Investigation of Wall Thickness, Corrosion, and Deposits in Industrial Pipelines Using Radiographic Technique

IF 1.5 Q4 ELECTROCHEMISTRY International Journal of Corrosion Pub Date : 2023-07-24 DOI:10.1155/2023/4924399
P. Amoah, Sandyson Owusu-Poku, Gordon Asartenga Ajubala
{"title":"Investigation of Wall Thickness, Corrosion, and Deposits in Industrial Pipelines Using Radiographic Technique","authors":"P. Amoah, Sandyson Owusu-Poku, Gordon Asartenga Ajubala","doi":"10.1155/2023/4924399","DOIUrl":null,"url":null,"abstract":"In this study, radiographic techniques were used to inspect large-diameter pipes that are used for transporting fluids in some industries in Ghana. Radiographic approaches such as the double wall technique (DWT) and tangential radiographic technique (TRT) were used to evaluate the remaining wall thickness, deposits, and corrosion in the pipes. Two steel pipes with known varying wall thicknesses ranging from 4.00 mm to 13.00 mm with a diameter of 150.00 mm were examined to authenticate the accuracy and reliability of the tangential method that was used to measure the remaining wall thickness. The tangential configuration resulted in a higher material thickness, which therefore required more time of exposure compared to the DWT method. The exposure angle of the source to the tangential part of the specimen was approximately 87°. The film generated was compared with a normal pipe piece that was not machined to serve as a control. From the radiograph obtained, an average of 6 and 7 rounded indications depicting pitting corrosion were revealed on the radiograph of the internally and externally fabricated pipe, respectively. Radiographs after the TRT revealed that the recorded wall thickness obtained from the film is about twice the value of the calculated true wall thickness.","PeriodicalId":13893,"journal":{"name":"International Journal of Corrosion","volume":null,"pages":null},"PeriodicalIF":1.5000,"publicationDate":"2023-07-24","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Corrosion","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1155/2023/4924399","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"ELECTROCHEMISTRY","Score":null,"Total":0}
引用次数: 0

Abstract

In this study, radiographic techniques were used to inspect large-diameter pipes that are used for transporting fluids in some industries in Ghana. Radiographic approaches such as the double wall technique (DWT) and tangential radiographic technique (TRT) were used to evaluate the remaining wall thickness, deposits, and corrosion in the pipes. Two steel pipes with known varying wall thicknesses ranging from 4.00 mm to 13.00 mm with a diameter of 150.00 mm were examined to authenticate the accuracy and reliability of the tangential method that was used to measure the remaining wall thickness. The tangential configuration resulted in a higher material thickness, which therefore required more time of exposure compared to the DWT method. The exposure angle of the source to the tangential part of the specimen was approximately 87°. The film generated was compared with a normal pipe piece that was not machined to serve as a control. From the radiograph obtained, an average of 6 and 7 rounded indications depicting pitting corrosion were revealed on the radiograph of the internally and externally fabricated pipe, respectively. Radiographs after the TRT revealed that the recorded wall thickness obtained from the film is about twice the value of the calculated true wall thickness.
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
用射线照相技术研究工业管道的壁厚、腐蚀和沉积
在这项研究中,射线照相技术被用于检查加纳一些行业中用于输送流体的大直径管道。射线照相方法,如双壁技术(DWT)和切向射线照相技术(TRT),用于评估管道中的剩余壁厚、沉积物和腐蚀。两个已知壁厚变化范围为4.00的钢管 mm至13.00 mm,直径150.00 mm,以验证用于测量剩余壁厚的切向法的准确性和可靠性。切向配置导致更高的材料厚度,因此与DWT方法相比,这需要更多的曝光时间。光源与试样切向部分的暴露角度约为87°。将产生的薄膜与未经机械加工的正常管件进行比较,以用作对照。从获得的射线照片中,内部和外部制造的管道的射线照片上分别显示了平均6个和7个圆形显示,显示了点蚀。TRT后的射线照片显示,从薄膜中获得的记录壁厚大约是计算出的真实壁厚值的两倍。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 去求助
来源期刊
CiteScore
5.70
自引率
0.00%
发文量
8
审稿时长
14 weeks
期刊最新文献
Empirical Study of the Effect of Nanocoolant Particles on Corrosion Rate of 316 Stainless Steel Walk-Through Corrosion Assessment of Slurry Pipeline Using Machine Learning Corrosion Behaviour of a Cr2O3 Coating on Mild Steel in Synthetic Mine Water The Inhibitory Properties of the Ambroxol Derivative on the Corrosion of Mild Steel in Hydrochloric Acid Medium Investigation of Wall Thickness, Corrosion, and Deposits in Industrial Pipelines Using Radiographic Technique
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1