B. Omrane, J. Aristizabal, C. Landrock, Y. Chuo, D. Fournier, S. V. Grayli, B. Kaminska
{"title":"Enhancement of indium-based organic photovoltaics","authors":"B. Omrane, J. Aristizabal, C. Landrock, Y. Chuo, D. Fournier, S. V. Grayli, B. Kaminska","doi":"10.1109/PVSC.2012.6318062","DOIUrl":null,"url":null,"abstract":"We report on the optimization of poly(3-hexylthiopene) and [6,6]-phenyl C61 butyric acid methyl ester bulk heterojunction photovoltaics using indium tin oxide anode and metallic indium cathode. The devices are fabricated, tested, and stored at ambient atmosphere, without encapsulation. By tuning the spin coating conditions for the hole-transport and the photoactive layers, along with a combination of mechanical pressure and annealing conditions during the cathode deposition, a 3-fold improvement is achieved, while maintaining devices stability. Consequently, the cells undergo a less than 10% loss in power conversion efficiency after 200 days.","PeriodicalId":6318,"journal":{"name":"2012 38th IEEE Photovoltaic Specialists Conference","volume":"1 1","pages":"002321-002323"},"PeriodicalIF":0.0000,"publicationDate":"2012-10-04","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2012 38th IEEE Photovoltaic Specialists Conference","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/PVSC.2012.6318062","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
We report on the optimization of poly(3-hexylthiopene) and [6,6]-phenyl C61 butyric acid methyl ester bulk heterojunction photovoltaics using indium tin oxide anode and metallic indium cathode. The devices are fabricated, tested, and stored at ambient atmosphere, without encapsulation. By tuning the spin coating conditions for the hole-transport and the photoactive layers, along with a combination of mechanical pressure and annealing conditions during the cathode deposition, a 3-fold improvement is achieved, while maintaining devices stability. Consequently, the cells undergo a less than 10% loss in power conversion efficiency after 200 days.