Shaohua Li , Junheng Gao , Zhenyu Han , Haibo Feng , Chongmu Chen , Haitao Zhao , Shuize Wang , Kexiao Wang , Guilin Wu , Honghui Wu , Xinping Mao
{"title":"通过多元合金化和加速冷却提高珠光体轨道钢的强度和韧性","authors":"Shaohua Li , Junheng Gao , Zhenyu Han , Haibo Feng , Chongmu Chen , Haitao Zhao , Shuize Wang , Kexiao Wang , Guilin Wu , Honghui Wu , Xinping Mao","doi":"10.1016/j.msea.2024.147444","DOIUrl":null,"url":null,"abstract":"<div><div>The demand for higher speeds and heavier loads has emphasized the necessity to tackle the inherent trade-off between strength and toughness in pearlitic rail steels. Herein, the co-additions of Cr, Ni and Cu and accelerated cooling rate on the microstructure and mechanical properties of a medium carbon pearlitic steel were systematically investigated. In comparison with base alloy, the new steel exhibits smaller prior austenite grain size (PAGS) due to the drag effect of Cu and Ni solutes. The finer PAGS and lower C content increased the volume fraction of proeutectoid ferrite. The finer pearlitic nodule size (PNS) and pearlitic colony size (PCS) were attributed to the small PAGS and greater extent of undercooling due to the combined effect of multi-alloying and accelerated cooling. Additionally, the synergistic effects of multi-alloying and accelerated cooling rate decrease the pearlitic phase transformation temperature, accountable for the finer interlamellar spacing (IS). Compared with the base steel, the yield strength and ultimate tensile strength of the new steel increased from 587 MPa to 1069 MPa to 740 MPa and 1178 MPa, respectively, with a simultaneous increase of ductility from 12.4 % to 14.7 %. The strength increments are mainly attributed to the finer IS in the new steel. Meanwhile, the new steel possesses a higher impact toughness compared to the base steel due to the increased volume fraction of proeutectoid ferrite, and finer PNS and IS.</div></div>","PeriodicalId":385,"journal":{"name":"Materials Science and Engineering: A","volume":"918 ","pages":"Article 147444"},"PeriodicalIF":6.1000,"publicationDate":"2024-10-24","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Enhancing strength and toughness in a pearlitic rail steel via multi-alloying and accelerated cooling\",\"authors\":\"Shaohua Li , Junheng Gao , Zhenyu Han , Haibo Feng , Chongmu Chen , Haitao Zhao , Shuize Wang , Kexiao Wang , Guilin Wu , Honghui Wu , Xinping Mao\",\"doi\":\"10.1016/j.msea.2024.147444\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><div>The demand for higher speeds and heavier loads has emphasized the necessity to tackle the inherent trade-off between strength and toughness in pearlitic rail steels. Herein, the co-additions of Cr, Ni and Cu and accelerated cooling rate on the microstructure and mechanical properties of a medium carbon pearlitic steel were systematically investigated. In comparison with base alloy, the new steel exhibits smaller prior austenite grain size (PAGS) due to the drag effect of Cu and Ni solutes. The finer PAGS and lower C content increased the volume fraction of proeutectoid ferrite. The finer pearlitic nodule size (PNS) and pearlitic colony size (PCS) were attributed to the small PAGS and greater extent of undercooling due to the combined effect of multi-alloying and accelerated cooling. Additionally, the synergistic effects of multi-alloying and accelerated cooling rate decrease the pearlitic phase transformation temperature, accountable for the finer interlamellar spacing (IS). Compared with the base steel, the yield strength and ultimate tensile strength of the new steel increased from 587 MPa to 1069 MPa to 740 MPa and 1178 MPa, respectively, with a simultaneous increase of ductility from 12.4 % to 14.7 %. The strength increments are mainly attributed to the finer IS in the new steel. Meanwhile, the new steel possesses a higher impact toughness compared to the base steel due to the increased volume fraction of proeutectoid ferrite, and finer PNS and IS.</div></div>\",\"PeriodicalId\":385,\"journal\":{\"name\":\"Materials Science and Engineering: A\",\"volume\":\"918 \",\"pages\":\"Article 147444\"},\"PeriodicalIF\":6.1000,\"publicationDate\":\"2024-10-24\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Materials Science and Engineering: A\",\"FirstCategoryId\":\"5\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/S0921509324013753\",\"RegionNum\":2,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"MATERIALS SCIENCE, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials Science and Engineering: A","FirstCategoryId":"5","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S0921509324013753","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
Enhancing strength and toughness in a pearlitic rail steel via multi-alloying and accelerated cooling
The demand for higher speeds and heavier loads has emphasized the necessity to tackle the inherent trade-off between strength and toughness in pearlitic rail steels. Herein, the co-additions of Cr, Ni and Cu and accelerated cooling rate on the microstructure and mechanical properties of a medium carbon pearlitic steel were systematically investigated. In comparison with base alloy, the new steel exhibits smaller prior austenite grain size (PAGS) due to the drag effect of Cu and Ni solutes. The finer PAGS and lower C content increased the volume fraction of proeutectoid ferrite. The finer pearlitic nodule size (PNS) and pearlitic colony size (PCS) were attributed to the small PAGS and greater extent of undercooling due to the combined effect of multi-alloying and accelerated cooling. Additionally, the synergistic effects of multi-alloying and accelerated cooling rate decrease the pearlitic phase transformation temperature, accountable for the finer interlamellar spacing (IS). Compared with the base steel, the yield strength and ultimate tensile strength of the new steel increased from 587 MPa to 1069 MPa to 740 MPa and 1178 MPa, respectively, with a simultaneous increase of ductility from 12.4 % to 14.7 %. The strength increments are mainly attributed to the finer IS in the new steel. Meanwhile, the new steel possesses a higher impact toughness compared to the base steel due to the increased volume fraction of proeutectoid ferrite, and finer PNS and IS.
期刊介绍:
Materials Science and Engineering A provides an international medium for the publication of theoretical and experimental studies related to the load-bearing capacity of materials as influenced by their basic properties, processing history, microstructure and operating environment. Appropriate submissions to Materials Science and Engineering A should include scientific and/or engineering factors which affect the microstructure - strength relationships of materials and report the changes to mechanical behavior.