{"title":"Thermo-oxidative Oligomerization of Aromatic Diamine","authors":"B. Zaitsev, L. G. Kleptsova, I. D. Shvabskaya, А.E. Bursian","doi":"10.30564/OPMR.V3I1.3612","DOIUrl":null,"url":null,"abstract":"Molecular spectroscopy (electronic, FT-IR, NMR), methods of thermal and elemental analysis were used for the first time to describe the process of thermo-oxidative oligomerization of 1,3-bis-(4-aminophenoxy)benzene. Introduction of this monomer into linear and network copolymers makes it possible to improve processability, mechanical strength and heat resistance of materials. The structures of copolymers obtained by thermo-oxidation of the diamine in various thermal regimes were studied. It was demonstrated that during prolonged heating of this diamine in air in the temperature range from 220 to 320°C, oligomeric aromatic diamines were formed; these products contained fragments of benzenoid and quinoid types.","PeriodicalId":19583,"journal":{"name":"Organic Polymer Material Research","volume":"65 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2021-09-24","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Organic Polymer Material Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.30564/OPMR.V3I1.3612","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
Molecular spectroscopy (electronic, FT-IR, NMR), methods of thermal and elemental analysis were used for the first time to describe the process of thermo-oxidative oligomerization of 1,3-bis-(4-aminophenoxy)benzene. Introduction of this monomer into linear and network copolymers makes it possible to improve processability, mechanical strength and heat resistance of materials. The structures of copolymers obtained by thermo-oxidation of the diamine in various thermal regimes were studied. It was demonstrated that during prolonged heating of this diamine in air in the temperature range from 220 to 320°C, oligomeric aromatic diamines were formed; these products contained fragments of benzenoid and quinoid types.