{"title":"Extraction of gold from boulangerite ore using sodium cyanide","authors":"Sajjad Ali","doi":"10.54693/piche.04721","DOIUrl":null,"url":null,"abstract":"Present study focuses over the extraction of gold via sodium cyanide (NaCN) from boulangerite ore. Since the presence of antimony hinders the extraction of gold by cyanidation therefore, the ore was first treated with sodium sulphide (Na2S) and sodium hydroxide (NaOH) to remove/minimize the antimony content. Gold extraction via cyanidation was then studied for different parameters including concentration of NaCN, time effect and influence of temperature on leaching of gold. It was observed that extraction of gold increases with increase in concentration of NaCN and ore amount. Maximum leaching of gold (52.89 - 76.53 %) was carried out at 80 oC, 100 minutes leaching time, 300 rpm and a pH level of 10.5.","PeriodicalId":17383,"journal":{"name":"Journal of the Pakistan Institute of Chemical Engineers","volume":null,"pages":null},"PeriodicalIF":0.1000,"publicationDate":"2020-04-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of the Pakistan Institute of Chemical Engineers","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.54693/piche.04721","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"ENGINEERING, CHEMICAL","Score":null,"Total":0}
引用次数: 0
Abstract
Present study focuses over the extraction of gold via sodium cyanide (NaCN) from boulangerite ore. Since the presence of antimony hinders the extraction of gold by cyanidation therefore, the ore was first treated with sodium sulphide (Na2S) and sodium hydroxide (NaOH) to remove/minimize the antimony content. Gold extraction via cyanidation was then studied for different parameters including concentration of NaCN, time effect and influence of temperature on leaching of gold. It was observed that extraction of gold increases with increase in concentration of NaCN and ore amount. Maximum leaching of gold (52.89 - 76.53 %) was carried out at 80 oC, 100 minutes leaching time, 300 rpm and a pH level of 10.5.