S. Suresh, P. Kumari, J. M. Jha, S. Verma, S. Arisutha, P. Lens
{"title":"Sonocatalytic removal of naphthalene from an aqueous solution using ZnO nanoparticles","authors":"S. Suresh, P. Kumari, J. M. Jha, S. Verma, S. Arisutha, P. Lens","doi":"10.2166/aqua.2022.042","DOIUrl":null,"url":null,"abstract":"\n This research presents the sonocatalytic degradation of naphthalene from an aqueous medium using a zinc oxide (ZnO) catalyst synthesised by the thermal decomposition method. The present paper also aims to apply the response surface methodology for the evaluation of the effect of different parameters on the degradation rate. The optimum parameters were found to be 50 min of reaction time, 2.2 g/l of the ZnO catalyst mass, 30 °C, 280 V, and 80 mg/l of initial concentration under a constant ultrasonic treatment at 20 kHz and 260 W of power intensity. The elemental composition of the catalyst was as follows: Zn 25.18%, O 37.03%, Mg 3.20%, K 0.83%, Ca 4.05%, N 5.07%, Na 4.13%, Cl 3.43%, and Fe 0.32%. Fourier Transform Infra-Red (FTIR) confirmed the Zn–O bond stretching at 510 cm−1. The degradation efficiency of naphthalene was almost double when the ZnO catalyst was used. The naphthalene degradation rate was a first-order reaction. Analysis of variance (ANOVA) results show that the quadratic model is suitable for the obtained data (P-value = 0.0001) and in an optimal process, performance conditions were set equal to 100%. Regression analysis with a high correlation coefficient (R2 = 0.989) and the model F-value of 6.94 indicated the adequacy of the model. The reusability study revealed that ZnO as a catalyst sustained the catalytic activity over five cycles.","PeriodicalId":17666,"journal":{"name":"Journal of Water Supply: Research and Technology-Aqua","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2022-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Water Supply: Research and Technology-Aqua","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2166/aqua.2022.042","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
This research presents the sonocatalytic degradation of naphthalene from an aqueous medium using a zinc oxide (ZnO) catalyst synthesised by the thermal decomposition method. The present paper also aims to apply the response surface methodology for the evaluation of the effect of different parameters on the degradation rate. The optimum parameters were found to be 50 min of reaction time, 2.2 g/l of the ZnO catalyst mass, 30 °C, 280 V, and 80 mg/l of initial concentration under a constant ultrasonic treatment at 20 kHz and 260 W of power intensity. The elemental composition of the catalyst was as follows: Zn 25.18%, O 37.03%, Mg 3.20%, K 0.83%, Ca 4.05%, N 5.07%, Na 4.13%, Cl 3.43%, and Fe 0.32%. Fourier Transform Infra-Red (FTIR) confirmed the Zn–O bond stretching at 510 cm−1. The degradation efficiency of naphthalene was almost double when the ZnO catalyst was used. The naphthalene degradation rate was a first-order reaction. Analysis of variance (ANOVA) results show that the quadratic model is suitable for the obtained data (P-value = 0.0001) and in an optimal process, performance conditions were set equal to 100%. Regression analysis with a high correlation coefficient (R2 = 0.989) and the model F-value of 6.94 indicated the adequacy of the model. The reusability study revealed that ZnO as a catalyst sustained the catalytic activity over five cycles.
本文研究了用热分解法合成的氧化锌(ZnO)催化剂对萘的声催化降解。本文还旨在应用响应面法评价不同参数对降解率的影响。结果表明,在20 kHz、260 W的恒定超声处理下,反应时间为50 min,催化剂质量为2.2 g/l,反应温度为30℃,反应电压为280 V,初始浓度为80 mg/l。催化剂的元素组成为:Zn 25.18%, O 37.03%, Mg 3.20%, K 0.83%, Ca 4.05%, N 5.07%, Na 4.13%, Cl 3.43%, Fe 0.32%。傅里叶变换红外(FTIR)证实了Zn-O键在510 cm−1处的拉伸。使用ZnO催化剂时,萘的降解效率几乎提高了一倍。萘的降解速率为一级反应。方差分析(ANOVA)结果表明,二次模型适用于所获得的数据(p值= 0.0001),在最优工艺中,性能条件设置为100%。回归分析显示相关系数较高(R2 = 0.989),模型f值为6.94,表明模型的充分性。重复使用研究表明,ZnO作为催化剂的催化活性可维持5个循环以上。