在延迟添加低剂量氢氧化钠的水浸出过程中二次铝渣(SAD)的脱硝机理

IF 4.8 2区 材料科学 Q1 METALLURGY & METALLURGICAL ENGINEERING Hydrometallurgy Pub Date : 2024-04-21 DOI:10.1016/j.hydromet.2024.106318
Chuan Wang , Yongchun Guo , YongYi He , Sen Li , Jun Liu , Hu Liu
{"title":"在延迟添加低剂量氢氧化钠的水浸出过程中二次铝渣(SAD)的脱硝机理","authors":"Chuan Wang ,&nbsp;Yongchun Guo ,&nbsp;YongYi He ,&nbsp;Sen Li ,&nbsp;Jun Liu ,&nbsp;Hu Liu","doi":"10.1016/j.hydromet.2024.106318","DOIUrl":null,"url":null,"abstract":"<div><p>Secondary aluminum dross (SAD) has been identified as a hazardous waste because it contains refractory AlN, fluoride, and other salts. Considering that Al(OH)<sub>3</sub> produced during the hydrolysis of AlN in SAD hinders spontaneous AlN hydrolysis, which is amplified by the partial embedment of AlN in other oxide phases present in SAD particles, the complete removal of AlN from SAD is difficult. Herein, we propose a new catalytic hydrolytic denitrification process of SAD, which requires a low additive dose. By changing the time at which the additive (NaOH) was added to the SAD slurry, the proportion of nitrogen removed from SAD was increased. The additive (NaOH) reacted with Al(OH)<sub>3</sub>, thereby mitigating its hindering effect on spontaneous AlN hydrolysis and facilitating the complete hydrolysis of the semi-encapsulated AlN in SAD particles. Concurrently, the reaction between NaOH and Al<sub>2</sub>O<sub>3</sub> and SiO<sub>2</sub> phases present in SAD was mitigated, resulting in the maximal retention of residual materials (phases other than Al resources) in the solid phase. A SAD denitrification efficiency of 99.0% was achieved under optimal processing conditions (<em>T</em> = 95 °C, <em>t</em> = 240 min, Liquid-to-solid ratio = 6:1, stirring speed = 400 rpm, and the addition of 7 wt% NaOH at 0.5 h), and a slightly lower efficiency of 98.2% was achieved when 50% lower amount of NaOH (3 wt%) was used. Thus, approximately 50% less additive is required for nitrogen removal from SAD, relative to that used in traditional catalytic water-washing processes.</p></div>","PeriodicalId":13193,"journal":{"name":"Hydrometallurgy","volume":"226 ","pages":"Article 106318"},"PeriodicalIF":4.8000,"publicationDate":"2024-04-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Mechanism of the denitrification of secondary aluminum dross (SAD) during water leaching with delayed addition of a low dosage of sodium hydroxide\",\"authors\":\"Chuan Wang ,&nbsp;Yongchun Guo ,&nbsp;YongYi He ,&nbsp;Sen Li ,&nbsp;Jun Liu ,&nbsp;Hu Liu\",\"doi\":\"10.1016/j.hydromet.2024.106318\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>Secondary aluminum dross (SAD) has been identified as a hazardous waste because it contains refractory AlN, fluoride, and other salts. Considering that Al(OH)<sub>3</sub> produced during the hydrolysis of AlN in SAD hinders spontaneous AlN hydrolysis, which is amplified by the partial embedment of AlN in other oxide phases present in SAD particles, the complete removal of AlN from SAD is difficult. Herein, we propose a new catalytic hydrolytic denitrification process of SAD, which requires a low additive dose. By changing the time at which the additive (NaOH) was added to the SAD slurry, the proportion of nitrogen removed from SAD was increased. The additive (NaOH) reacted with Al(OH)<sub>3</sub>, thereby mitigating its hindering effect on spontaneous AlN hydrolysis and facilitating the complete hydrolysis of the semi-encapsulated AlN in SAD particles. Concurrently, the reaction between NaOH and Al<sub>2</sub>O<sub>3</sub> and SiO<sub>2</sub> phases present in SAD was mitigated, resulting in the maximal retention of residual materials (phases other than Al resources) in the solid phase. A SAD denitrification efficiency of 99.0% was achieved under optimal processing conditions (<em>T</em> = 95 °C, <em>t</em> = 240 min, Liquid-to-solid ratio = 6:1, stirring speed = 400 rpm, and the addition of 7 wt% NaOH at 0.5 h), and a slightly lower efficiency of 98.2% was achieved when 50% lower amount of NaOH (3 wt%) was used. Thus, approximately 50% less additive is required for nitrogen removal from SAD, relative to that used in traditional catalytic water-washing processes.</p></div>\",\"PeriodicalId\":13193,\"journal\":{\"name\":\"Hydrometallurgy\",\"volume\":\"226 \",\"pages\":\"Article 106318\"},\"PeriodicalIF\":4.8000,\"publicationDate\":\"2024-04-21\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Hydrometallurgy\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/S0304386X24000586\",\"RegionNum\":2,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"METALLURGY & METALLURGICAL ENGINEERING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Hydrometallurgy","FirstCategoryId":"88","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S0304386X24000586","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 0

摘要

二次铝渣(SAD)因含有难熔铝氧化物、氟化物和其他盐类而被认定为危险废物。考虑到二次铝渣中的 AlN 在水解过程中产生的 Al(OH)会阻碍 AlN 的自发水解,而 AlN 部分嵌入二次铝渣颗粒中的其他氧化物相中又会放大自发水解,因此很难完全去除二次铝渣中的 AlN。在此,我们提出了一种新的 SAD 催化水解脱硝工艺,只需较低的添加剂剂量。通过改变添加剂(NaOH)加入 SAD 泥浆的时间,提高了 SAD 中脱氮的比例。添加剂(NaOH)与 Al(OH)发生反应,从而减轻了其对自发 AlN 水解的阻碍作用,促进了 SAD 颗粒中半封装 AlN 的完全水解。同时,NaOH 与 SAD 中的 AlO 和 SiO 相之间的反应也得到了缓解,从而最大限度地保留了固相中的残留物质(除 Al 资源外的其他相)。在最佳加工条件下(= 95 °C、= 240 分钟、液固比 = 6:1、搅拌速度 = 400 rpm、0.5 小时内添加 7 wt% 的 NaOH),SAD 脱硝效率达到 99.0%,而在使用较少 50% 的 NaOH(3 wt%)时,脱硝效率略低,为 98.2%。因此,与传统的催化水洗工艺相比,从 SAD 中脱氮所需的添加剂大约减少了 50%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

摘要图片

摘要图片

查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Mechanism of the denitrification of secondary aluminum dross (SAD) during water leaching with delayed addition of a low dosage of sodium hydroxide

Secondary aluminum dross (SAD) has been identified as a hazardous waste because it contains refractory AlN, fluoride, and other salts. Considering that Al(OH)3 produced during the hydrolysis of AlN in SAD hinders spontaneous AlN hydrolysis, which is amplified by the partial embedment of AlN in other oxide phases present in SAD particles, the complete removal of AlN from SAD is difficult. Herein, we propose a new catalytic hydrolytic denitrification process of SAD, which requires a low additive dose. By changing the time at which the additive (NaOH) was added to the SAD slurry, the proportion of nitrogen removed from SAD was increased. The additive (NaOH) reacted with Al(OH)3, thereby mitigating its hindering effect on spontaneous AlN hydrolysis and facilitating the complete hydrolysis of the semi-encapsulated AlN in SAD particles. Concurrently, the reaction between NaOH and Al2O3 and SiO2 phases present in SAD was mitigated, resulting in the maximal retention of residual materials (phases other than Al resources) in the solid phase. A SAD denitrification efficiency of 99.0% was achieved under optimal processing conditions (T = 95 °C, t = 240 min, Liquid-to-solid ratio = 6:1, stirring speed = 400 rpm, and the addition of 7 wt% NaOH at 0.5 h), and a slightly lower efficiency of 98.2% was achieved when 50% lower amount of NaOH (3 wt%) was used. Thus, approximately 50% less additive is required for nitrogen removal from SAD, relative to that used in traditional catalytic water-washing processes.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Hydrometallurgy
Hydrometallurgy 工程技术-冶金工程
CiteScore
9.50
自引率
6.40%
发文量
144
审稿时长
3.4 months
期刊介绍: Hydrometallurgy aims to compile studies on novel processes, process design, chemistry, modelling, control, economics and interfaces between unit operations, and to provide a forum for discussions on case histories and operational difficulties. Topics covered include: leaching of metal values by chemical reagents or bacterial action at ambient or elevated pressures and temperatures; separation of solids from leach liquors; removal of impurities and recovery of metal values by precipitation, ion exchange, solvent extraction, gaseous reduction, cementation, electro-winning and electro-refining; pre-treatment of ores by roasting or chemical treatments such as halogenation or reduction; recycling of reagents and treatment of effluents.
期刊最新文献
Preparation of high-purity iron oxide from end-of-life NdFeB magnet waste Efficient separation and recovery of cobalt from grinding waste of cemented carbide using a sulfuric acid-sodium persulfate mixed solution Separation of cerium from solution by oxidative precipitation with hydrogen peroxide: The reaction mechanism Phase evolution and elemental distribution of zinc and germanium during the sulfide roasting, zinc fuming and leaching processes: Benefit of pretreating zinc oxide dust Technological advancements in rare earth elements recovery from ionic clays: A comprehensive review
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1