{"title":"Synthesis of Nanocrystalline CdS by SILAR and Their Characterization","authors":"P. P. Chandra, A. Mukherjee, P. Mitra","doi":"10.1155/2014/138163","DOIUrl":null,"url":null,"abstract":"A simple and cost effective chemical technique has been utilized to prepare cadmium sulphide (CdS) nanoparticles at room temperature. The sample is characterized with XRD (X-ray diffractometer), SEM (scanning electron microscope), TEM (transmission electron microscope), FTIR (Fourier transform infrared), EDX (energy dispersive X-rays), and UV-VIS (ultraviolet visible) spectrophotometer. The particle size estimated using X-ray line broadening method is ~21.5 nm. While particle size estimation, both instrumental and strain broadening was taken into account. The lattice strain was evaluated using Williamson-Hall equation. SEM illustrates formation of submicron size crystallites and TEM image gives a particle size of ~23.5 nm. The characteristic stretching vibration frequency of CdS was observed in the absorption band in FTIR spectrum. Optical absorption study exhibits a band gap energy value of about 2.44 eV.","PeriodicalId":17611,"journal":{"name":"Journal: Materials","volume":"233 1","pages":"1-6"},"PeriodicalIF":0.0000,"publicationDate":"2014-06-17","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"19","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal: Materials","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1155/2014/138163","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 19
Abstract
A simple and cost effective chemical technique has been utilized to prepare cadmium sulphide (CdS) nanoparticles at room temperature. The sample is characterized with XRD (X-ray diffractometer), SEM (scanning electron microscope), TEM (transmission electron microscope), FTIR (Fourier transform infrared), EDX (energy dispersive X-rays), and UV-VIS (ultraviolet visible) spectrophotometer. The particle size estimated using X-ray line broadening method is ~21.5 nm. While particle size estimation, both instrumental and strain broadening was taken into account. The lattice strain was evaluated using Williamson-Hall equation. SEM illustrates formation of submicron size crystallites and TEM image gives a particle size of ~23.5 nm. The characteristic stretching vibration frequency of CdS was observed in the absorption band in FTIR spectrum. Optical absorption study exhibits a band gap energy value of about 2.44 eV.