激光切割时工件在托板上的位置对热影响区形成的影响

IF 0.9 4区 物理与天体物理 Q4 PHYSICS, CONDENSED MATTER Physics of the Solid State Pub Date : 2023-12-08 DOI:10.1134/S1063783423700117
Ya. A. Erisov, V. V. Afrikantov, Yu. S. Gorshkov, V. A. Razzhivin
{"title":"激光切割时工件在托板上的位置对热影响区形成的影响","authors":"Ya. A. Erisov,&nbsp;V. V. Afrikantov,&nbsp;Yu. S. Gorshkov,&nbsp;V. A. Razzhivin","doi":"10.1134/S1063783423700117","DOIUrl":null,"url":null,"abstract":"<p>The study in this work focuses on the properties and structure of the material in the heat-affected zone that occurs during laser metal cutting, depending on the positioning of the workpiece on the pallet: above the protrusion and between the protrusions of the pallet. Significant differences in properties and structure in these areas are demonstrated. Recommendations on the positioning of the workpiece relative to the pallet protrusions are given. Material properties in the cutting zone above the pallet protrusion and between the protrusions differ significantly. Microhardness values in the zone above the pallet protrusions at the edge are approximately 50% lower than in the zone between the protrusions. As the analysis moves deeper into the sample, the difference decreases. The magnesium concentration is nearly two times lower in the zone above the protrusions than between the protrusions. In the surface layers of the workpiece above the protrusions, the sizes of inclusions are larger than in the depth. This is due to additional quenching of the metal in the workpiece located between the protrusions and prolonged contact with the bath of liquid metal due to difficulties in its removal during cutting on the pallet protrusion. Removing the defective layer by milling to a depth of 0.5 mm neutralizes the difference in the material properties in the zone above the pallet protrusion, between the protrusions, and in the depth.</p>","PeriodicalId":731,"journal":{"name":"Physics of the Solid State","volume":"65 1","pages":"12 - 16"},"PeriodicalIF":0.9000,"publicationDate":"2023-12-08","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Impact of Workpiece Position on Pallet during Laser Cutting on Heat-Affected Zone Formation\",\"authors\":\"Ya. A. Erisov,&nbsp;V. V. Afrikantov,&nbsp;Yu. S. Gorshkov,&nbsp;V. A. Razzhivin\",\"doi\":\"10.1134/S1063783423700117\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The study in this work focuses on the properties and structure of the material in the heat-affected zone that occurs during laser metal cutting, depending on the positioning of the workpiece on the pallet: above the protrusion and between the protrusions of the pallet. Significant differences in properties and structure in these areas are demonstrated. Recommendations on the positioning of the workpiece relative to the pallet protrusions are given. Material properties in the cutting zone above the pallet protrusion and between the protrusions differ significantly. Microhardness values in the zone above the pallet protrusions at the edge are approximately 50% lower than in the zone between the protrusions. As the analysis moves deeper into the sample, the difference decreases. The magnesium concentration is nearly two times lower in the zone above the protrusions than between the protrusions. In the surface layers of the workpiece above the protrusions, the sizes of inclusions are larger than in the depth. This is due to additional quenching of the metal in the workpiece located between the protrusions and prolonged contact with the bath of liquid metal due to difficulties in its removal during cutting on the pallet protrusion. Removing the defective layer by milling to a depth of 0.5 mm neutralizes the difference in the material properties in the zone above the pallet protrusion, between the protrusions, and in the depth.</p>\",\"PeriodicalId\":731,\"journal\":{\"name\":\"Physics of the Solid State\",\"volume\":\"65 1\",\"pages\":\"12 - 16\"},\"PeriodicalIF\":0.9000,\"publicationDate\":\"2023-12-08\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Physics of the Solid State\",\"FirstCategoryId\":\"101\",\"ListUrlMain\":\"https://link.springer.com/article/10.1134/S1063783423700117\",\"RegionNum\":4,\"RegionCategory\":\"物理与天体物理\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"PHYSICS, CONDENSED MATTER\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Physics of the Solid State","FirstCategoryId":"101","ListUrlMain":"https://link.springer.com/article/10.1134/S1063783423700117","RegionNum":4,"RegionCategory":"物理与天体物理","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"PHYSICS, CONDENSED MATTER","Score":null,"Total":0}
引用次数: 0

摘要

摘要 这项工作的研究重点是激光金属切割过程中热影响区材料的特性和结构,这取决于工件在托板上的位置:托板突出部分上方和突出部分之间。这些区域的特性和结构存在显著差异。给出了工件相对于托板突出部分的定位建议。托板突出物上方和突出物之间切削区域的材料特性差异显著。边缘处托板突起上方区域的显微硬度值比突起之间区域低约 50%。随着分析深入样品,差异逐渐减小。突出物上方区域的镁浓度比突出物之间区域低近两倍。在突出物上方的工件表层,夹杂物的尺寸比深度大。这是由于位于突起之间的工件中的金属发生了额外的淬火,以及在托板突起上进行切割时,由于难以去除液态金属而与液态金属浴长时间接触。通过铣削 0.5 mm 的深度去除缺陷层,可以中和托板突起上方区域、突起之间以及深度区域的材料特性差异。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

摘要图片

摘要图片

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Impact of Workpiece Position on Pallet during Laser Cutting on Heat-Affected Zone Formation

The study in this work focuses on the properties and structure of the material in the heat-affected zone that occurs during laser metal cutting, depending on the positioning of the workpiece on the pallet: above the protrusion and between the protrusions of the pallet. Significant differences in properties and structure in these areas are demonstrated. Recommendations on the positioning of the workpiece relative to the pallet protrusions are given. Material properties in the cutting zone above the pallet protrusion and between the protrusions differ significantly. Microhardness values in the zone above the pallet protrusions at the edge are approximately 50% lower than in the zone between the protrusions. As the analysis moves deeper into the sample, the difference decreases. The magnesium concentration is nearly two times lower in the zone above the protrusions than between the protrusions. In the surface layers of the workpiece above the protrusions, the sizes of inclusions are larger than in the depth. This is due to additional quenching of the metal in the workpiece located between the protrusions and prolonged contact with the bath of liquid metal due to difficulties in its removal during cutting on the pallet protrusion. Removing the defective layer by milling to a depth of 0.5 mm neutralizes the difference in the material properties in the zone above the pallet protrusion, between the protrusions, and in the depth.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Physics of the Solid State
Physics of the Solid State 物理-物理:凝聚态物理
CiteScore
1.70
自引率
0.00%
发文量
60
审稿时长
2-4 weeks
期刊介绍: Presents the latest results from Russia’s leading researchers in condensed matter physics at the Russian Academy of Sciences and other prestigious institutions. Covers all areas of solid state physics including solid state optics, solid state acoustics, electronic and vibrational spectra, phase transitions, ferroelectricity, magnetism, and superconductivity. Also presents review papers on the most important problems in solid state physics.
期刊最新文献
Thermoelectric Power Characteristics of Quaternary Layered Structured Tl4In3GaS8 Crystals Elastic Properties and Regularities in Frequencies of Optical Phonons of \({{{\mathbf{A}}}^{{{\mathbf{II}}}}}{\mathbf{B}}_{2}^{{{\mathbf{III}}}}{\mathbf{C}}_{4}^{{{\mathbf{VI}}}}\) Compounds Impact of Temperature on the Structural and Optical Properties of Silver Sulfide Films Prepared by Chemical Bath Deposition Optical Properties of GaS Nanoparticles Prepared by Laser Ablation Evaluating the Potential of Ca3SbBr3 Halide Perovskite for Photovoltaics: A Structural, Mechanical, and Optoelectronic Study Using GGA-PBE and HSE06 Functionals
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1