-1) min(-1), the 1 min CaF2 depositions in the model substrate (cellulose filter paper, pores 0.2 µm) expressed as mean ± SD of deposited F per substrate surface area were (3.78 ± 0.31, 11.45 ± 0.89, 9.31 ± 0.68, 8.20 ± 0.56, 6.63 ± 0.43, and 2.09 ± 0.28) µg/cm(2), respectively (n = 10 for each group). The 1-min F depositions did not show positive correlation to Ca-addition rates. The lowest 1-min F deposition was obtained in the systems with the highest Ca-addition rate of 20 mmol L(-1) min(-1) for which CaF2 precipitation rate reached the maximum value of 0.31 mmol L(-1) s(-1) almost immediately after beginning of reaction (6 s). The largest 1-min F depositions were obtained from the systems with Ca addition rates of (7.5 to 12.5) mmol L(-1) min(-1) in which CaF2 precipitation rates continuously increased reaching the maximum values of (0.13 to 0.20) mmol L(-1) s(-1) after (18 to 29) s, respectively. The 1-min F depositions were greatly enhanced in comparison with the control F solutions that did not have continuous Ca-addition. This indicates that continuous Ca addition that controls the rate of CaF2 formation could be a critical factor for larger F depositions from F solutions. The efficacy of conventional F mouthrinses could be improved with addition of a substance that continuously releases Ca.</p>","PeriodicalId":17039,"journal":{"name":"Journal of Research of the National Institute of Standards and Technology","volume":"114 5","pages":"293-301"},"PeriodicalIF":1.5000,"publicationDate":"2009-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.6028/jres.114.021","citationCount":"14","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Research of the National Institute of Standards and Technology","FirstCategoryId":"5","ListUrlMain":"https://doi.org/10.6028/jres.114.021","RegionNum":4,"RegionCategory":"工程技术","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2009/9/1 0:00:00","PubModel":"Print","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 14
Abstract
The effects of different Ca-addition rates on calcium fluoride (CaF2) precipitation and deposition were investigated in 12 mmol/L sodium fluoride solutions to which 0.1 mol/L calcium chloride solution was continuously added at average rates of (5, 7.5, 10, 12.5, 15 or 20) mmol L(-1) min(-1). The changes in ionic fluoride and calcium concentrations, as well as turbidity, were continuously recorded by F and Ca electrodes, and a fiber optic based spectrophotometer, respectively. The F(-) concentration decreased and turbidity increased with time indicating precipitation of CaF2. For the systems with Ca-addition rates of (5, 7.5, 10, 12.5, 15, and 20) mmol L(-1) min(-1), the 1 min CaF2 depositions in the model substrate (cellulose filter paper, pores 0.2 µm) expressed as mean ± SD of deposited F per substrate surface area were (3.78 ± 0.31, 11.45 ± 0.89, 9.31 ± 0.68, 8.20 ± 0.56, 6.63 ± 0.43, and 2.09 ± 0.28) µg/cm(2), respectively (n = 10 for each group). The 1-min F depositions did not show positive correlation to Ca-addition rates. The lowest 1-min F deposition was obtained in the systems with the highest Ca-addition rate of 20 mmol L(-1) min(-1) for which CaF2 precipitation rate reached the maximum value of 0.31 mmol L(-1) s(-1) almost immediately after beginning of reaction (6 s). The largest 1-min F depositions were obtained from the systems with Ca addition rates of (7.5 to 12.5) mmol L(-1) min(-1) in which CaF2 precipitation rates continuously increased reaching the maximum values of (0.13 to 0.20) mmol L(-1) s(-1) after (18 to 29) s, respectively. The 1-min F depositions were greatly enhanced in comparison with the control F solutions that did not have continuous Ca-addition. This indicates that continuous Ca addition that controls the rate of CaF2 formation could be a critical factor for larger F depositions from F solutions. The efficacy of conventional F mouthrinses could be improved with addition of a substance that continuously releases Ca.
期刊介绍:
The Journal of Research of the National Institute of Standards and Technology is the flagship publication of the National Institute of Standards and Technology. It has been published under various titles and forms since 1904, with its roots as Scientific Papers issued as the Bulletin of the Bureau of Standards.
In 1928, the Scientific Papers were combined with Technologic Papers, which reported results of investigations of material and methods of testing. This new publication was titled the Bureau of Standards Journal of Research.
The Journal of Research of NIST reports NIST research and development in metrology and related fields of physical science, engineering, applied mathematics, statistics, biotechnology, information technology.