{"title":"Structure Property Correlation of Thin Wall Ductile Iron","authors":"R. Upadhyaya, K. Singh","doi":"10.5539/JMSR.V8N1P1","DOIUrl":null,"url":null,"abstract":"This research work concerns an assessment of the effect of one step inoculation method on thin section castings (2-5) mm analyzed. In this study inoculants representing Ce, Zr and Sr bearing Fe-Si alloys were used. It has been observed that section thickness of 2 mm thin plate containing Ce bearing Fe-Si alloys at 0.4wt% contain mainly pearlitic matrix having microhardness (HV20), ultimate tensile strength (UTS) and percentage of elongation are 272 HV, 720 MPa and 4.5% respectively. It was observed that wear of 2 mm section thickness of thin plate containing Ce bearing Fe-Si alloys have greater wear resistance (272HV) compare to Zr bearing Fe-Si alloys (262HV) and Sr bearing Fe-Si alloys (259HV) respectively at 0.4wt% due to reason of pearlitic and ferritic volume fraction contents present in matrix.","PeriodicalId":16111,"journal":{"name":"Journal of Materials Science Research","volume":"18 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2018-11-14","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Materials Science Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5539/JMSR.V8N1P1","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
This research work concerns an assessment of the effect of one step inoculation method on thin section castings (2-5) mm analyzed. In this study inoculants representing Ce, Zr and Sr bearing Fe-Si alloys were used. It has been observed that section thickness of 2 mm thin plate containing Ce bearing Fe-Si alloys at 0.4wt% contain mainly pearlitic matrix having microhardness (HV20), ultimate tensile strength (UTS) and percentage of elongation are 272 HV, 720 MPa and 4.5% respectively. It was observed that wear of 2 mm section thickness of thin plate containing Ce bearing Fe-Si alloys have greater wear resistance (272HV) compare to Zr bearing Fe-Si alloys (262HV) and Sr bearing Fe-Si alloys (259HV) respectively at 0.4wt% due to reason of pearlitic and ferritic volume fraction contents present in matrix.