{"title":"环氧树脂-砾石复合浓度对球试验硬度变化的影响","authors":"A. Mikhalchenkov, Yu. I. Filin, S. Feskov","doi":"10.36652/1813-1336-2022-18-9-393-395","DOIUrl":null,"url":null,"abstract":"The hardness value of the epoxy-gravel composite, measured by a ball sample, is determined by the amount of gravel component, as well as the degree of heterogeneity (heterogeneity) of the structure. The maximum hardness value is a composite with a granite component content of 70 wt.h.","PeriodicalId":178558,"journal":{"name":"Strengthening Technologies and Coatings","volume":"47 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Effect of epoxy-gravel composite concentration on change in ball test hardness\",\"authors\":\"A. Mikhalchenkov, Yu. I. Filin, S. Feskov\",\"doi\":\"10.36652/1813-1336-2022-18-9-393-395\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The hardness value of the epoxy-gravel composite, measured by a ball sample, is determined by the amount of gravel component, as well as the degree of heterogeneity (heterogeneity) of the structure. The maximum hardness value is a composite with a granite component content of 70 wt.h.\",\"PeriodicalId\":178558,\"journal\":{\"name\":\"Strengthening Technologies and Coatings\",\"volume\":\"47 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1900-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Strengthening Technologies and Coatings\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.36652/1813-1336-2022-18-9-393-395\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Strengthening Technologies and Coatings","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.36652/1813-1336-2022-18-9-393-395","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Effect of epoxy-gravel composite concentration on change in ball test hardness
The hardness value of the epoxy-gravel composite, measured by a ball sample, is determined by the amount of gravel component, as well as the degree of heterogeneity (heterogeneity) of the structure. The maximum hardness value is a composite with a granite component content of 70 wt.h.