热电用机械合金化法合成Cu2ZnSnS4

IF 1.1 Q3 METALLURGY & METALLURGICAL ENGINEERING Acta Metallurgica Slovaca Pub Date : 2019-09-25 DOI:10.12776/ams.v25i3.1311
L. Bui, Khanh-Van Nguyen, B. Duong, Thang Hong Le, Bang Thi Le, S. Said
{"title":"热电用机械合金化法合成Cu2ZnSnS4","authors":"L. Bui, Khanh-Van Nguyen, B. Duong, Thang Hong Le, Bang Thi Le, S. Said","doi":"10.12776/ams.v25i3.1311","DOIUrl":null,"url":null,"abstract":"Quaternary chalcogenide Cu2ZnSnS4 is a potential candidate for thermoelectric (TE) application due to a number of advantages including containing only non-toxic and abundant elements, high Seebeck coefficient and low thermal conductivity. In this study, Cu2ZnSnS4 was synthesized using mechanical alloying method from Cu, Zn, Sn and S powders. In order to study the effect of milling duration on the formation of Cu2ZnSnS4, different milling duration of 2, 4, 12 and 16 h were investigated. As the results, Cu2ZnSnS4 was started to form after milling for 12 h. The formation of Cu2ZnSnS4 was completed after 16 h of milling. In addition, Cu2ZnSnS4 nanoparticles were obtained after 16 h of milling with the distribution mostly in the range of 50 - 60 nm.","PeriodicalId":44511,"journal":{"name":"Acta Metallurgica Slovaca","volume":null,"pages":null},"PeriodicalIF":1.1000,"publicationDate":"2019-09-25","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"SYNTHESIS OF Cu2ZnSnS4 BY MECHANICAL ALLOYING METHOD FOR THERMOELECTRIC APPLICATION\",\"authors\":\"L. Bui, Khanh-Van Nguyen, B. Duong, Thang Hong Le, Bang Thi Le, S. Said\",\"doi\":\"10.12776/ams.v25i3.1311\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Quaternary chalcogenide Cu2ZnSnS4 is a potential candidate for thermoelectric (TE) application due to a number of advantages including containing only non-toxic and abundant elements, high Seebeck coefficient and low thermal conductivity. In this study, Cu2ZnSnS4 was synthesized using mechanical alloying method from Cu, Zn, Sn and S powders. In order to study the effect of milling duration on the formation of Cu2ZnSnS4, different milling duration of 2, 4, 12 and 16 h were investigated. As the results, Cu2ZnSnS4 was started to form after milling for 12 h. The formation of Cu2ZnSnS4 was completed after 16 h of milling. In addition, Cu2ZnSnS4 nanoparticles were obtained after 16 h of milling with the distribution mostly in the range of 50 - 60 nm.\",\"PeriodicalId\":44511,\"journal\":{\"name\":\"Acta Metallurgica Slovaca\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":1.1000,\"publicationDate\":\"2019-09-25\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Acta Metallurgica Slovaca\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.12776/ams.v25i3.1311\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"METALLURGY & METALLURGICAL ENGINEERING\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Acta Metallurgica Slovaca","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.12776/ams.v25i3.1311","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 1

摘要

第四代硫系化合物Cu2ZnSnS4具有无毒、元素丰富、塞贝克系数高、导热系数低等优点,是热电(TE)材料的潜在候选材料。本研究以Cu、Zn、Sn和S粉末为原料,采用机械合金化法制备了Cu2ZnSnS4。为了研究铣削时间对Cu2ZnSnS4形成的影响,分别对铣削时间2、4、12和16 h进行了研究。结果表明,铣削12 h后Cu2ZnSnS4开始形成,铣削16 h后Cu2ZnSnS4完全形成。另外,经过16 h的铣削,得到了Cu2ZnSnS4纳米颗粒,其分布范围主要在50 ~ 60 nm。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
SYNTHESIS OF Cu2ZnSnS4 BY MECHANICAL ALLOYING METHOD FOR THERMOELECTRIC APPLICATION
Quaternary chalcogenide Cu2ZnSnS4 is a potential candidate for thermoelectric (TE) application due to a number of advantages including containing only non-toxic and abundant elements, high Seebeck coefficient and low thermal conductivity. In this study, Cu2ZnSnS4 was synthesized using mechanical alloying method from Cu, Zn, Sn and S powders. In order to study the effect of milling duration on the formation of Cu2ZnSnS4, different milling duration of 2, 4, 12 and 16 h were investigated. As the results, Cu2ZnSnS4 was started to form after milling for 12 h. The formation of Cu2ZnSnS4 was completed after 16 h of milling. In addition, Cu2ZnSnS4 nanoparticles were obtained after 16 h of milling with the distribution mostly in the range of 50 - 60 nm.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Acta Metallurgica Slovaca
Acta Metallurgica Slovaca METALLURGY & METALLURGICAL ENGINEERING-
CiteScore
2.00
自引率
30.00%
发文量
22
审稿时长
12 weeks
期刊最新文献
PHYSICO-MECHANICAL PROPERTIES OF POLYMER MATRIX COMPOSITE MATERIAL REINFORCED WITH CARBONIZED CASSAVA BACK PEEL AND IRON FILLINGS EFFECT OF MIXING METHODS PRIOR THE DECOMPOSITION PROCESS ON THE DECOMPOSED FERRONICKEL SLAG WEAR AND ADHESION PROPERTIES OF MULTILAYER Ti/TiN ,(TiC)/TiCN/TaN THIN FILMS DEPOSITED ON Ti13Nb13Zr ALLOY BY CLOSE FIELD UNBALANCED MAGNETRON SPUTTERING Explicit and Implicit Integration of Constitutive Equations of Chaboche Isotropic-Kinematic Hardening Material Model INFLUENCE OF SINTERING TEMPERATURE ON THE STRUCTURAL OF Mg2Si0.3Sn0.7 ALLOY PREPARED BY POWDER METALLURGY
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1