{"title":"Effect of sensitization on corrosion properties of TIG welded Al-Mg alloy","authors":"L. Radović, J. Marinković","doi":"10.5937/STR2001047R","DOIUrl":null,"url":null,"abstract":"The effect of sensitization on the intergranular corrosion (IGC) of TIG welded AlMg6Mn was investigated by means of scanning electron microscopy (SEM) and corrosion NAMLT tests. The as-received hot rolled AlMg6Mn alloy plates with a thickness of 8 mm were welded by TIG welding with S-AlMg5 as a filler material. Specimens were sensitized at 100°C for 7 days. It was found that welded specimens are sensitive to IGC. The. mass loss in NAML test was 106.7 mg/cm². The welding increases the susceptibility to IGC, since the mass loss of the base metal at the same test was 70.7 mg/cm². The increase of susceptibility to IGC is attributed to significant continually precipitated Mg-rich phase along the grain boundaries during the sensitization treatment.","PeriodicalId":33842,"journal":{"name":"Scientific Technical Review","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2020-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Scientific Technical Review","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5937/STR2001047R","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The effect of sensitization on the intergranular corrosion (IGC) of TIG welded AlMg6Mn was investigated by means of scanning electron microscopy (SEM) and corrosion NAMLT tests. The as-received hot rolled AlMg6Mn alloy plates with a thickness of 8 mm were welded by TIG welding with S-AlMg5 as a filler material. Specimens were sensitized at 100°C for 7 days. It was found that welded specimens are sensitive to IGC. The. mass loss in NAML test was 106.7 mg/cm². The welding increases the susceptibility to IGC, since the mass loss of the base metal at the same test was 70.7 mg/cm². The increase of susceptibility to IGC is attributed to significant continually precipitated Mg-rich phase along the grain boundaries during the sensitization treatment.