{"title":"充氢316L奥氏体不锈钢的延展性和疲劳强度损失","authors":"U. Baek, T. Nguyen, S. Nahm, K. Ryu","doi":"10.1115/pvp2019-93180","DOIUrl":null,"url":null,"abstract":"\n The susceptibility of 316L-type austenite stainless steel to hydrogen was quantified by means of SSRT results and low-cycle fatigue life measurement. Both tests were conducted in the air condition after being charged with high-pressure hydrogen gas of 10 MPa and a temperature of 300°C for 120 hours. In addition, SSRT tests in gaseous hydrogen at a pressure of 10 MPa were also performed and compared to the tests conducted in hydrogen pre-charged and as-received conditions. The 0.2% yield strength and tensile strength did not show there to be a considerable difference between hydrogen pre-charging and the as-received conditions, whereas the gaseous hydrogen condition revealed a remarkable degradation in tensile properties, especially in terms of fracture elongation. In the case of fatigue life test, a considerable influence of hydrogen pre-charging in fatigue life properties was observed in the high strain amplitude regime whereas the measured values in the low strain deformation region are consistently comparable to that in the as-received condition. Fatigue limit was not affected by hydrogen pre-charging.","PeriodicalId":23651,"journal":{"name":"Volume 6B: Materials and Fabrication","volume":"38 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-11-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"Ductility and Fatigue Strength Loss of a Hydrogen-Charged 316L Austenitic Stainless Steel\",\"authors\":\"U. Baek, T. Nguyen, S. Nahm, K. Ryu\",\"doi\":\"10.1115/pvp2019-93180\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"\\n The susceptibility of 316L-type austenite stainless steel to hydrogen was quantified by means of SSRT results and low-cycle fatigue life measurement. Both tests were conducted in the air condition after being charged with high-pressure hydrogen gas of 10 MPa and a temperature of 300°C for 120 hours. In addition, SSRT tests in gaseous hydrogen at a pressure of 10 MPa were also performed and compared to the tests conducted in hydrogen pre-charged and as-received conditions. The 0.2% yield strength and tensile strength did not show there to be a considerable difference between hydrogen pre-charging and the as-received conditions, whereas the gaseous hydrogen condition revealed a remarkable degradation in tensile properties, especially in terms of fracture elongation. In the case of fatigue life test, a considerable influence of hydrogen pre-charging in fatigue life properties was observed in the high strain amplitude regime whereas the measured values in the low strain deformation region are consistently comparable to that in the as-received condition. Fatigue limit was not affected by hydrogen pre-charging.\",\"PeriodicalId\":23651,\"journal\":{\"name\":\"Volume 6B: Materials and Fabrication\",\"volume\":\"38 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2019-11-15\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Volume 6B: Materials and Fabrication\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1115/pvp2019-93180\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Volume 6B: Materials and Fabrication","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1115/pvp2019-93180","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

摘要

采用SSRT试验和低周疲劳寿命测定方法,定量研究了316l型奥氏体不锈钢对氢的敏感性。两项试验均在空气条件下进行,在300℃温度下充入10 MPa高压氢气120小时。此外,还在10 MPa压力下进行了气态氢的SSRT试验,并与氢气预充和接收条件下进行的试验进行了比较。在0.2%屈服强度和抗拉强度方面,预充氢与接收条件之间没有太大的差异,而气态氢条件显示拉伸性能明显下降,尤其是断裂伸长率。在疲劳寿命试验中,预充氢对高应变幅值区域的疲劳寿命性能有较大影响,而在低应变变形区域的测量值与接收条件下的测量值一致。预充氢对疲劳极限没有影响。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Ductility and Fatigue Strength Loss of a Hydrogen-Charged 316L Austenitic Stainless Steel
The susceptibility of 316L-type austenite stainless steel to hydrogen was quantified by means of SSRT results and low-cycle fatigue life measurement. Both tests were conducted in the air condition after being charged with high-pressure hydrogen gas of 10 MPa and a temperature of 300°C for 120 hours. In addition, SSRT tests in gaseous hydrogen at a pressure of 10 MPa were also performed and compared to the tests conducted in hydrogen pre-charged and as-received conditions. The 0.2% yield strength and tensile strength did not show there to be a considerable difference between hydrogen pre-charging and the as-received conditions, whereas the gaseous hydrogen condition revealed a remarkable degradation in tensile properties, especially in terms of fracture elongation. In the case of fatigue life test, a considerable influence of hydrogen pre-charging in fatigue life properties was observed in the high strain amplitude regime whereas the measured values in the low strain deformation region are consistently comparable to that in the as-received condition. Fatigue limit was not affected by hydrogen pre-charging.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Evaluating the Resistance of Austenitic Stainless Steel Welds to Hydrogen Embrittlement Improvement of Low-Temperature Toughness in Weld Metal Made of 9Cr-1Mo-V Steel by GTAW Method Load Normalization Method Accounting for Elastic and Elastic-Plastic Crack Growth Crack Growth Rate Testing and Large Plate Demonstration Under Chloride-Induced Stress Corrosion Cracking Conditions in Stainless Steel Canisters for Storage of Spent Nuclear Fuel An Efficient Modelling Approach for Predicting Residual Stress in Power-Beam Welds
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1