{"title":"PIND测试失败的SEM/EDAX分析","authors":"J. F. D. Porto, D. Loescher, H. Olson, P. Plunkett","doi":"10.1109/IRPS.1981.362989","DOIUrl":null,"url":null,"abstract":"Packaged LSI and hybrid devices used in high reliability military and space applications must pass a rigorous series of screens defined by Method 5004 of Mil Standard 883B. One of these screens is the Particle Impact Noise Detection (PIND) test. This test uses a very sensitive acoustic transducer to listen for particles within the package while the package is vibrated and shocked. We have used SEM, EDAX, and optical microscopy to analyze the particles from PIND failures. From these analyses we have identified the primary sources of PIND failures and have developed procedures that yield a low reject rate at PIND test. The device used in this investigation was a 1 K RAM die eutectically attached to a 24-pin leadless hermetic package (LHP). The package is solder sealed in a belt furnace with a gold-tin eutectic preform and a gold-plated cover. We have recovered the particles from PIND test failures by placing lead tape over a punched hole in the gold plated Kovar lid. The package is then vibrated until the particles pass through the hole and are attached to the adhesive on the tape. From the analyses we have identified many sources of particles that cause PIND test failures; the main source being the gold-tin solder preform used in the sealing process. We have investigated the effect of sealing materials, furnace temperature, furnace ambient, and package orientation on the number of gold-tin solder spheres.","PeriodicalId":376954,"journal":{"name":"19th International Reliability Physics Symposium","volume":"23 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"SEM/EDAX Analysis of PIND Test Failures\",\"authors\":\"J. F. D. Porto, D. Loescher, H. Olson, P. Plunkett\",\"doi\":\"10.1109/IRPS.1981.362989\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Packaged LSI and hybrid devices used in high reliability military and space applications must pass a rigorous series of screens defined by Method 5004 of Mil Standard 883B. One of these screens is the Particle Impact Noise Detection (PIND) test. This test uses a very sensitive acoustic transducer to listen for particles within the package while the package is vibrated and shocked. We have used SEM, EDAX, and optical microscopy to analyze the particles from PIND failures. From these analyses we have identified the primary sources of PIND failures and have developed procedures that yield a low reject rate at PIND test. The device used in this investigation was a 1 K RAM die eutectically attached to a 24-pin leadless hermetic package (LHP). The package is solder sealed in a belt furnace with a gold-tin eutectic preform and a gold-plated cover. We have recovered the particles from PIND test failures by placing lead tape over a punched hole in the gold plated Kovar lid. The package is then vibrated until the particles pass through the hole and are attached to the adhesive on the tape. From the analyses we have identified many sources of particles that cause PIND test failures; the main source being the gold-tin solder preform used in the sealing process. We have investigated the effect of sealing materials, furnace temperature, furnace ambient, and package orientation on the number of gold-tin solder spheres.\",\"PeriodicalId\":376954,\"journal\":{\"name\":\"19th International Reliability Physics Symposium\",\"volume\":\"23 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1900-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"19th International Reliability Physics Symposium\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/IRPS.1981.362989\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"19th International Reliability Physics Symposium","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/IRPS.1981.362989","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

摘要

用于高可靠性军事和空间应用的封装LSI和混合器件必须通过Mil标准883B方法5004定义的一系列严格的筛选。其中一个屏幕是粒子冲击噪声检测(PIND)测试。该测试使用一个非常灵敏的声学换能器,在包装受到振动和冲击时,聆听包装内的颗粒。我们使用SEM, EDAX和光学显微镜来分析PIND失效的颗粒。从这些分析中,我们已经确定了PIND失败的主要来源,并制定了在PIND测试中产生低废品率的程序。本研究中使用的器件是一个1k RAM芯片,共晶连接到一个24针无引线密封封装(LHP)。该包是焊料密封在带炉与金-锡共晶预铸和镀金盖。我们已经从PIND测试失败中恢复了颗粒,将铅带放在镀金科瓦尔盖的穿孔上。然后,包装被振动,直到颗粒穿过孔并附着在胶带上的粘合剂上。从分析中,我们已经确定了导致PIND测试失败的许多颗粒来源;主要来源是密封过程中使用的金锡焊料预制体。我们研究了密封材料、炉温、炉环境和封装方向对金锡焊料球数量的影响。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
SEM/EDAX Analysis of PIND Test Failures
Packaged LSI and hybrid devices used in high reliability military and space applications must pass a rigorous series of screens defined by Method 5004 of Mil Standard 883B. One of these screens is the Particle Impact Noise Detection (PIND) test. This test uses a very sensitive acoustic transducer to listen for particles within the package while the package is vibrated and shocked. We have used SEM, EDAX, and optical microscopy to analyze the particles from PIND failures. From these analyses we have identified the primary sources of PIND failures and have developed procedures that yield a low reject rate at PIND test. The device used in this investigation was a 1 K RAM die eutectically attached to a 24-pin leadless hermetic package (LHP). The package is solder sealed in a belt furnace with a gold-tin eutectic preform and a gold-plated cover. We have recovered the particles from PIND test failures by placing lead tape over a punched hole in the gold plated Kovar lid. The package is then vibrated until the particles pass through the hole and are attached to the adhesive on the tape. From the analyses we have identified many sources of particles that cause PIND test failures; the main source being the gold-tin solder preform used in the sealing process. We have investigated the effect of sealing materials, furnace temperature, furnace ambient, and package orientation on the number of gold-tin solder spheres.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
NMOS Voltage Breakdown Characteristics Compared with Accelerated Life Tests and Field use Data The Effect of Insulation Coatings on Forward Beta Degradation in Bipolar Transistors The use of Silicone RTV Rubber for Alpha Particle Protection on Silicon Integrated Circuits Reliability of DH Ga1-XAlX As LEDs For Lightwave Communications A Method of Detecting Hot Spots on Semiconductors using Liquid Crystals
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1