{"title":"Effect of Rolling and Heat Treatment on the Irreversible Magnetization in Nickel–Chromium Wire","authors":"A. Wafik","doi":"10.1002/PSSA.2211110127","DOIUrl":null,"url":null,"abstract":"The mean potential difference (UB) of Barkhausen jumps and the frequency of the cluster of jumps (FB) are measured as a function of the percentage of thickness reduction. An increase of the percentage of thickness reduction up to 55% causes a decrease of UB and FB. UB vanishes at certain values of the magnetizing frequencies. The vanishing magnetizing frequency depends on the percentage of thickness reduction. The vanishing of UB is attributed to the produced eddy current in the sample. Heat treatment has a considerable effecton both UB and the vanishing magnetizing frequency. \n \n \n \nDie mittlere Potentialdifferenz (UB) von Barkhausensprungen und die Frequenz der Sprungcluster (FB) werden als Funktion der prozentualen Dickenreduzierung gemessen. Der prozentuale Anstieg der Dickenreduzierung bis zu 55% verursacht den Abfall von UB und FB. UB verschwindet bei gewissen Werten der Magnetisierungsfrequenz. Die verschwindende Magnetisierungsfrequenz hangt von der prozentualen Dickenreduzierung ab. Das Verschwinden von UB wird den Wirbelstromen in der Probe zugeordnet. Warmebehandlung hat einen betrachtlichen Einflus sowohl auf UB als auch auf die verschwindende Magnetisierungsfrequenz.","PeriodicalId":87717,"journal":{"name":"Physica status solidi (A): Applied research","volume":"85 1","pages":"265-269"},"PeriodicalIF":0.0000,"publicationDate":"1989-01-16","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"5","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Physica status solidi (A): Applied research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1002/PSSA.2211110127","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 5
Abstract
The mean potential difference (UB) of Barkhausen jumps and the frequency of the cluster of jumps (FB) are measured as a function of the percentage of thickness reduction. An increase of the percentage of thickness reduction up to 55% causes a decrease of UB and FB. UB vanishes at certain values of the magnetizing frequencies. The vanishing magnetizing frequency depends on the percentage of thickness reduction. The vanishing of UB is attributed to the produced eddy current in the sample. Heat treatment has a considerable effecton both UB and the vanishing magnetizing frequency.
Die mittlere Potentialdifferenz (UB) von Barkhausensprungen und die Frequenz der Sprungcluster (FB) werden als Funktion der prozentualen Dickenreduzierung gemessen. Der prozentuale Anstieg der Dickenreduzierung bis zu 55% verursacht den Abfall von UB und FB. UB verschwindet bei gewissen Werten der Magnetisierungsfrequenz. Die verschwindende Magnetisierungsfrequenz hangt von der prozentualen Dickenreduzierung ab. Das Verschwinden von UB wird den Wirbelstromen in der Probe zugeordnet. Warmebehandlung hat einen betrachtlichen Einflus sowohl auf UB als auch auf die verschwindende Magnetisierungsfrequenz.