{"title":"Fe 3 O 4 纳米棒和Fe 2 O 3 纳米线的热氧化制备与表征","authors":"焦华 杨合情, Yang Hua","doi":"10.1360/ZB2009-39-1-39","DOIUrl":null,"url":null,"abstract":"以铁单质和草酸溶液为原料, 将0.75 mol/L的草酸溶液滴在铁片上, 于空气中200 ~ 600℃范围内加热1 h, 制备了Fe 3 O 4 纳米棒和Fe 2 O 3 纳米线, 用扫描电镜(SEM)、X射线衍射仪(XRD)和透射电子显微镜(TEM)对产物进行表征, 并研究了反应温度对产物形貌的影响. 结果表明, 在200 ~ 500℃下空气中反应1 h 在铁片上直接生长出矩形截面的多晶的立方相Fe3O4纳米棒, 其直径范围约为0.5 ~ 0.8 µm. 当反应温度为600℃, 得到的产物为六方相的Fe 2 O 3 纳米线. 研究表明, C 2 H 2 O 4 对纳米棒的形成起关键作用, 并提出了可能生长机理.","PeriodicalId":49128,"journal":{"name":"Science in China. Series B, Chemistry","volume":"14 1","pages":"39-45"},"PeriodicalIF":0.0000,"publicationDate":"2009-01-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Fe 3 O 4 纳米棒和Fe 2 O 3 纳米线的热氧化制备与表征\",\"authors\":\"焦华 杨合情, Yang Hua\",\"doi\":\"10.1360/ZB2009-39-1-39\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"以铁单质和草酸溶液为原料, 将0.75 mol/L的草酸溶液滴在铁片上, 于空气中200 ~ 600℃范围内加热1 h, 制备了Fe 3 O 4 纳米棒和Fe 2 O 3 纳米线, 用扫描电镜(SEM)、X射线衍射仪(XRD)和透射电子显微镜(TEM)对产物进行表征, 并研究了反应温度对产物形貌的影响. 结果表明, 在200 ~ 500℃下空气中反应1 h 在铁片上直接生长出矩形截面的多晶的立方相Fe3O4纳米棒, 其直径范围约为0.5 ~ 0.8 µm. 当反应温度为600℃, 得到的产物为六方相的Fe 2 O 3 纳米线. 研究表明, C 2 H 2 O 4 对纳米棒的形成起关键作用, 并提出了可能生长机理.\",\"PeriodicalId\":49128,\"journal\":{\"name\":\"Science in China. Series B, Chemistry\",\"volume\":\"14 1\",\"pages\":\"39-45\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2009-01-20\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Science in China. Series B, Chemistry\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1360/ZB2009-39-1-39\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Science in China. Series B, Chemistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1360/ZB2009-39-1-39","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
摘要
以铁单质和草酸溶液为原料, 将0.75 mol/L的草酸溶液滴在铁片上, 于空气中200 ~ 600℃范围内加热1 h, 制备了Fe 3 O 4 纳米棒和Fe 2 O 3 纳米线, 用扫描电镜(SEM)、X射线衍射仪(XRD)和透射电子显微镜(TEM)对产物进行表征, 并研究了反应温度对产物形貌的影响. 结果表明, 在200 ~ 500℃下空气中反应1 h 在铁片上直接生长出矩形截面的多晶的立方相Fe3O4纳米棒, 其直径范围约为0.5 ~ 0.8 µm. 当反应温度为600℃, 得到的产物为六方相的Fe 2 O 3 纳米线. 研究表明, C 2 H 2 O 4 对纳米棒的形成起关键作用, 并提出了可能生长机理.