上料设备引入的表面污染与电接触电阻的关系

H.A. Francisco, K. Koeneke, J. Wallace
{"title":"上料设备引入的表面污染与电接触电阻的关系","authors":"H.A. Francisco, K. Koeneke, J. Wallace","doi":"10.1109/HOLM.1991.170832","DOIUrl":null,"url":null,"abstract":"Contact degradation caused by austenitic stainless steel feeder bowls has raised concern among manufacturers of electrical contacts. The surface contamination of three contact materials, fine silver, silver cadmium oxide (90%Ag 10%CdO), and a silver alloy (75%Ag 24.5%Cu 0. 5%Ni) with 15-microinch (Ra) surface finish, was investigated. Contact resistance probing was employed and surfaces were analyzed to explain the degradation process. The investigation elucidated the effects of various vibratory feeder bowl coatings which reduced surface contamination. The attainment of low contact resistance was explained as interactions among nobility of contact material, type of coating, and time spent in the vibratory feeder bowl.<<ETX>>","PeriodicalId":368900,"journal":{"name":"Electrical Contacts - 1991 Proceedings of the Thirty-Seventh IEEE HOLM Conference on Electrical Contacts","volume":"110 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":"{\"title\":\"Correlation of surface contamination introduced by feeding equipment on electrical contact resistance\",\"authors\":\"H.A. Francisco, K. Koeneke, J. Wallace\",\"doi\":\"10.1109/HOLM.1991.170832\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Contact degradation caused by austenitic stainless steel feeder bowls has raised concern among manufacturers of electrical contacts. The surface contamination of three contact materials, fine silver, silver cadmium oxide (90%Ag 10%CdO), and a silver alloy (75%Ag 24.5%Cu 0. 5%Ni) with 15-microinch (Ra) surface finish, was investigated. Contact resistance probing was employed and surfaces were analyzed to explain the degradation process. The investigation elucidated the effects of various vibratory feeder bowl coatings which reduced surface contamination. The attainment of low contact resistance was explained as interactions among nobility of contact material, type of coating, and time spent in the vibratory feeder bowl.<<ETX>>\",\"PeriodicalId\":368900,\"journal\":{\"name\":\"Electrical Contacts - 1991 Proceedings of the Thirty-Seventh IEEE HOLM Conference on Electrical Contacts\",\"volume\":\"110 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1900-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"3\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Electrical Contacts - 1991 Proceedings of the Thirty-Seventh IEEE HOLM Conference on Electrical Contacts\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/HOLM.1991.170832\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Electrical Contacts - 1991 Proceedings of the Thirty-Seventh IEEE HOLM Conference on Electrical Contacts","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/HOLM.1991.170832","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

摘要

奥氏体不锈钢给料碗引起的触点退化引起了电触点制造商的关注。三种接触材料,细银,氧化银镉(90%Ag 10%CdO)和银合金(75%Ag 24.5%Cu 0)的表面污染。5%Ni),表面光洁度为15微英寸(Ra)。采用接触电阻探测和表面分析来解释降解过程。研究了各种振动给料碗涂层对降低给料碗表面污染的效果。低接触电阻的实现被解释为接触材料的高贵程度、涂层类型和在振动给料碗中度过的时间的相互作用
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Correlation of surface contamination introduced by feeding equipment on electrical contact resistance
Contact degradation caused by austenitic stainless steel feeder bowls has raised concern among manufacturers of electrical contacts. The surface contamination of three contact materials, fine silver, silver cadmium oxide (90%Ag 10%CdO), and a silver alloy (75%Ag 24.5%Cu 0. 5%Ni) with 15-microinch (Ra) surface finish, was investigated. Contact resistance probing was employed and surfaces were analyzed to explain the degradation process. The investigation elucidated the effects of various vibratory feeder bowl coatings which reduced surface contamination. The attainment of low contact resistance was explained as interactions among nobility of contact material, type of coating, and time spent in the vibratory feeder bowl.<>
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Evaluation of a mixed flowing gas test Description and test results of a current collection system for continuous duty HPG Influence of the power factor on the degradation of Ag-W electrical contact circuit-breakers The importance of the thickness of silver coating in the corrosion behaviour of copper contacts Reliability of commercial relays during life tests with intermediate or low power contact load
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1